daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Research Progress of Traditional Grating Preparation Technology and Amorphous Alloy Grating Preparation AITranslate

1.State Key Laboratory of Advanced Processing and Recycling of Nonferrous Metals,Lanzhou University of Technology,Lanzhou 730050,China
2.School of Materials Science and Engineering,Lanzhou University of Technology,Lanzhou 730050,China
3.Wenzhou Engineering Institute of Pump & Valve,Lanzhou University of Technology,Wenzhou 325105,China
4.School of Mechanical and Electrical Engineering,Lanzhou University of Technology,Lanzhou 730050,China
AITranslate
Publisher: Youke Publishing Co., Ltd
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The feature size of micro-optical elements is typically on the order of microns or nanometers. Due to the development of micro- and nano-detection and test systems for industrial,commercial and civil applications in the last decade,researchers have conducted detailed and in-depth studies on increasingly miniaturized and integrated micro-optical components and systems,and the rapidly developing microelectronic manufacturing processes have contributed to the design,fabrication and application of micro-optical components. As a used basic optical element,optical grating consists of a large number of equal-width,equally spaced slits arranged periodically,and has four basic functions of dispersion,beam splitting,polarization and phase matching. Although the classical concept of diffraction grating is simple,its connotation is extremely rich. Over the years,gratings have been used for much more than their traditional applications,becoming irreplaceable and important components in many fields of technology. For example,gratings are used in integrated optics,optical holography,spectral analysis,fuzzy processing,digital-to-analog conversion correlation storage,beam coupling,beam sampling,beam splitting,data storage optical testing,bit-phase co-choking,mode-locking,signal processing,solar focused spatial light modulation,optical switching,diagnostic measurements,image recognition,and many more,while gratings continue to be used in new areas. With the development of science and technology,the requirements for grating are constantly improving. At present,many micro-opto-mechanical systems containing optical components are developing toward miniaturization,integration and arraying,so the size of many optical components is also reduced,such as micro-lens arrays,micro-nano gratings,etc. Therefore,the use of new materials for grating preparation and the development of new grating preparation techniques are crucial. Metallic glass has generated a great deal of research,while creating an increasing number of new opportunities for various basic research and commercial applications. Metallic glasses,also known as amorphous alloys,are new metallic materials in which atoms lose their long-range order and maintain their short-range order in three-dimensional space. The inherent structure and properties of metallic glasses further broaden their development field. Compared to crystalline materials,metallic glasses have a unique structure,which gives them many unique physical,chemical and mechanical properties and is one of the most active areas of research in the materials and physics communities today. Metallic glasses possess an amazing property that is not found in traditional metallic materials,which greatly compensates for the lack of mechanical properties of metallic glasses at room temperature and allows us to process this material more easily than traditional metals. This amazing property of metallic glass is its ability to soften after heating to a certain temperature,like glass or plastic,and is called the thermoplastic nature of metallic glass. The viscosity of metallic glass decreases significantly with increasing temperature,so that after heating to a certain temperature (also known as the supercooled liquid region),it can be molded at temperatures and stresses much lower than those required for conventional metal processing. In addition,metallic glass has no dislocations,grain boundaries and other crystalline defects,and its low coefficient of thermal expansion ensures excellent dimensional accuracy in thermoplastic molding,which makes it possible to produce precise microstructures on its surface by thermoplastic molding technology. At the same time,the researchers found that metallic glass has the advantages of high preparation efficiency (molding cycle in seconds,usually less than 30 s),good molding accuracy (dimensional error of about 2%),excellent surface quality (surface roughness of about 10 nm or less),simple process and low cost,etc.,so it has a very broad application prospect in the field of medicine,precision instruments and especially the emerging microelectromechanical systems. Based on this,metallic glasses have injected new blood into the preparation of gratings. Metallic glass has an exceptional surface finish after thermoplastic forming and is significantly more productive than conventional methods. Compared to crystalline glasses,metallic glasses have a smooth and glossy surface,which makes them promising for preparing grating structures with higher performance than common metals (e.g.,pure nickel,etc.). Compared to conventional materials such as polydimethylsiloxane and polymethyl methacrylate,the unique mechanical and physical properties of metallic glasses improve the grating quality. In summary,the selection of materials and preparation processes for grating at the micro and nano scale are of particular importance as the quality requirements for optical devices continue to increase. Metallic glasses are ideal materials for grating preparation,but related research is still in its infancy. In this paper,the definition,classification and application of grating were reviewed. And the research status and unsolved scientific problems of the fabrication technology for traditional grating technology and amorphous alloy grating were presented,and the development opportunities and challenges of amorphous alloy grating in the future were prospected. The discussion in this paper provided a theoretical basis for micro-electro-mechanical (MEMS) system,which showed important theoretical and practical significance to promote the engineering application of amorphous alloy as a new material.

