Rapid Determination of Molybdenum in Solution AITranslate
Abstract AITranslate
Standard solution is prepared with spectral-pure molybdenum trioxide. The relationship curve between molybdenum concentration and absorbency is determined by Thiocyanate spectro-photometrical colorimetry.c= 0. 397 2×A,which is used to analyze molybdenum content in leach solution. And verification is done through the testing of Mo content in the leach able, the relative standard error is O. 34 %. Meanwhile termined with the same method and operating steps. standard error is O. 29 %. residue. The results showed both are well conform able,the relative standard error is 0.34%. Meanwhile Mo content in the waste water from a smelter is determined with the same method and operating steps. The results are also well conformable, the relative standard error is 0. 29 %.
KeyWords AITranslate
1席永红.原子荧光法同时测定塑料管浸出液中的砷和锑[J].净水技术,2005,24(6):66-67. 被引量:2
2施友富,黄宪法.加压浸出-萃取法从钼钴废催化剂中回收钼[J].中国钼业,2006,30(3):21-23. 被引量:7
3张惠,季剑波.茶自然冲泡状态下茶汤中锌浸出量的研究[J].茶业通报,2006,28(2):68-71. 被引量:3
4李桂春,纪守峰,王会平.碘化浸金时从浸出液中提金及碘再生方法研究[J].矿冶工程,2006,26(3):42-44. 被引量:17
5唐吉旺,黄坚.黄钠铁矾渣及其浸出液中铁的测定[J].四川化工,2005,8(3):40-42. 被引量:4
6陈小兰,林海山,佘璐.活性炭富集、比色法测定冶金浸出液中低含量的铂、钯[J].广东有色金属学报,2002,12(1):64-67. 被引量:5
7陈庆根,曾青云.离子交换法处理铜矿浸出渗透液的研究[J].有色金属:冶炼部分,2006(1):20-22. 被引量:2
8张军成.铜钼矿石的选矿及铜钼分离工艺[J].矿业快报,2006,22(8):13-15. 被引量:38
9许多丰,王开群,赵宏,何国才.钼钴废催化剂回收利用的研究[J].中国有色冶金,2005,34(3):45-47. 被引量:11
10乌红绪.亚铵法治理低浓度SO2生产工艺实践与理论分析[J].中国钼业,2005,29(2):26-28. 被引量:1
1李圆原,邱丽娜,弓爱君,王子佳,闫海,苑海涛.分光光度法测定生物浸矿培养基中的钼含量[J].金属世界,2009(5):44-47. 被引量:1
2孙宝莲,李波,王国栋,杨平平.硫氰酸盐光度法测定氨浸渣中的钼[J].稀有金属材料与工程,2009,38(12):2253-2256. 被引量:8
3赵志刚,刘治国,何峻荣,程福银.硫氰酸盐光度法测定三氧化钼中钼含量[J].固体火箭技术,2012,35(5):707-710. 被引量:2
4李延超,李来平,张新,刘燕.电感耦合等离子体原子发射光谱法测定碳化钼催化剂中钼[J].冶金分析,2014,34(11):61-64. 被引量:9
5丁海云,陈强,苑海涛,杨洁,王欣.分光光度法测定钼萃原液中钼含量的研究[J].铀矿冶,2017,36(3):227-230.
6赵晶晶.循环水中钼酸盐分析方法的改进[J].化工设计通讯,2019,45(9):136-138.
1周长玉.氯化亚锡还原硫氰酸钾分光光度法测定矿石中钼含量[J].内蒙古科技与经济,2012(4):76-77. 被引量:5
2孙宝莲,周恺,李波,薛丽英,杨平平.原子吸收光谱法测定工业氧化钼及氨浸渣中铁、铜和铅[J].理化检验:化学分册,2011,47(11):1351-1352. 被引量:1
3朱丽,孙宝莲,李海燕,李波.硫氰酸盐光度法测定加压氧化钼精矿萃取液中的钼[J].中国无机分析化学,2011,1(4):47-49. 被引量:5
4孙宝莲,李波,周恺,张磊,杨平平.钼精矿及烟道灰中铼的测定[J].稀有金属材料与工程,2011,40(11):2065-2068. 被引量:8
5余文丽,魏艳华,魏俊生,孙佩士.矿石中钼的测定方法的比较[J].广州化工,2014,42(3):75-76. 被引量:3
6张梦晗,陈宏,张晗,励建荣.薄膜梯度扩散-硫氰酸钾分光光度法富集测量水中痕量Mo(VI)[J].化学通报,2016,79(2):175-178. 被引量:4
7李延超,林小辉,梁静,李来平,王晖,张小明.电感耦合等离子体原子发射光谱法测定TaNb6合金中铌和10种杂质元素[J].冶金分析,2016,36(5):64-68. 被引量:8
8郑明光,生金峰,吴学纲,王永桃,隋大千,姬茹一,魏星,郑晓荣.一种测定高钼合金钢中钼元素质量分数的方法[J].石油化工设备,2017,46(1):20-23.
