Effect of Cu Content on Microstructure and Mechanical Properties of Porous Ti-5Mn Alloys AITranslate
Abstract AITranslate
Porous Ti-5Mn-xCu(x=0,3,5,10)alloys were prepared by powder metallurgy process with va-cuum sintering using 50%ammonium bicarbonate particles as pore-forming agent,and the effects of Cu content on the microstructure and mechanical properties of porous Ti-5Mn alloys were investigated.The results show that the porosity of the prepared porous Ti-Mn-Cu alloys gradually decreases with increasing Cu content.The macropore diameter slightly reduces,and the number of micropores on the walls of the macropores also decreases gradually.The Ti2Cu phase appears in the porous Ti-Mn-Cu alloys,with its relative amount increasing gradually with the rise in Cu content.The elastic modulus and compressive strength of porous Ti-Mn-Cu alloys increase accordingly with the increase of Cu content.Porous Ti-Mn-Cu alloys containing 3%~10%Cu and 5%Mn exhibit appropriate pore structures and mechanical properties similar to human bone,showing the potential as antibacterial orthopedic implant materials.
KeyWords AITranslate
1郭春会,黄雨欣,唐柏彬,袁腾港,张进忠.负载多壁碳纳米管的Ti/SnO_(2)-Sb-Ni电极电催化降解水中左氧氟沙星[J].环境科学学报,2024,44(1):242-251.
2朱绍林,孙明慧,刘湛,余申,吕佳敏,李小云,陈丽华.原位晶化法合成大孔-微孔MFI型分子筛[J].应用化工,2024,53(1):25-30.
Basic Information:
DOI:
Chinese Library Classification Number:TG146.23[金属学及工艺—金属材料]
Citation Information:
Porous Ti-5Mn-xCu(x=0,3,5,10)alloys were prepared by powder metallurgy process with va-cuum sintering using 50%ammonium bicarbonate particles as pore-forming agent,and the effects of Cu content on the microstructure and mechanical properties of porous Ti-5Mn alloys were investigated.The results show that the porosity of the prepared porous Ti-Mn-Cu alloys gradually decreases with increasing Cu content.The macropore diameter slightly reduces,and the number of micropores on the walls of the macropores also decreases gradually.The Ti2Cu phase appears in the porous Ti-Mn-Cu alloys,with its relative amount increasing gradually with the rise in Cu content.The elastic modulus and compressive strength of porous Ti-Mn-Cu alloys increase accordingly with the increase of Cu content.Porous Ti-Mn-Cu alloys containing 3%~10%Cu and 5%Mn exhibit appropriate pore structures and mechanical properties similar to human bone,showing the potential as antibacterial orthopedic implant materials.
quote
| GB/T 7714-2015 | [1] ZHAO Chao-yong, WU Cai-hong, MAI Ping. Effect of Cu Content on Microstructure and Mechanical Properties of Porous Ti-5Mn Alloys[J]. Rare Metals and Cemented Carbides, 2024(1): 57-62. |
| MLA | [1] ZHAO Chao-yong, et al., "Effect of Cu Content on Microstructure and Mechanical Properties of Porous Ti-5Mn Alloys." Rare Metals and Cemented Carbides, no. 1, 2024, pp. 57-62. |
| APA | [1] ZHAO Chao-yong, WU Cai-hong, & MAI Ping. (2024). Effect of Cu Content on Microstructure and Mechanical Properties of Porous Ti-5Mn Alloys. Rare Metals and Cemented Carbides(1), 57-62. |
| IEEE | [1] ZHAO Chao-yong, WU Cai-hong, and MAI Ping, "Effect of Cu Content on Microstructure and Mechanical Properties of Porous Ti-5Mn Alloys," Rare Metals and Cemented Carbides, no. 1, pp. 57-62, 2024. keywords: {porousti tanium alloy;Ti-Mn-Cu;ammonium bicarbonate;antibacterial property;bone repair ma-terial;powder metallurgy} |