Control of As-/NH_3/N-containing Waste Water in W Metallurgy AITranslate
Abstract AITranslate
Description is made of the practice of As-/NHa/N-containing waste water treatment in W metallurgy in terms of process, principle, process flowsheet, efficiency, existing problems and improvement. The results showed that the waste water from APT production can be effectively controlled with combined process of "Lime ferrous salt for As removal;wet-method catalytic oxidation blowing for N removal".
KeyWords AITranslate
1蒋竹筠.治理钨离子交换废水流程的设计和研究[J].中国钨业,1995,0(9):15-19. 被引量:4
1曾琳,朱琼芳,卢贯能,陈来琳,匡庐峰,柯林.一株具砷氧化和反硝化功能的无色杆菌的筛选和鉴定[J].环境科学研究,2011,24(10):1123-1128.
2吴昆泽,钟常明,王汝胜,余夏静.同步硝化反硝化膜生物反应器脱除钨冶炼废水中氨氮的影响因素研究[J].水处理技术,2013,39(12):83-87. 被引量:4
3陈云嫩,王东霜,罗晓燕.钨冶炼过程含砷及氨氮废水处理技术研究[J].中国资源综合利用,2014,32(1):19-21. 被引量:8
4熊以俊,余欢荣,胡昌,刘东辉.钨及钴冶炼高氨氮废液处理的实践[J].中国钨业,2014,29(2):41-44. 被引量:3
5陈云嫩,罗小燕,熊昌狮,罗仙平.改性粉煤灰处理低浓度含砷含氨氮废水[J].广州化工,2014,42(22):146-148. 被引量:3
6陈云嫩,罗小燕,熊昌狮,罗仙平.改性粉煤灰吸附低浓度含砷含氨氮废水的机理研究[J].山东化工,2014,43(12):198-200. 被引量:4
7于亮,吴绍祖,程红光.季铵盐GW05和N263对Na_2WO_4溶液的萃钨性能对比研究[J].稀有金属,2015,39(3):193-200. 被引量:2
8欧阳婷,樊华,王涛.次氯酸钙—硫酸亚铁处理钨冶炼含砷含氨氮废水[J].有色金属:冶炼部分,2017(2):63-66. 被引量:5
9赖兰萍,陈后兴,陈冬英.氧化-铁盐混凝沉淀法处理钨冶炼含砷废水的试验研究[J].中国钨业,2018,33(1):66-70. 被引量:9
10王涛,万莹.APT生产废水水质及适用处理技术分析[J].工业水处理,2020,40(6):18-22. 被引量:3
1史明,唐忠阳,陈星宇.现代钨冶炼过程中废水处理现状与发展[J].稀有金属与硬质合金,2015,43(2):1-5. 被引量:6
2柴子绯,褚红.膜技术在高氨氮废水中的应用[J].水处理技术,2015,41(8):103-106. 被引量:5
3邓书妍,罗智江,简陈生,王汝胜,钟常明.钨冶炼废水SNDMBR过程膜阻力和清洗的研究[J].江西理工大学学报,2015,36(5):11-16. 被引量:1
4马清亮,廖俊杰,纵瑞涵,马建超,常丽萍,鲍卫仁,高梦凡,马红竹.粉煤灰-聚丙烯酸复合微凝胶对亚甲基蓝的吸附探究[J].硅酸盐通报,2016,35(2):380-385. 被引量:6
5韦建华,肖连生,曾理.碱性条件下钨萃取过程中铝的行为研究[J].中国钨业,2016,31(2):43-48.
6缪应菊,敖显字,胡庆林,李琳,陈定梅.改性粉煤灰超声辅助吸附低浓度氨氮废水的研究[J].环境科学与技术,2016,39(6):145-149. 被引量:4
7欧阳婷,樊华,王涛.次氯酸钙—硫酸亚铁处理钨冶炼含砷含氨氮废水[J].有色金属:冶炼部分,2017(2):63-66. 被引量:5
8薛磊,胡睦周.电催化氧化法在含氨氮废水处理中的应用[J].中国新技术新产品,2017(9):102-103.
9李昱秀,张焕祯,李海燕.负载铁氧化物吸附剂水处理除砷研究进展[J].水处理技术,2017,43(7):5-11. 被引量:8
10罗军,袁喜振.溶剂萃取法提取钨研究现状[J].中国钨业,2017,32(2):56-59. 被引量:5
1姚丽华,陈树茂,杨红.钨冶炼离子交换工艺废水的治理[J].湖南有色金属,2007,23(1):42-44. 被引量:8
2欧阳婷,樊华,王涛.次氯酸钙—硫酸亚铁处理钨冶炼含砷含氨氮废水[J].有色金属:冶炼部分,2017(2):63-66. 被引量:5
3陈云嫩,罗小燕,熊昌狮,罗仙平.改性粉煤灰处理低浓度含砷含氨氮废水[J].广州化工,2014,42(22):146-148. 被引量:3
4钟常明,王汝胜,吴昆泽,余夏静.铁盐絮凝+MBR处理钨冶炼含砷含氨氮废水[J].环境工程学报,2014,8(5):1840-1844. 被引量:12
5史明,唐忠阳,陈星宇.现代钨冶炼过程中废水处理现状与发展[J].稀有金属与硬质合金,2015,43(2):1-5. 被引量:6
6廖城城,魏立安,包亚强,刘章.清洁生产是企业实现可持续发展的有效措施[J].江西化工,2009,25(1):37-39. 被引量:1
7陈云嫩,王东霜,罗晓燕.钨冶炼过程含砷及氨氮废水处理技术研究[J].中国资源综合利用,2014,32(1):19-21. 被引量:8
8一种钨冶炼离子交换工艺废水的综合净化方法[J].化工环保,2012,32(4):324-324.
9刘常进,陈志民.含砷、氟酸性污水处理装置的设计与运行评价[J].化肥工业,1997,24(6):50-53.
10刘荣利.浅析污水处理的基本方法与原理[J].科学大众:智慧教育,2014(9):175-175.
Basic Information:
DOI:
Chinese Library Classification Number:X758[环境科学与工程—环境工程]
Citation Information:
Description is made of the practice of As-/NHa/N-containing waste water treatment in W metallurgy in terms of process, principle, process flowsheet, efficiency, existing problems and improvement. The results showed that the waste water from APT production can be effectively controlled with combined process of "Lime ferrous salt for As removal;wet-method catalytic oxidation blowing for N removal".
quote
| GB/T 7714-2015 | [1] YAO Li-hua, CHEN Shu-mao. Control of As-/NH_3/N-containing Waste Water in W Metallurgy[J]. Rare Metals and Cemented Carbides, 2007(3): 31-33. |
| MLA | [1] YAO Li-hua, and CHEN Shu-mao. "Control of As-/NH_3/N-containing Waste Water in W Metallurgy." Rare Metals and Cemented Carbides, no. 3, 2007, pp. 31-33. |
| APA | [1] YAO Li-hua, & CHEN Shu-mao. (2007). Control of As-/NH_3/N-containing Waste Water in W Metallurgy. Rare Metals and Cemented Carbides(3), 31-33. |
| IEEE | [1] YAO Li-hua and CHEN Shu-mao, "Control of As-/NH_3/N-containing Waste Water in W Metallurgy," Rare Metals and Cemented Carbides, no. 3, pp. 31-33, 2007. keywords: {W metallurgy;As-/NH3/N-containing waste water;lime-ferrous salt;wet-method catalytic oxi-dation;control works} |