daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study on Effect of Pressing Pressure on Microstructure and Mechanical Properties of Nano Ti(C,N)-Based Cermet AITranslate

College of Mechanical Engineering,Sichuan University of Science and Technology;College of Mechanical Engineering,Sichuan University of Science and Technology;College of Mechanical Engineering,Sichuan University of Science and Technology;College of Mechanical Engineering,Sichuan University of Science and Technology;College of Mechanical Engineering,Sichuan University of Science and Technology;College of Mechanical Engineering,Sichuan University of Science and Technology;College of Mechanical Engineering,Sichuan University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Nano Ti(C,N)-based green cermet was prepared with different pressing pressures to study the microstructure,shrinkage,and mechanical properties of the cermet after low-pressure sintering.The results show that with the extremely low pressing pressure,the powder arrangement is not tight and the microstructure of the cermet is uneven.And with the extremely high pressing pressure,the microstructure of the cermet is layered,and the porosity and defects are increased.When the pressing pressure is 180 MPa,the obtained nano Ti(C,N)-based cermet exhibits the highest density,with a relative density of 97.06%,a shrinkage coefficient of 1.23,and the lowest porosity of A02B00C00.Simultaneously,the cermet presents the best comprehensive mechanical properties,with a Vickers hardness of 1680 HV30,a flexural strength of 1650 MPa,and a fracture toughness of 8.8 MPa·m1/2.

KeyWords AITranslate

nano Ti(C N)-based cermet pressing pressure low-pressure sintering microstructure shrin-kage mechanical property

1黄绍锋,甘志伟,胡宁飞,陆静,李东旭.核壳结构SiC@Ti(C,N)复合材料的制备及性能研究[J].表面技术,2023,52(4):410-416.

2黄祥,张立,聂仁鑫,钟志强,徐涛,朱骥飞.异质结构Ti(C,N)-(Fe)CoCrNi基金属陶瓷及其电化学腐蚀行为[J].硬质合金,2024,41(1):43-53.

3黄晗晔,郭雪萍,徐佳微,李倩倩,蔡鑫铠,关雄,潘晓鸿.纳米TiO_(2)负载盐酸莫西沙星体系的构建及其抗菌效果评价[J].农业生物技术学报,2024,32(2):484-492.

4刘云鹏,余海洲,刘文俊,曹攀.N_(2)分压烧结时间对超细晶粒Ti(C,N)基金属陶瓷组织和力学性能的影响[J].硬质合金,2024,41(1):37-42.

5龙航飞,叶金文,曹之南.(Cr,La)_(2)(C,N)添加对Ti(C,N)基金属陶瓷结构与性能的影响[J].粉末冶金技术,2024,42(1):45-52.

6桂子顺,李延凤,刘文俊,余海洲.Fe-44.4%Mo-4.9%B-2.5%Cr-2.9%Ni金属陶瓷烧结阶段晶粒生长机理[J].硬质合金,2024,41(1):20-27.

7张金伟,张曼,赵奔奔,刘杰胜,彭浩,谭晓明.Nb添加量对金属陶瓷显微组织和磁学性能的影响[J].有色金属工程,2024,14(2):9-16.

8刘洋,王明登,徐国忠,郑亚杰,李超,钟祥云,刘洋,白金锋.炼焦煤热解收缩特性对焦炭成块性能影响[J].煤炭学报,2023,48(11):4183-4191.

9吕涛,刘芳,刘畅,董德秀,张伟红,蔡桂喜.GH907合金机匣锻环的超声衰减性能与其组织的关系[J].材料研究学报,2024,38(1):14-22.

10毛献昌,易幼平,黄始全,何海林.多向锻造变形温度对2219铝合金微观组织和力学性能的影响[J].机械工程学报,2023,59(22):275-286.

Basic Information:

DOI:

Chinese Library Classification Number:TG148[金属学及工艺—金属材料]

Citation Information:

Nano Ti(C,N)-based green cermet was prepared with different pressing pressures to study the microstructure,shrinkage,and mechanical properties of the cermet after low-pressure sintering.The results show that with the extremely low pressing pressure,the powder arrangement is not tight and the microstructure of the cermet is uneven.And with the extremely high pressing pressure,the microstructure of the cermet is layered,and the porosity and defects are increased.When the pressing pressure is 180 MPa,the obtained nano Ti(C,N)-based cermet exhibits the highest density,with a relative density of 97.06%,a shrinkage coefficient of 1.23,and the lowest porosity of A02B00C00.Simultaneously,the cermet presents the best comprehensive mechanical properties,with a Vickers hardness of 1680 HV30,a flexural strength of 1650 MPa,and a fracture toughness of 8.8 MPa·m1/2.

quote

GB/T 7714-2015 [1] HE Feng-yuan, ZHANG Wen-ke, XIONG Xiao, et al. Study on Effect of Pressing Pressure on Microstructure and Mechanical Properties of Nano Ti(C,N)-Based Cermet[J]. Rare Metals and Cemented Carbides, 2024(1): 51-56.
MLA [1] HE Feng-yuan, et al., "Study on Effect of Pressing Pressure on Microstructure and Mechanical Properties of Nano Ti(C,N)-Based Cermet." Rare Metals and Cemented Carbides, no. 1, 2024, pp. 51-56.
APA [1] HE Feng-yuan, ZHANG Wen-ke, XIONG Xiao, CHEN Xin-hui, XIONG Jian-song, DONG Ding-qian, & LI Hui. (2024). Study on Effect of Pressing Pressure on Microstructure and Mechanical Properties of Nano Ti(C,N)-Based Cermet. Rare Metals and Cemented Carbides(1), 51-56.
IEEE [1] HE Feng-yuan, ZHANG Wen-ke, XIONG Xiao, CHEN Xin-hui, XIONG Jian-song, DONG Ding-qian, and LI Hui, "Study on Effect of Pressing Pressure on Microstructure and Mechanical Properties of Nano Ti(C,N)-Based Cermet," Rare Metals and Cemented Carbides, no. 1, pp. 51-56, 2024. keywords: {nano Ti(C,N)-based cermet;pressing pressure;low-pressure sintering;microstructure;shrin-kage;mechanical property}