KeyWords AITranslate

grating metallic glass surface patterning diffraction efficiency

[1]Sun P,Zhou C H,Jia W,Wang J,Xiang C C,Xie Y F,Zhao D. Self-referenced refractive index sensor based on hybrid mode resonances in 2D metal-dielectric grating[J].Journal of Physics D-Applied Physics,2020,53(14):1.

[2]Gong B W,Wen H Y,Li H T. Polarization-independent two-layer grating with five-port splitting output under normal incidence[J].IEEE Photonics Journal,2020,12(2):1.

[3]Zhan T,Xiong J H,Tan G J,Wu S T. Absorption-based polarization gratings[J].Optics Express,2020,28(9):13907.

[4]Zou F,Liu Y Q,Mou C B,Zhu S. Optimization of refractive index sensitivity in nanofilm-coated long-period fiber gratings near the dispersion turning point[J].Journal of Lightwave Technology,2020,38(4):889.

[5]Ma W Q,Zhang P Q,Zhou W J,Qi Q Y,Wu Z H,Wang L L,Zhang W,Song B A,Dai S X. Femtosecond-laser direct-writing volume phase gratings inside Ge-As-S chalcogenide glass[J].Ceramics International,2020,46(11):17599.

[6]孙宝玉,许济琛,谷岩,林洁琼,李洁. 振动辅助纳米压印制备大面积光栅结构[J].应用光学,2022,43(1):124.

B Y Sun,J C Xu,Y Gu,J Q Lin,J L. Preparation of large-area grating structure by vibration-assisted nanoimprint[J].Journal of Applied Optics,2022,43(1):124.

[7]范雪茹,凡双玉,谢磊,黄照文,高梦琦,李永泰,李强,王安定. Cu元素添加对Fe基非晶合金结构-性能影响的研究进展[J].铜业工程,2023,(2):15.

X R Fan,S Y Fan,L Xie,Z W Huang,M Q Gao,Y T Li,Q Li,A D Wang. Structure properties of Fe-based metallic glasses with different Cu addition[J].Copper Engineering,2023,(2):15.

[8]田霖,李春燕,翟建树,卢煜,寇生中. 非晶合金的功能性研究进展[J].稀有金属,2021,45(8):998.

L Tian,C Y Li,J S Zhai,Y Lu,S Z Kou. Progress in functional research of amorphous alloys[J].Chinese Journal of Rare Metals,2021,45(8):998.

[9]郑航兵,闫梦阳,安蓉,周雪锋,冯涛,兰司. 纳米非晶及其在生物医学中的应用[J].稀有金属,2023,47(6):854.

H B Zheng,M Y Yan,R An,X F Zhou,T Feng,S Lan. Nanoglass and applications in biomedicine[J].Chinese Journal of Rare Metals,2023,47(6):854.

[10]Khan M M,Deen K M,Haider W. Combinatorial development and assessment of a Zr-based metallic glass for prospective biomedical applications[J].Journal of Non-Crystalline Solids,2019,523,119544.

[11]Ismagilov F R,Papini L,Vavilov V E,Gusakov D V. Design and performance of a high-speed permanent magnet generator with amorphous alloy magnetic core for aerospace applications[J].IEEE Transactions on Industrial Electronics,2020,67(3):1750.

[12]吉丽丽,运新兵,吕云卓. 放电等离子烧结制备Zr50Ti5Cu27Ni10Al8块体非晶合金[J].稀有金属,2020,44(11):1221.

L L Ji,X B Yun,Y Z Lu. Preparation of Zr50Ti5Cu27Ni10Al8 bulk amorphous alloy by spark plasma sintering[J].Chinese Journal of Rare Metals,2020,44(11):1221.

