Emerging WS2/WSe2@graphene nanocomposites: synthesis and electrochemical energy storage applications AITranslate
Abstract AITranslate
In recent years, tungsten disulfide(WS2) and tungsten selenide(WSe2) have emerged as favorable electrode materials because of their high theoretical capacity, large interlayer spacing, and high chemical activity;nevertheless, they have relatively low electronic conductivity and undergo large volume expansion during cycling, which greatly hinder them in practical applications. These drawbacks are addressed by combining a superior type of carbon material, graphene, with WS2 and WSe2 to form a WS2/WSe2@graphene nanocomposites.These materials have received considerable attention in electro-chemical energy storage applications such as lithium-ion batteries(LIBs), sodium-ion batteries(SIBs),and supercapacitors. Considering the rapidly growing research enthusiasm on this topic over the past several years, here the recent progress of WS2/WSe2@graphene nanocomposites in electrochemical energy storage applications is summarized. Furthermore, various methods for the synthesis of WS2/WSe2@graphene nanocomposites are reported and the relationships among these methods, nano/microstructures, and electrochemical performance are systematically summarized and discussed. In addition, the challenges and prospects for the future study and application of WS2/WSe2@graphene nanocomposites in electrochemical energy storage applications are proposed.
KeyWords AITranslate
1郭淼,朱晓宇,李茂东,朱俊陆,黄国家,李运勇.静电自组装制备三维石墨烯包覆红磷用于锂离子电池负极材料[J].稀有金属,2022,46(8):1048-1054. 被引量:2
2Ke Meng,La-Mei Zhao,Ning-Yuan Zhang,Zhuang-Fei Zhang,Wei-Xia Shen,Yue-Wen Zhang,Biao Wan,Chao Fang,Liang-Chao Chen,Qian-Qian Wang,Ju-Long He,Xiao-Peng Jia.Thermoelectric properties of n-type SiGe alloys with Sn incorporation[J].Rare Metals,2022,41(12):4156-4163. 被引量:1
3Jin-Bo Wu,Chao Zhen,Gang Liu.Photo-assisted Cl doping of SnO_(2) electron transport layer for hysteresis-less perovskite solar cells with enhanced efficiency[J].Rare Metals,2022,41(2):361-367. 被引量:3
4甘億,王聪,李敬迎,郑俊杰,万厚钊,王浩.水系锌离子电池的稳定性优化策略[J].稀有金属,2022,46(6):753-775. 被引量:6
5Jing-Han Zuo,Peng-Bo Zhai,Qian-Qian He,Lei Wang,Qian Chen,Xiao-Kang Gu,Zhi-Lin Yang,Yong-Ji Gong.In-situ constructed three-dimensional MoS_(2)–MoN heterostructure as the cathode of lithium–sulfur battery[J].Rare Metals,2022,41(5):1743-1752. 被引量:6
6Kaijia Feng,Zhefei Sun,Yong Liu,Feng Tao,Junqing Ma,Han Qian,Renhong Yu,Kunming Pan,Guangxin Wang,Shizhong Wei,Qiaobao Zhang.Shining light on transition metal tungstate-based nanomaterials for electrochemical applications:Structures,progress,and perspectives[J].Nano Research,2022,15(8):6924-6960. 被引量:2
7Limin Zhu,Zhen Li,Guochun Ding,Lingling Xie,Yongxia Miao,Xiaoyu Cao.Review on the recent development of Li_(3)VO_(4)as anode materials for lithium-ion batteries[J].Journal of Materials Science & Technology,2021(30):68-87. 被引量:4
8Ji-Qiu Qi,Meng-Yuan Huang,Chen-Ya Ruan,Dong-Dong Zhu,Lei Zhu,Fu-Xiang Wei,Yan-Wei Sui,Qing-Kun Meng.Construction of CoNi_(2)S_(4) nanocubes interlinked by few-layer Ti_(3)C_(2)T_(x) MXene with high performance for asymmetric supercapacitors[J].Rare Metals,2022,41(12):4116-4126. 被引量:2
9Fei Wang,Yong Liu,Hui-Jie Wei,Teng-Fei Li,Xun-Hui Xiong,Shi-Zhong Wei,Feng-Zhang Ren,Alex A.Volinsky.Recent advances and perspective in metal coordination materialsbased electrode materials for potassium-ion batteries[J].Rare Metals,2021,40(2):448-470. 被引量:9
10Yi-Tian Wang,Xi Chen.Single crystal growth and electrochemical studies of garnet-type fast Li-ion conductors[J].Tungsten,2022,4(4):263-268. 被引量:2
1Francesco Pieri,Gianluca Fiori.Paper-based WS_(2) photodetectors fabricated by all-dry techniques[J].Opto-Electronic Advances,2023,6(11):1-3.
2Yuntao Xiao,Xinfang Zhang,Can Wang,Jinsong Rao,Yuxin Zhang.Recent advances in electrochemical performance of Mg-based electrochemical energy storage materials in supercapacitors:Enhancement and mechanism[J].Journal of Magnesium and Alloys,2024,12(1):35-58.