9贾春芳,陈小迪.电感耦合等离子体发射光谱法测定矿石中的钼[J].化学工程与装备,2017(7):242-243.
10曾明国,李永生,赵炀,杜鑫.基于流动注射光度法同时测定催化剂浸渍液中CoO/MoO_3[J].化工学报,2017,68(8):3056-3063.
1张雪娇,刘春叶,杨莉宁.果胶含量测定方法研究现状[J].应用化工,2015,44(4):729-731. 被引量:9
2徐灿丁.原子吸收法测定阳极泥及其浸出渣中银[J].铀矿冶,1994,13(2):133-136.
3孙媚华,陈迁,陈泽智,宋亭,宋光泉.紫外-可见分光光度法测定单质碘含量[J].仲恺农业工程学院学报,2012,25(2):37-41. 被引量:3
4郑一新,黄文川,程新胜,陈高昌,郑根武.一种快速测定一元弱酸pK_a的方法[J].化学教育,2005,26(10):55-56. 被引量:1
5晋霞,刘世斌.铋膜电极阳极溶出伏安法测定人发中锌的含量[J].太原理工大学学报,2008,39(2):199-202. 被引量:3
6郑再就.天然水中碳酸测定有关问题的探讨[J].杨凌职业技术学院学报,2007,6(1):9-11.
7张秀莉.环烷酸中异辛醇的简便测定方法[J].吉林工学院学报:自然科学版,1999,20(1):37-39. 被引量:1
8曹宏.原子吸收法测定浸出渣中的硒[J].有色矿冶,2005,21(5):61-62.
9曾波,付韬,贺铀,付志军.库仑滴定在锰矿石中硫的分析应用[J].中国锰业,2003,21(3):41-42. 被引量:2
10马萱.分光光度计波长误差及灵敏度校核初探[J].武汉工业大学学报,1992,14(1):130-130. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:O657.32[理学—分析化学]
Citation Information:
Standard solution is prepared with spectral-pure molybdenum trioxide. The relationship curve between molybdenum concentration and absorbency is determined by Thiocyanate spectro-photometrical colorimetry.c= 0. 397 2×A,which is used to analyze molybdenum content in leach solution. And verification is done through the testing of Mo content in the leach able, the relative standard error is O. 34 %. Meanwhile termined with the same method and operating steps. standard error is O. 29 %. residue. The results showed both are well conform able,the relative standard error is 0.34%. Meanwhile Mo content in the waste water from a smelter is determined with the same method and operating steps. The results are also well conformable, the relative standard error is 0. 29 %.
quote
| GB/T 7714-2015 | [1] JIA Li-juan, ZHONG Hong, FU Jian-gang. Rapid Determination of Molybdenum in Solution[J]. Rare Metals and Cemented Carbides, 2007(3): 34-37. |
| MLA | [1] JIA Li-juan, et al., "Rapid Determination of Molybdenum in Solution." Rare Metals and Cemented Carbides, no. 3, 2007, pp. 34-37. |
| APA | [1] JIA Li-juan, ZHONG Hong, & FU Jian-gang. (2007). Rapid Determination of Molybdenum in Solution. Rare Metals and Cemented Carbides(3), 34-37. |
| IEEE | [1] JIA Li-juan, ZHONG Hong, and FU Jian-gang, "Rapid Determination of Molybdenum in Solution," Rare Metals and Cemented Carbides, no. 3, pp. 34-37, 2007. keywords: {molybdenum;determine;absorbency;standard curve;thiocyanate} |