[13]Magagnosc D J,Ehrbar R,Kumar G,He M R,Schroers J,Gianola D S. Tunable tensile ductility in metallic glasses[J].Scientific Reports,2013,3(1):1.

[14]仲健魁,黄元申,倪争技,徐邦联,张大伟. 全息离子束摆动刻蚀凸面闪耀光栅制备技术[J].光学仪器,2021,43(3):86.

J K Zhong,Y S Huang,Z J Ni,B L Xu,D W Zhang. Fabrication of convex blazed grating by holographic ion beam swing etching[J].Optical Instruments,2021,43(3):86.

[15]谈治信. 离子束刻蚀技术[J].纳米科技,1993,(2):103.

Z X Tan. Ion beam etching technology[J].Nanoscience & Nanotechnology,1993,(2):103.

[16]徐向东,洪义麟,傅绍军,王占山. 全息离子束刻蚀衍射光栅[J].物理,2004,33(5):340.

X D Xu,Y L Hong,S J Fu,Z S Wang. Holographic ion beam etched diffraction grating[J].Physics,2004,33(5):340.

[17]Aoyagi Y,Namba S. Blazed ion-etched holographic gratings[J].Optica Acta:International Journal of Optics,1976,23(9):701.

[18]Johnson L F. Evolution of grating profiles under ion-beam erosion[J].Applied Optics,1979,18(15):2559.

[19]刘玉娟,崔继承,巴音贺希格,陈少杰,齐向东,唐玉国. 凸面光栅成像光谱仪的研制与应用[J].光学精密工程,2012,20(1):52.

Y J Liu,J C Cui,H Bayan,S J Chen,X D Qi,Y G Tang. Design and application of imaging spectrometer convex grating[J].Optical and Precision Engineering,2012,20(1):52.

[20]郑衍畅,王铭,胡华奎,王雅楠,杨春来,王海. 全息光刻-反应离子束刻蚀制作硅光栅[J].安徽工程大学学报,2019,34(6):28.

Y C Zheng,M Wang,H K Hu,Y N Wang,C L Yang,H Wang. Fabrication of silicon gratings by holographic photolithography and reactive ion beam etching[J].Journal of Anhui Polytechnic University,2019,34(6):28.

[21]Du K,Wathuthanthri I,Mao W,Xu W,Choi C H. Large-area pattern transfer of metallic nanostructures on glass substrates via interference lithography[J].Nanotechnology,2011,22(28):285306.

[22]白云峰,范杰,邹永刚,王海珠,海一娜,田锟. 激光干涉光刻制备976 nm分布反馈式激光器光栅[J].激光与光电子学进展,2017,54(12):88.

Y F Bai,J Fan,Y G Zou,H Z Wang,Y N Hai,K Tian. Fabrication of gratings used in 976 nm distributed feedback lasers based on laser interference lithography[J].Laser & Optoelectronics Progress,2017,54(12):88.

[23]Koch F,Lehr D,Schönbrodt O,Glaser T,Fechner R,Frost F. Manufacturing of highly-dispersive,high-efficiency transmission gratings by laser interference lithography and dry etching[J].Microelectronic Engineering,2018,191:60.

[24]Yang G F,Gu Y,Zhang X M,Ding Y,Hua B,Gu X. Fabrication of monolayer MoS2 nanogratings via single-pulse nanosecond laser interference lithography[J].Materials Letters,2020,262:127171.

[25]雷宇. 双光束激光干涉纳米光刻设备研发[D].北京:中国科学院大学,2018. 1.

Y Lei. The Development of Two Beam Laser Interference Nano Lithography Equipment[D].Beijing:University of Chinese Academy of Sciences,2018. 1.

[26]李润超. 微纳尺度衍射光栅的制造方法及其应用实验研究[D].武汉:华中科技大学,2019. 1.

R C Li. Research on Fabrication and Application of Micro-Nano Scale Diffraction Grating[D].Wuhan:Huazhong University of Science and Technology,2019. 1.

[27]况国文. 聚合物光栅的制作及衍射性质分析[D].南昌:南昌航空大学,2016. 1.

