daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Research Status and Development Trend of Bismuth Metallurgical Technology AITranslate

CINF Engineering Co.,Ltd.;CINF Engineering Co.,Ltd.;CINF Engineering Co.,Ltd.;CINF Engineering Co.,Ltd.;CINF Engineering Co.,Ltd.
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The research status and development trend of bismuth pyrometallurgical and hydrometallurgical processes are reviewed.The characteristics,application scope and existing problems of bismuth metallurgical process in the research stage and industrial production practice are clarified.A method for extracting bismuth from bismuth sulfide concentrates by oxygen pressure leaching with methanesulfonic acid as the leaching agent is proposed.This method has the advantages of high bismuth leaching rate,ittle corrosiveness to the reactor,and no SO emission in the process,and has a good development prospect.

KeyWords AITranslate

bismuth pyrometallurgy hydrometallurgy oxygen pressure leaching research status development trend

1陈永明,叶龙刚,唐朝波,杨声海,唐谟堂,张文海.锑在Na_2CO_3-NaCl二元熔盐中的溶解度(英文)[J].中国有色金属学报:英文版,2015,25(9):3146-3151. 被引量:1

2胡宇杰,唐朝波,唐谟堂,陈永明.再生铅低温碱性固硫熔炼的实验研究[J].工程科学学报,2015,37(5):588-594. 被引量:10

3郭学益,刘静欣,田庆华,李栋.有色金属复杂资源低温碱性熔炼原理与方法[J].有色金属科学与工程,2013,4(2):8-13. 被引量:28

4熊德强,肖金娥.从金银冶炼氧化渣中回收铋的生产实践[J].贵金属,2005,26(2):16-20. 被引量:4

5谢祥贵.铋矿浆电解实践[J].湖南有色金属,1999,15(6):28-30. 被引量:3

6周晓源,张自军.湖南柿竹园铋冶炼改扩建工艺设计[J].有色金属,2007,59(3):75-79. 被引量:7

7唐朝波,刘永,叶龙刚,陈永明,唐谟堂,杨声海.硫化铋精矿还原造锍熔炼一步炼铋[J].中国有色金属学报,2017,27(2):363-370. 被引量:3

8王继峰,李静,杨建广.用隔膜电积法从辉铋矿精矿中回收铋[J].湿法冶金,2012,31(1):45-48. 被引量:7

9王成彦,邱定蕃,张寅生,江培海.矿浆电解法处理铋精矿的研究[J].有色金属,1995,47(3):55-60. 被引量:14

10唐谟堂,鲁君乐,晏德生,韦元基,贺青蒲,袁延胜.新氯化-水解法处理大厂脆硫锑铅矿精矿[J].有色金属:冶炼部分,1991(5):20-22. 被引量:14

1吴苏喜,周东蓉,王彦心,黄艳慧,李普选,李昌珠.高品质油茶籽油的湿法提取工艺优化[J].中国油脂,2022,47(4):19-23. 被引量:3

2沈楼燕,欧阳涛,胡申琛.浅析非洲某尾矿湿法铜钴项目电积剥片机组改造与升级[J].世界有色金属,2022(10):53-55.

3何鲨,邱兆富,单兆阳,杨骥,金锡标.P204-P507-HCl体系回收废FCC催化剂中稀土的优化[J].环境工程学报,2022,16(7):2317-2325.

4何德文,李俊杰,周康根,陈伟,龚丹丹.白钨矿焙烧转料的氢氧化钠浸出动力学研究[J].稀有金属,2022,46(7):926-934.

Basic Information:

DOI:

Chinese Library Classification Number:TF817[冶金工程—有色金属冶金]

Citation Information:

The research status and development trend of bismuth pyrometallurgical and hydrometallurgical processes are reviewed.The characteristics,application scope and existing problems of bismuth metallurgical process in the research stage and industrial production practice are clarified.A method for extracting bismuth from bismuth sulfide concentrates by oxygen pressure leaching with methanesulfonic acid as the leaching agent is proposed.This method has the advantages of high bismuth leaching rate,ittle corrosiveness to the reactor,and no SO emission in the process,and has a good development prospect.

quote

GB/T 7714-2015 [1] WANG Heng-hui, CHEN Yong-min, CHANG Cong, et al. Research Status and Development Trend of Bismuth Metallurgical Technology[J]. Rare Metals and Cemented Carbides, 2022(4): 33-38.
MLA [1] WANG Heng-hui, et al., "Research Status and Development Trend of Bismuth Metallurgical Technology." Rare Metals and Cemented Carbides, no. 4, 2022, pp. 33-38.
APA [1] WANG Heng-hui, CHEN Yong-min, CHANG Cong, ZHOU Xiao-yuan, & YANG Sheng-hai. (2022). Research Status and Development Trend of Bismuth Metallurgical Technology. Rare Metals and Cemented Carbides(4), 33-38.
IEEE [1] WANG Heng-hui, CHEN Yong-min, CHANG Cong, ZHOU Xiao-yuan, and YANG Sheng-hai, "Research Status and Development Trend of Bismuth Metallurgical Technology," Rare Metals and Cemented Carbides, no. 4, pp. 33-38, 2022. keywords: {bismuth;pyrometallurgy;hydrometallurgy;oxygen pressure leaching;research status;development trend}