Process Design of Neutralization Pretreatment of In Raffinate AITranslate

Changsha Nonferrous Metallurgical Design Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Based on the analysis of In raffinate composition,three process design proposals are presented for In raffinate neutralization pretreatment. After comparison, 2-stage neutralization is selected. The paper briefly describes the layout and actual effect of the said process.

KeyWords AITranslate

In raffinate neutralization treatment 2-stage neutralization process design

1刘志祥.活性碳吸附法脱除铟萃余液中有机物的探索与实践[J].湖南有色金属,2005,21(3):11-13. 被引量:1

2陈雪云.利用铟萃余液和烟化炉ZnO生产ZnSO_4·7H_2O的试验研究[J].湖南有色金属,2003,19(4):24-26. 被引量:1

1陈吉阳.从湿法炼锌综合回收萃铜余液中脱除有机物的工艺设计[J].世界有色金属,2020(7):21-22.

1丁烯楼.石灰石—石灰乳二段中和法处理矿山酸性废水[J].黑色金属矿山通讯,1992(3):25-26.

2丁希楼,丁春生.石灰石—石灰乳二段中和法处理矿山酸性废水[J].能源环境保护,2004,18(2):27-29. 被引量:32

3郑雅杰,彭映林,李长虹.二段中和法处理酸性矿山废水[J].中南大学学报:自然科学版,2011,42(5):1215-1219. 被引量:30

4宁树才.马钢南山矿酸性废水的治理及改进[J].金属矿山,2000(6):43-44. 被引量:5

5苗雨,刘闻菲,王国胜.乙基氯化物的生产废水处理研究[J].辽宁化工,2009,38(12):843-844. 被引量:2

6谭玉虎,孙戈,刘柏年,俞金山.电催化氧化法处理含氨氮废水及工艺设计方案[J].科技创新与应用,2016,6(34):39-40. 被引量:4

7李建华,张蒙,郜春花,卢朝东.山西省水资源承载力及其可持续利用[J].国土与自然资源研究,2009(1):77-78. 被引量:8

8余良旺,陈祥宏.南方某污水处理厂工程设计与实践[J].水处理技术,2011,37(9):126-128. 被引量:1

9连西美,曾志农.钻井废水酸化中和预处理研究[J].重庆环境科学,1999,21(5):45-46. 被引量:6

10连西美,曾志农.钻井废水酸化中和预处理研究[J].油气田环境保护,2000,10(2):31-32. 被引量:2

Basic Information:

DOI:

Chinese Library Classification Number:X758[环境科学与工程—环境工程]

Citation Information:

Based on the analysis of In raffinate composition,three process design proposals are presented for In raffinate neutralization pretreatment. After comparison, 2-stage neutralization is selected. The paper briefly describes the layout and actual effect of the said process.

quote

GB/T 7714-2015 [1] ZHANG Xiao-lin. Process Design of Neutralization Pretreatment of In Raffinate[J]. Rare Metals and Cemented Carbides, 2007(3): 28-30.
MLA [1] ZHANG Xiao-lin. "Process Design of Neutralization Pretreatment of In Raffinate." Rare Metals and Cemented Carbides, no. 3, 2007, pp. 28-30.
APA [1] ZHANG Xiao-lin. (2007). Process Design of Neutralization Pretreatment of In Raffinate. Rare Metals and Cemented Carbides(3), 28-30.
IEEE [1] ZHANG Xiao-lin, "Process Design of Neutralization Pretreatment of In Raffinate," Rare Metals and Cemented Carbides, no. 3, pp. 28-30, 2007. keywords: {In raffinate;neutralization treatment;2-stage neutralization;process design}