G W Kuang. Research on the Fabrication and Properties of Polymer Grating[D].Nanchang:Nanchang Hangkong University,2016. 1.

[28]雷刚. 数字光刻制作微光学器件的评价研究[D].南昌:南昌航空大学,2011. 1.

G Lei. Research on Evaluation of Digital Lithography to Fabricate Micro-Optical Elements[D].Nanchang:Nanchang Hangkong University,2011. 1.

[29]张思琪,周思翰,杨卓俊,许治,兰长勇,李春. 基于数字微镜器件的无掩膜光刻技术进展[J].光学精密工程,2022,30(1):12.

S Q Zhang,S H Zhou,Z J Yang,Z Xu,C Y Lan,C Li. Advances in maskless lithography based on digital micromirror devices[J].Optics and Precision Engineering,2022,30(1):12.

[30]饶玉芳. 无掩模光刻系统的研究与设计[D].南昌:南昌航空大学,2010. 1.

Y F Rao. Research and Design on Maskless Lithography System[D].Nanchang:Nanchang Hangkong University,2010. 1.

[31]崔晓峰. 基于数字掩模技术聚合物二元相位光栅的制作[D].南昌:南昌航空大学,2015. 1.

X F Cui. Fabrication of Polymer Binary Grating Based on Digital Mask Technique[D].Nanchang:Nanchang Hangkong University,2015. 1.

[32]Dinh D H,Chien H L,Lee Y C. Maskless lithography based on digital micromirror device (DMD) and double sided microlens and spatial filter array[J].Optics & Laser Technology,2019,113:407.

[33]Zheng Q,Zhou J Y,Chen Q M,Lei L,Wen K H,Hu Y M. Rapid prototyping of a dammann grating in DMD-based maskless lithography[J].IEEE Photonics Journal,2019,11(6):1.

[34]丁玉成. 纳米压印光刻工艺的研究进展和技术挑战[J].青岛理工大学学报,2010,31(1):9.

Y C Ding. Research progress of nanoimprint lithography and its technical challenges[J].Journal of Qingdao Technological University,2010,31(1):9.

[35]Oda H,Ohtake T,Takaoka T,Nakagawa M. Photoreactive chemisorbed monolayer suppressing polymer dewetting in thermal nanoimprint lithography[J].Langmuir,2009,25(12):6604.

[36]Lan H B,Liu H Z. UV-nanoimprint lithography:structure,materials and fabrication of flexible molds[J].Journal of Nanoscience and Nanotechnology,2013,13(5):3145.

[37]Qian F,He Z,Thelen M P,Li Y. A microfluidic microbial fuel cell fabricated by soft lithography[J].Bioresource Technology,2011,102(10):5836.

[38]王明洋. 基于纳米压印技术的微纳结构制备研究[D].哈尔滨:哈尔滨工业大学,2019. 1.

M Y Wang. Fabrication Reaserch of Micro/Nano Structure Based on Nanoimprint Lithographing[D].Harbin:Harbin Institute of Technology,2019. 1.

[39]褚金奎,康维东,曾祥伟,张然. 基于柔性纳米压印工艺制备中红外双层金属纳米光栅[J].光学精密工程,2017,25(12):3034.

J K Zhu,W D Kang,X W Zeng,R Zhang. Fabricated of bilayer metallic nano gratings in mid-infrared based on flexible nanoimprint technology[J].Optics and Precision Engineering,2017,25(12):3034.

[40]Kasztelanic R,Kujawa I,Stepien R,Waddie A J,Taghizadeh M R,Buczynski R. Development of diffraction binary grating using hot embossing processing with electroformed nickel mold for broadband IR optics[J].Infrared Physics & Technology,2020,107,103293.

[41]Gu Y,Xu J C,Lin J Q,Ma H H,Zhao H B,Zhang Y S,Sun B Y. The fabrication of anti-reflection grating structures film for solar cells using vibration-assisted UV nanoimprint lithography[J].Solar Energy,2022,241:172.

[42]王迪,胡伟南,杨永强,冯永伟,张英杰,伊浩. 激光选区熔化纯钨防散射栅格的工艺及性能研究[J].稀有金属,2023,47(5):757.

