Experimental Study on Extraction of Gallium from Sulfuric Acid Leaching Solution of Coal Gangue by Using P507 AITranslate
Abstract AITranslate
Gallium and iron from sulfuric acid leaching solution of coal gangue were separated by extraction with 2-ethylhexyl phosphate mono-2-ethylhexyl ester(P507).The effects of solution pH value,P507 concentration,oscillation time,oscillation intensity and extraction temperature on the extraction efficiency of gallium and iron were investigated.The results show that the single-stage extraction rate of Ga3+reaches 82%while that of Fe2+is lower than 18%,under the conditions of A/O ratio of 1:1,P507 concentration of 20%,solution pH value of 1.5,oscillation time of 15 min,oscillation intensity of 200 r/min and extraction temperature of 35℃.The extraction experiments were performed by changing the A/O ratio,and then the equilibrium isotherm of gallium extraction was determined.Under the condition of 4:1 A/O ratio,the theoretical extraction stage of gallium is four,and the extraction rate of gallium is 98.4%while the extraction rate of iron is 17.4%,and the extraction rate of other metal ions is less than 10%.Therefore,the selective extraction of gallium from sulfuric acid leaching solution of coal gangue could be realized.
KeyWords AITranslate
1朱晓波,王涛,李望.醋酸浸出赤泥及P507萃取浸出液回收钇的实验研究[J].工程科学与技术,2021,53(4):240-246. 被引量:1
2王海涛,王文宝,华南平.紫外分光光度法间接测定铁的价态[J].光谱实验室,2004,21(6):1047-1050. 被引量:4
3Xiaobo Zhu,Wang Li,Baolin Xing,Yude Zhang.Extraction of scandium from red mud by acid leaching with CaF2 and solvent extraction with P507[J].稀土学报:英文版,2020,38(9):1003-1008. 被引量:10
4张魁芳,刘志强.用P507从硫酸体系中萃取分离镓与铁锌离子[J].过程工程学报,2014,14(3):427-432. 被引量:6
5刘凯华.用P204从硫酸体系中萃取分离铟镓[J].湿法冶金,2021,40(5):386-389. 被引量:4
6丘丽莉,张魁芳,刘志强,王瑞祥,陈金清,钟晓聪,袁祥奕.硫酸体系中Cyanex272的萃镓性能研究[J].有色金属:冶炼部分,2021(5):86-91. 被引量:2
7李超,王丽萍,郭昭华,王永旺,陈东.盐酸体系下镓的提取技术研究进展[J].稀有金属与硬质合金,2019,47(1):6-10. 被引量:7
8廖亚龙,曹磊,王祎洋,叶朝.溶液中镓的提取与分离研究进展[J].材料导报,2017,31(15):133-138. 被引量:5
9黄中省.富镓物中镓的浸出、分离试验研究[J].稀有金属与硬质合金,2016,44(4):5-10. 被引量:2
10刘有才,李丽峰,符剑刚,刘悟辉,王晖.高铝高镓煤矸石的综合利用[J].广东化工,2009,36(7):137-138. 被引量:6
1甘胤,禄瑜.利用煤矸石提取有价元素技术的研究进展[J].煤炭加工与综合利用,2023(5):85-91.
2康超,乔金鹏,杨胜超,彭超,付元鹏,刘斌,刘建荣,Tatiana Aleksandrova,段晨龙.煤矸石中有价关键金属活化提取研究进展[J].化工学报,2023,74(7):2783-2799.
1裴亮,廖晓勇,马栋.组合液膜对土壤淋洗液中砷(As)的提取效果[J].环境化学,2018,37(9):2002-2007. 被引量:1
2李瑞琛,马岗岥,张龙升,赵京阳,高艳芳.高效离心萃取机处理含巯基丙酸废水的性能研究[J].工业用水与废水,2022,53(4):34-36.
3冯艳红,应蓉蓉,王国庆,张亚,杜俊洋,林玉锁.中国中西部地区土壤和农产品中邻苯二甲酸酯污染特征及评价[J].环境化学,2022,41(5):1591-1602. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TF843.1[冶金工程—有色金属冶金]
Citation Information:
Gallium and iron from sulfuric acid leaching solution of coal gangue were separated by extraction with 2-ethylhexyl phosphate mono-2-ethylhexyl ester(P507).The effects of solution pH value,P507 concentration,oscillation time,oscillation intensity and extraction temperature on the extraction efficiency of gallium and iron were investigated.The results show that the single-stage extraction rate of Ga3+reaches 82%while that of Fe2+is lower than 18%,under the conditions of A/O ratio of 1:1,P507 concentration of 20%,solution pH value of 1.5,oscillation time of 15 min,oscillation intensity of 200 r/min and extraction temperature of 35℃.The extraction experiments were performed by changing the A/O ratio,and then the equilibrium isotherm of gallium extraction was determined.Under the condition of 4:1 A/O ratio,the theoretical extraction stage of gallium is four,and the extraction rate of gallium is 98.4%while the extraction rate of iron is 17.4%,and the extraction rate of other metal ions is less than 10%.Therefore,the selective extraction of gallium from sulfuric acid leaching solution of coal gangue could be realized.
quote
| GB/T 7714-2015 | [1] GUO Wen-chao, LI Wang, ZHU Xiao-bo, et al. Experimental Study on Extraction of Gallium from Sulfuric Acid Leaching Solution of Coal Gangue by Using P507[J]. Rare Metals and Cemented Carbides, 2022(4): 28-32. |
| MLA | [1] GUO Wen-chao, et al., "Experimental Study on Extraction of Gallium from Sulfuric Acid Leaching Solution of Coal Gangue by Using P507." Rare Metals and Cemented Carbides, no. 4, 2022, pp. 28-32. |
| APA | [1] GUO Wen-chao, LI Wang, ZHU Xiao-bo, ZHANG Zhi-guo, & ZHANG Chuan-xiang. (2022). Experimental Study on Extraction of Gallium from Sulfuric Acid Leaching Solution of Coal Gangue by Using P507. Rare Metals and Cemented Carbides(4), 28-32. |
| IEEE | [1] GUO Wen-chao, LI Wang, ZHU Xiao-bo, ZHANG Zhi-guo, and ZHANG Chuan-xiang, "Experimental Study on Extraction of Gallium from Sulfuric Acid Leaching Solution of Coal Gangue by Using P507," Rare Metals and Cemented Carbides, no. 4, pp. 28-32, 2022. keywords: {gallium;extraction;P507;coal gangue;leaching solution;iron} |