3Ning Xu,Jiahui Ma,Qi Liu,Yuxin Luo,Yongping Pu.Preparation of CeO_(2) abrasives by reducing atmosphere-assisted molten salt method for enhancing their chemical mechanical polishing performance on SiO_(2)substrates[J].Journal of Rare Earths,2023,41(10):1627-1635. 被引量:1
4Tong Yu,Chunyang Wang,Huicong Yang,Feng Li.Machine learning in metal-ion battery research: Advancing material prediction, characterization, and status evaluation[J].Journal of Energy Chemistry,2024,90(3):191-204.
5Bo-Qiang Miao,Wen-Sheng Fang,Bin Sun,Fu-Min Li,Xiao-Chen Wang,Bao-Yu Xia,Yu Chen.Defect-rich bismuth metallene for efficient CO_(2) electroconversion[J].Chinese Journal of Structural Chemistry,2023,42(8):11-16.
6Longsheng Zhong,Hongneng Chen,Yanzhe Sheng,Yiting Sun,Yanhe Xiao,Baochang Cheng,Shuijin Lei.Two-dimensional layered In_(2)P_(3)S_(9): A novel superior anode material for sodium-ion batteries[J].Journal of Energy Chemistry,2024,90(3):294-304.
7Zhihao Zhang,Danyang Song,Hengxing Bao,Xiang Ling,Xiaogang Jin.Experimental and numerical studies of Ca(OH)_(2)/CaO dehydration process in a fixed-bed reactor for thermochemical energy storage[J].Chinese Journal of Chemical Engineering,2023,62(10):11-20.
8ZHAO LeYi,WANG Hai,LIU TianYu,LI FangFei,ZHOU Qiang,WANG HaiYu.Ultrafast investigation of room temperature valley polarization in“optical bilayer”WS_(2)[J].Science China(Technological Sciences),2024,67(1):91-97.
9Wei Wang.主编寄语[J].汕头大学医学院学报,2024,37(1):1-1.
10Yan Deng,Shuai Feng,Zhiwen Deng,Ye Jia,Xuemei Zhang,Changhaoyue Xu,Sicheng Miao,Meng Yao,Kaipeng Wu,Yun Zhang,Wenlong Cai.Rationalizing Na-ion solvation structure by weakening carbonate solvent coordination ability for high-voltage sodium metal batteries[J].Journal of Energy Chemistry,2023(12):105-113.
Basic Information:
DOI:10.1007/s12598-023-02424-8
Chinese Library Classification Number:TB332[一般工业技术—材料科学与工程];TM912[电气工程—电力电子与电力传动];TM53[电气工程—电器]
Citation Information:
In recent years, tungsten disulfide(WS2) and tungsten selenide(WSe2) have emerged as favorable electrode materials because of their high theoretical capacity, large interlayer spacing, and high chemical activity;nevertheless, they have relatively low electronic conductivity and undergo large volume expansion during cycling, which greatly hinder them in practical applications. These drawbacks are addressed by combining a superior type of carbon material, graphene, with WS2 and WSe2 to form a WS2/WSe2@graphene nanocomposites.These materials have received considerable attention in electro-chemical energy storage applications such as lithium-ion batteries(LIBs), sodium-ion batteries(SIBs),and supercapacitors. Considering the rapidly growing research enthusiasm on this topic over the past several years, here the recent progress of WS2/WSe2@graphene nanocomposites in electrochemical energy storage applications is summarized. Furthermore, various methods for the synthesis of WS2/WSe2@graphene nanocomposites are reported and the relationships among these methods, nano/microstructures, and electrochemical performance are systematically summarized and discussed. In addition, the challenges and prospects for the future study and application of WS2/WSe2@graphene nanocomposites in electrochemical energy storage applications are proposed.
quote
| GB/T 7714-2015 | [1] Yu-Meng Gao, Yong Liu, Kai-Jia Feng, et al. Rare Metals, 2024(1): 1-19. DOI:10.1007/s12598-023-02424-8. |
| MLA | [1] Yu-Meng Gao, et al., Rare Metals, no. 1, 2024, pp. 1-19, https://doi.org/10.1007/s12598-023-02424-8. |
| APA | [1] Yu-Meng Gao, Yong Liu, Kai-Jia Feng, Jun-Qing Ma, Ying-Jie Miao, Bin-Rui Xu, Kun-Ming Pan, Osaka Akiyoshi, Guang-Xin Wang, Ke-Ke Zhang, & Qiao-Bao Zhang. (2024). Rare Metals(1), 1-19. https://doi.org/10.1007/s12598-023-02424-8 |
| IEEE | [1] Yu-Meng Gao, Yong Liu, Kai-Jia Feng, Jun-Qing Ma, Ying-Jie Miao, Bin-Rui Xu, Kun-Ming Pan, Osaka Akiyoshi, Guang-Xin Wang, Ke-Ke Zhang, and Qiao-Bao Zhang, Rare Metals, no. 1, pp. 1-19, 2024, doi: 10.1007/s12598-023-02424-8. |