Effects of Combined Addition of Sc and Zr on Microstructure and Mechanical Properties of ZL 114A Alloy AITranslate

AECC Beijing Institute of Aeronautical Materials;AECC Beijing Institute of Aeronautical Materials;AECC Beijing Institute of Aeronautical Materials;AECC Beijing Institute of Aeronautical Materials;AECC Beijing Institute of Aeronautical Materials;AECC Beijing Institute of Aeronautical Materials
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The effects of the combined addition of Sc and Zr on the microstructure and mechanical properties of ZL114A alloy were studied by polarized light microscope,DSC,SEM and Vickers hardness tester.The results show that for ZLll4A alloy with Al-Ti-B grain refinement,the nucleation temperature of primaryα-Al grains increases from 619.2 C to 621.6 C after the combined addition of Sc and Zr,and the number of nucleation cores also increases.The nucleation ofα-Al grains becomes easier and the grains are further refined,of which the size decreases by 9.8%from 319.2μm to 287.8μm.The combined addition of Sc and Zr has little effect on the eutectic Si of ZLll4A alloy,indicating that the change in mechanical properties of ZLl14A+Sc+Zr alloy is mainly attributed to the change in the size of primaryα-Al grains.After the combined addition of Sc and Zr,the hardness of ZL1l4A alloy increases due to grain refinement.

KeyWords AITranslate

ZL114A alloy combined addition Sc Zr primaryα-Al grain eutectic Si hardness

1魏作山,丁海民,孙晓,王娜娜,王丽艳.Sc、Zr联合作用对Al-Si合金组织和性能的影响[J].特种铸造及有色合金,2012,32(12):1171-1174. 被引量:4

2郭震,陈文琳.固溶处理对Al-13.0Si-4.5Cu-1.0Mg-2.0Ni合金组织和性能的影响[J].铸造,2017,66(3):273-276. 被引量:6

3康福伟,李如一,乔昕,张继敏,樊德智.热处理工艺对ZL114A铝合金组织及力学性能的影响[J].哈尔滨理工大学学报,2019,24(1):113-117. 被引量:12

4何兵,覃铭,兰旅.热处理对A356铝合金组织与性能的影响[J].长春工业大学学报,2015,36(6):617-625. 被引量:7

5曹丽云,陈淑英,王建中.Al-Si合金在汽车工业中的应用前景及研究现状[J].辽宁工学院学报,2000,20(4):1-3. 被引量:18

6熊梅.热处理对Al-12Si建筑储能材料性能的影响分析[J].热加工工艺,2014,43(20):149-151. 被引量:4

1仲崇宇,房灿峰,王蓉,冯杰涛,尹家新,王德清,羌建兵,王英敏.ZL114A合金的双级固溶处理工艺研究[J].稀有金属材料与工程,2022,51(12):4788-4792.

2吕长生,王立权,伊俊振.激光沉积制造SiC/ZL114A复合材料组织及力学性能研究[J].哈尔滨工程大学学报,2023,44(4):615-621.

3祝捷,王培卿,薛彦庆,陈易山,张晗,郝启堂,李新雷.5 mass%TiB_(2)/Al-4.5Cu-xSc-yZr复合材料的微观组织和力学性能[J].材料热处理学报,2023,44(3):41-51.

4覃明路,王利春.体育器材铝基复合材料微观组织及性能研究[J].精密成形工程,2023,15(3):47-54. 被引量:1

5蔡春波,高少伟,高桂丽,石德全.脉冲电流对Al-Cu-Mn-Zr合金时效处理组织及性能的影响[J].金属热处理,2023,48(4):104-110. 被引量:1

6李振,韩维娜,王晓民,赫丽杰,郭丽莉,张全庆,薛亮,张淼,卢伟.Y对再生A356铝合金凝固组织及力学性能的影响[J].铸造,2023,72(3):275-281.

7Zhi-qiang Chen,Wen-xin Hu,Lei Shi,Wei Wang.Effect of rare earth on morphology and dispersion of TiB2 phase in Al-Ti-B alloy refiner[J].中国铸造:英文版,2023,20(2):115-124.

8薛超,杜江雪,叶树鑫,任煜,刘婉婉.基于液态金属的可拉伸导电织物制备及性能[J].上海纺织科技,2023,51(3):50-54.

9沈志远,杜玉栋,张浩,李小燕,胡燕峰,张奇,罗发亮.HPN-68L成核剂对顺丁橡胶增韧PP材料结晶行为和力学性能的影响[J].塑料工业,2023,51(4):143-148.

10李星,陈义胜,闫永旺.镧-铈添加下A356铝合金组织性能及力学特性[J].天津化工,2023,37(2):55-59.

Basic Information:

DOI:

Chinese Library Classification Number:TG146.21[金属学及工艺—金属材料]

Citation Information:

The effects of the combined addition of Sc and Zr on the microstructure and mechanical properties of ZL114A alloy were studied by polarized light microscope,DSC,SEM and Vickers hardness tester.The results show that for ZLll4A alloy with Al-Ti-B grain refinement,the nucleation temperature of primaryα-Al grains increases from 619.2 C to 621.6 C after the combined addition of Sc and Zr,and the number of nucleation cores also increases.The nucleation ofα-Al grains becomes easier and the grains are further refined,of which the size decreases by 9.8%from 319.2μm to 287.8μm.The combined addition of Sc and Zr has little effect on the eutectic Si of ZLll4A alloy,indicating that the change in mechanical properties of ZLl14A+Sc+Zr alloy is mainly attributed to the change in the size of primaryα-Al grains.After the combined addition of Sc and Zr,the hardness of ZL1l4A alloy increases due to grain refinement.

quote

GB/T 7714-2015 [1] LIU Shan-guang, DONG Ming-hui, ZHANG Wei, et al. Effects of Combined Addition of Sc and Zr on Microstructure and Mechanical Properties of ZL 114A Alloy[J]. Rare Metals and Cemented Carbides, 2023(2): 49-53.
MLA [1] LIU Shan-guang, et al., "Effects of Combined Addition of Sc and Zr on Microstructure and Mechanical Properties of ZL 114A Alloy." Rare Metals and Cemented Carbides, no. 2, 2023, pp. 49-53.
APA [1] LIU Shan-guang, DONG Ming-hui, ZHANG Wei, LI Da-kui, MAO Guo-ling, & GAO Wen-li. (2023). Effects of Combined Addition of Sc and Zr on Microstructure and Mechanical Properties of ZL 114A Alloy. Rare Metals and Cemented Carbides(2), 49-53.
IEEE [1] LIU Shan-guang, DONG Ming-hui, ZHANG Wei, LI Da-kui, MAO Guo-ling, and GAO Wen-li, "Effects of Combined Addition of Sc and Zr on Microstructure and Mechanical Properties of ZL 114A Alloy," Rare Metals and Cemented Carbides, no. 2, pp. 49-53, 2023. keywords: {ZL114A alloy;combined addition;Sc;Zr;primaryα-Al grain;eutectic Si;hardness}