Effects of Carbon Ion Irradiation on Microstructure and Surface Hardness of Pure Tungsten AITranslate
Abstract AITranslate
The effects of carbon ion irradiation at 7oo C on the surface morphology,microstructure and surface hardness of pure tungsten were studied by scanning electron microscopy,transmission electron microscopy and nanoindenter.The results show that carbon ion irradiation can lead to irradiated pits on the surface of the samples,and the size of the pits increases with the increase of irradiation dose.Carbon ion irradiation produces a large number of dislocation loops inside the sample,and the size and number density of the loops increase with the increase of radiation dose.Also,carbon ion irradiation causes a severe irradiation hardening effect on the tungsten surface,and the surface hardness of the samples increases significantly with the increases of irradiation dose.The average hardness of the tungsten surface reaches 15.85 GPa when the irradiation dose reaches 8.0 dpa.The dislocation loops generated by irradiation are the main cause of the irradiation hardening.
KeyWords AITranslate
1张德根,邹俊峰,赵敏福.离子溅射能量损失及射程的模拟研究[J].巢湖学院学报,2009,11(6):37-41. 被引量:1
2刘晓,马纪敏,郭海兵.混合堆第一壁中子辐照损伤模拟[J].强激光与粒子束,2015,27(1):250-253. 被引量:3
3罗来马,施静,昝祥,李萍,罗广南,陈俊凌,吴玉程.掺杂合金元素面向等离子体钨基材料的研究现状与发展趋势[J].中国有色金属学报,2016,26(9):1899-1911. 被引量:10
1杨宗辉,沈以赴,张旭,李晓泉,成家林,初雅杰.基于W-Fe-Cr混合粉末中间层的钨/钢连接研究[J].稀有金属与硬质合金,2022,50(4):46-50.
2吕源远,岳赟,杜志浩,杜三明,倪锋,张永振.不同温度低压真空渗氮对新型TiZr基合金微观组织及摩擦学性能的影响[J].材料导报,2022,36(17):163-169. 被引量:2
3耶曼,李婧,马怡飞,柯艳,李小桂.高频红外碳硫仪快速测定镍铅锌矿石中的硫含量[J].岩矿测试,2022,41(4):680-687. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TG146.411[金属学及工艺—金属材料]
Citation Information:
The effects of carbon ion irradiation at 7oo C on the surface morphology,microstructure and surface hardness of pure tungsten were studied by scanning electron microscopy,transmission electron microscopy and nanoindenter.The results show that carbon ion irradiation can lead to irradiated pits on the surface of the samples,and the size of the pits increases with the increase of irradiation dose.Carbon ion irradiation produces a large number of dislocation loops inside the sample,and the size and number density of the loops increase with the increase of radiation dose.Also,carbon ion irradiation causes a severe irradiation hardening effect on the tungsten surface,and the surface hardness of the samples increases significantly with the increases of irradiation dose.The average hardness of the tungsten surface reaches 15.85 GPa when the irradiation dose reaches 8.0 dpa.The dislocation loops generated by irradiation are the main cause of the irradiation hardening.
quote
| GB/T 7714-2015 | [1] LUO Chun yang, CUI Bo, XU Liu-jie, et al. Effects of Carbon Ion Irradiation on Microstructure and Surface Hardness of Pure Tungsten[J]. Rare Metals and Cemented Carbides, 2022(4): 39-45. |
| MLA | [1] LUO Chun yang, et al., "Effects of Carbon Ion Irradiation on Microstructure and Surface Hardness of Pure Tungsten." Rare Metals and Cemented Carbides, no. 4, 2022, pp. 39-45. |
| APA | [1] LUO Chun yang, CUI Bo, XU Liu-jie, SHEN Hua-hai, ZONG Le, ZHOU Xiao-song, & WEI Shi-zhong. (2022). Effects of Carbon Ion Irradiation on Microstructure and Surface Hardness of Pure Tungsten. Rare Metals and Cemented Carbides(4), 39-45. |
| IEEE | [1] LUO Chun yang, CUI Bo, XU Liu-jie, SHEN Hua-hai, ZONG Le, ZHOU Xiao-song, and WEI Shi-zhong, "Effects of Carbon Ion Irradiation on Microstructure and Surface Hardness of Pure Tungsten," Rare Metals and Cemented Carbides, no. 4, pp. 39-45, 2022. keywords: {tungsten;carbon ion irradiation;surface morphology;microstructure;dislocation loop;irradiation hardening;hardness} |