daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Research Progress of Molybdenum Coating Prepared by Electrodeposition AITranslate

College of Aerospace and Engineering,National University of Defense Technology;College of Aerospace and Engineering,National University of Defense Technology;College of Aerospace and Engineering,National University of Defense Technology;College of Aerospace and Engineering,National University of Defense Technology;College of Aerospace and Engineering,National University of Defense Technology;College of Aerospace and Engineering,National University of Defense Technology;College of Aerospace and Engineering,National University of Defense Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Due to its excellent physicochemical properties of high strength at high temperature,good corrosion resistance,and strong radiation resistance,molybdenum coating has promising application prospects in metallurgy,aerospace,and nuclear industry.This paper reviews the main preparation methods of the molybdenum coating,including thermal spraying,physical vapor deposition and electrodeposition,and compares the advantages and disadvantages of different methods.In addition,the research status of the electrodeposition of the molybdenum coating in molten salt and aqueous solution is emphasized.The comparisons of the effects of active salt,support electrolyte,and additives on molten salt electrodeposition and molybdenum coating quality are also conducted.At present,the molybdenum coating prepared in molybdate-fluoride-oxide molten salt system has the best comprehensive performance.Aqueous solution electrodeposition has low preparation temperature and wide applicability,but it faces the difficulty of restraining hydrogen evolution and the problem of MoO42-being sensitive to pH value,resulting in weak bonding between the molybdenum coating and the interface.

KeyWords AITranslate

molybdenum coating electrodeposition molten salt aqueous solution support electrolyte molybdate research progress

1杨慧玲,丁晶晶,江奕东,凌国平.钼在[BMP]Tf_2N离子液体中的低温电沉积[J].稀有金属材料与工程,2018,47(5):1523-1528. 被引量:2

2邢开源,汪欣,李争显,杜继红,耿娟娟.钼及其合金表面改性MoSi_2涂层研究进展[J].材料保护,2018,51(12):104-111. 被引量:7

3邱永红,姜宇飞,李烊,刘科鑫.轨道交通车轴喷钼技术攻关[J].金属加工:热加工,2022(1):25-29. 被引量:1

4刘贵民,杨忠须,张一帆,闫涛,魏敏.基于正交试验法的超音速等离子喷涂钼涂层组织及性能研究[J].兵工学报,2016,37(8):1489-1496. 被引量:14

5高名传,张永法,陈同舟.TA5-5钛合金表面热喷涂Mo涂层的耐磨耐蚀性能[J].中国钼业,2020,44(1):34-36. 被引量:3

6蒲泽林,刘宗德,杨昆,毛雪平.电热爆炸定向喷涂法制备钼涂层[J].稀有金属材料与工程,2005,34(4):670-672. 被引量:16

7曾归余,闵小兵,吴和元.钼系粉末等离子涂层及其在汽车工业上的应用研究[J].湖南冶金,2002,30(1):8-11. 被引量:9

8安树春,程汉池,栗桌新,高晨.热喷涂涂层的重熔后处理工艺研究进展[J].表面技术,2009,38(2):73-77. 被引量:22

9张志,颜建辉,徐健建.热处理对喷涂Mo涂层微观组织和性能的影响[J].热加工工艺,2015,44(12):163-166. 被引量:2

10范宏林,朱亮,韩峰.粉末电热爆炸喷涂方法制备钼涂层的工艺试验[J].热加工工艺,2018,47(20):144-146. 被引量:2

1李忠岐,徐建兵,梁鑫,洪侃,陈东英,郭家旺.氟盐-氧化物熔盐体系电解制备La-Cu合金及其表征[J].有色金属工程,2022,12(8):9-12.

2郭鹏,马佳,鲍丽,胡粟昕,王路乙.钼及钼合金与石墨焊接研究进展[J].电焊机,2023,53(4):73-80.

3曹子林,张林慧,仲斌年,王云思.铝基复合材料的制备和研究现状[J].金属功能材料,2023,30(2):29-39. 被引量:1

4蒋燕,陈敏,蒋志强.钨纤维/钨复合材料的断裂行为及热冲击损伤分析[J].稀有金属材料与工程,2023,52(2):623-629.

5孙晓玲.电沉积法制备钛基二氧化铅电极的研究[J].黑龙江水利科技,2023,51(3):35-37.

6杨国瑞,李晓雪,闫学荣,张燕,马鑫,高振珅.鬼箭羽栓剂的制备[J].广东化工,2023,50(7):63-65.

7宁裕,柏薇薇,刘佳琪.汽车装饰用彩色氧化亚铜薄膜电镀的研究[J].冶金与材料,2023,43(2):47-49.

8刘艳,冀杰.45#钢表面Ni-W/ZnO超疏水复合涂层的制备及性能研究[J].电镀与精饰,2023,45(5):26-33.

9秦欢,肖孟瑶.集团公司信息化战略目标与规划设计的总体架构研究——以中陕核集团为例[J].企业改革与管理,2023(6):46-48.

10毛望军,高志廷.齿轮钢电沉积Ni-W/MoS_(2)自润滑复合镀层及性能研究[J].电镀与精饰,2023,45(4):31-37.

Basic Information:

DOI:

Chinese Library Classification Number:TG178[金属学及工艺—金属表面处理]

Citation Information:

Due to its excellent physicochemical properties of high strength at high temperature,good corrosion resistance,and strong radiation resistance,molybdenum coating has promising application prospects in metallurgy,aerospace,and nuclear industry.This paper reviews the main preparation methods of the molybdenum coating,including thermal spraying,physical vapor deposition and electrodeposition,and compares the advantages and disadvantages of different methods.In addition,the research status of the electrodeposition of the molybdenum coating in molten salt and aqueous solution is emphasized.The comparisons of the effects of active salt,support electrolyte,and additives on molten salt electrodeposition and molybdenum coating quality are also conducted.At present,the molybdenum coating prepared in molybdate-fluoride-oxide molten salt system has the best comprehensive performance.Aqueous solution electrodeposition has low preparation temperature and wide applicability,but it faces the difficulty of restraining hydrogen evolution and the problem of MoO42-being sensitive to pH value,resulting in weak bonding between the molybdenum coating and the interface.

quote

GB/T 7714-2015 [1] WU Xiang-yang, BAI Shu-xin, WANG Zhen, et al. Research Progress of Molybdenum Coating Prepared by Electrodeposition[J]. Rare Metals and Cemented Carbides, 2023(2): 39-48.
MLA [1] WU Xiang-yang, et al., "Research Progress of Molybdenum Coating Prepared by Electrodeposition." Rare Metals and Cemented Carbides, no. 2, 2023, pp. 39-48.
APA [1] WU Xiang-yang, BAI Shu-xin, WANG Zhen, ZHU Li-an, YE Yi-cong, LI Shun, & TANG Yu. (2023). Research Progress of Molybdenum Coating Prepared by Electrodeposition. Rare Metals and Cemented Carbides(2), 39-48.
IEEE [1] WU Xiang-yang, BAI Shu-xin, WANG Zhen, ZHU Li-an, YE Yi-cong, LI Shun, and TANG Yu, "Research Progress of Molybdenum Coating Prepared by Electrodeposition," Rare Metals and Cemented Carbides, no. 2, pp. 39-48, 2023. keywords: {molybdenum coating;electrodeposition;molten salt;aqueous solution;support electrolyte;molybdate;research progress}