Study of Mg Reduction for Preparation of Niobium Suboxide New Material for Electrolytic Capacitor Anode AITranslate
Abstract AITranslate
Study is made of the preparation of niobium suboxide by Mg reduction.Niobium Suboxide powder is prepared by mixture grinding-reduction roasting-acid washing for impurity removal-drying.Study is made through XRD and SEM on the product phase and microscopic morphology.Anode is made from niobium suboxide powder with the process similar to that of tantalum electrolytic capacitor.The anode electrical property is tested with anode testing method of electrolytic capacitor.The results showed that Mg reduction process is difficult to control with complex product phase,coarse particle size,simple particle shape.The resultant anode is characterized by low specific capacity,high ESR and high leakage current.
KeyWords AITranslate
1吕义生,冷时铭,刘子文.中国钽电容器工业的进展[J].稀有金属材料与工程,1998,27(1):15-20. 被引量:5
2钟晖,李荐,戴艳阳,钟海云.铌电解电容器最新研究发展动态[J].稀有金属,2002,26(2):139-142. 被引量:10
3Boiko B T,et al.Comparison of the degradation modes in sandwich structures including amorphous oxides of niobium and tantalum[J].Thin Solid Films,1993,229(2):207.
4Fedorenko A I,et al.Layer systems on the base of nitrogen-doped tantalum with enhanced stability[J].Crystal Research and Technology,1997,32(6):843.
5Qiu Yongjian,et al.The stabilization of niobium solid electrolyte capacitors[J].Active and Passive Electronic Components,2002,25(2):201.
6Pozdeev Y.Reliability comparison of tantalum and niobium solid electrolytic capacitors[J].Quality and Reliability Engineering International,1998,14(2):79.
7David R,et al.Binary Alloy Phase Diagrams(Second printiong)[M].US:American society for metals,1987. 1 683.
1李荐,温俊杰,钟海云,易丹青.高能球磨法制备新型电解电容器阳极材料低价铌氧化物工艺研究[J].稀有金属与硬质合金,2005,33(3):4-8. 被引量:2
2李荐,温俊杰,钟海云.铌还原法制备新型电解电容器阳极材料低价铌氧化物工艺研究[J].稀有金属与硬质合金,2006,34(2):21-26.
3英特尔研发出三闸极式电晶体料大幅提升晶片效能[J].电子工程师,2002,28(10):38-38.
4高远,金明亚,曹洪扬.高振实密度低氧铌化物粉体的制备及表征[J].科学技术与工程,2018,18(7):109-112. 被引量:1
1李荐,温俊杰,钟海云.铌还原法制备新型电解电容器阳极材料低价铌氧化物工艺研究[J].稀有金属与硬质合金,2006,34(2):21-26.
2英特尔研发出三闸极式电晶体料大幅提升晶片效能[J].电子工程师,2002,28(10):38-38.
3陈超云,文慧卿,王灿.石墨粉振实密度的测量及其不确定度评定[J].计量技术,2020(7):32-34.
1李荐,温俊杰,钟海云.铌还原法制备新型电解电容器阳极材料低价铌氧化物工艺研究[J].稀有金属与硬质合金,2006,34(2):21-26.
2李荐,易丹青,温俊杰,钟海云.新型电解电容器阳极材料低价铌氧化物的制备[J].中国有色金属学报,2005,15(6):893-899. 被引量:4
3李荐,温俊杰,钟海云,易丹青.高能球磨法制备新型电解电容器阳极材料低价铌氧化物工艺研究[J].稀有金属与硬质合金,2005,33(3):4-8. 被引量:2
4李荐,易丹青,温俊杰,钟晖.NbH还原制备新型电容器阳极材料低价铌氧化物[J].中南大学学报:自然科学版,2006,37(3):461-466.
5Masoudeh Ahmadi,Mohammad Reza Ghasemi,Hassan Hashemipour Rafsanjani.Study of Different Parameters in Ti02 Nanoparticles Formation[J].材料科学与工程:中英文版,2011,5(1):87-93.
6喜琍.电解电容器的可靠性试验及失效分析[J].电子质量,2007(3):31-33. 被引量:2
7左宏,李新芳,刘春明.微量Ga对电容器阳极用铝箔组织及比电容的影响[J].东北大学学报:自然科学版,2013,34(10):1400-1403. 被引量:2
8铌电解电容器将成替代品[J].国际电子变压器,2005(5).
9江国健,徐家跃,庄汉锐,李文兰.Na_2B_4O_7+Mg+C体系燃烧合成B_4C及其反应机理[J].硅酸盐学报,2009,37(10):1634-1638.
10Jingbo SONG,Weimin MAO,Hong YANG,Huiping FENG.Effect of Trace Sn on Pitting Behaviors of High Voltage Anode Aluminum Foil[J].材料科学技术:英文版,2008,24(5):718-722. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TB34[一般工业技术—材料科学与工程]
Citation Information:
Study is made of the preparation of niobium suboxide by Mg reduction.Niobium Suboxide powder is prepared by mixture grinding-reduction roasting-acid washing for impurity removal-drying.Study is made through XRD and SEM on the product phase and microscopic morphology.Anode is made from niobium suboxide powder with the process similar to that of tantalum electrolytic capacitor.The anode electrical property is tested with anode testing method of electrolytic capacitor.The results showed that Mg reduction process is difficult to control with complex product phase,coarse particle size,simple particle shape.The resultant anode is characterized by low specific capacity,high ESR and high leakage current.
quote
| GB/T 7714-2015 | [1] LI Jian, WEN Jun-jie, ZHONG Hai-yun. Study of Mg Reduction for Preparation of Niobium Suboxide New Material for Electrolytic Capacitor Anode[J]. Rare Metals and Cemented Carbides, 2005(2): 19-22. |
| MLA | [1] LI Jian, et al., "Study of Mg Reduction for Preparation of Niobium Suboxide New Material for Electrolytic Capacitor Anode." Rare Metals and Cemented Carbides, no. 2, 2005, pp. 19-22. |
| APA | [1] LI Jian, WEN Jun-jie, & ZHONG Hai-yun. (2005). Study of Mg Reduction for Preparation of Niobium Suboxide New Material for Electrolytic Capacitor Anode. Rare Metals and Cemented Carbides(2), 19-22. |
| IEEE | [1] LI Jian, WEN Jun-jie, and ZHONG Hai-yun, "Study of Mg Reduction for Preparation of Niobium Suboxide New Material for Electrolytic Capacitor Anode," Rare Metals and Cemented Carbides, no. 2, pp. 19-22, 2005. keywords: {niobium suboxide;Mg reduction;preparation;electrolytic capacitor anode;electrical property} |