D Wang,W N Hu,Y Q Yang,Y W Feng,Y J Zhang,H Yi. Selective laser melting process and performance of pure tungsten anti-scatter grid[J].Chinese Journal of Rare Metals,2023,47(5):757.

[43]陈嘉玥,祁学军,刘勇,曹卫林,许梦绮. 一体式激光拼焊热成形门环的开发及应用[J].锻压技术,2023,48(2):77.

J Y Chen,X J Qi,Y Liu,W L Cao,M Q Xu. Development and application on integrated laser tailor welding hot forming for door ring[J].Forging & Stamping Technology,2023,48(2):77.

[44]戴文磊. 高熵非晶合金热塑性微成形能力及微尺度光栅表面性能研究[D].武汉:华中科技大学,2018. 1.

W L Dai. A Dissertation Submitted in Partial Fulfillment of the Requirements for the Degree of Master of Philosophy in Engineer[D].Wuhan:Huazhong University of Science and Technology,2018. 1.

[45]Williams E,Lavery N. Laser processing of bulk metallic glass:a review[J].Journal of Materials Processing Technology,2017,247:73.

[46]Fornell J,Pellicer E,Garcia-Lecina E,Nieto D,Suriñach S,Baró M D,Sort J. Structural and mechanical modifications induced on Cu47.5Zr47.5Al5 metallic glass by surface laser treatments[J].Applied Surface Science,2014,290:188.

[47]Lin H K,Lee C J,Hu T T,Li C H,Huang J C. Pulsed laser micromachining of Mg-Cu-Gd bulk metallic glass[J].Optics and Lasers in Engineering,2012,50(6):883.

[48]Chen B,Shi T L,Li M,Yang F,Yan F,Liao G L. Laser welding of annealed Zr55Cu30Ni5Al10 bulk metallic glass[J].Intermetallics,2014,46:111.

[49]Shao L,Datye A,Huang J,Ketkaew J,Woo S S,Zhao S F,Wu S J,Zhang Y M,Schwarz U,Schroers J. Pulsed laser beam welding of Pd43Cu27Ni10P20 bulk metallic glass[J]. Scientific Reports,2017,7(1):1.

[50]Chen B Q,Pang S J,Han P P,Li Y,Yavari A R,Vaughan G,Zhang T. Improvement in mechanical properties of a Zr-based bulk metallic glass by laser surface treatment[J].Journal of Alloys and Compounds,2010,504(S1):S45.

[51]Wei Y P,Xu G Y,Zhang K,Yang Z,Guo Y C,Huang C G,Wei B C. Anomalous shear band characteristics and extra-deep shock-affected zone in Zr-based bulk metallic glass treated with nanosecond laser peening[J].Scientific Reports,2017,7(1):43948.

[52]Yamada R,Nomura N,Saida J,Kawasaki A. Fabrication of optical gratings through surface patterning of zirconium-based metallic glass by laser irradiation[J].Intermetallics,2018,93:377.

[53]Lei Y H,Yang J J,Cong C,Guo C L. Fabrication of homogenous subwavelength grating structures on metallic glass using double-pulsed femtosecond lasers[J].Optics and Lasers in Engineering,2020,134,106273.

[54]Cui M,Huang H,Zhang L,Yan J. Nanosecond laser “pulling” patterning of micro-nano structures on Zr‐based metallic glass[J].Small,2023,19(4):2206516.

[55]李春燕,朱福平,丁娟强,尹金峰,赵燕春,寇生中. 非晶合金热塑性微成型技术研究概况及发展趋势[J].功能材料,2018,49(11):11033.

C Y Li,F P Zhu,J Q Ding,J F Yin,Y C Zhao,S Z Kou. Research and development trend of amorphous alloy thermoplastic microforming technology[J].Journal of Functional Materials,2018,49(11):11033.

[56]Schroers J. Processing of bulk metallic glass[J].Advanced Materials,2010,22(14):1566.

[57]罗应娜. 34CrNiMo6曲轴热成形工艺研究及优化[J].塑性工程学报,2023,30(2):70.

Y N Luo. Research and optimization of hot forming process of 34CrNiMo6 crankshaft[J].Journal of Plasticity Engineering,2023,30(2):70.

[58]Schroers J,Pham Q,Peker A,Paton N,Curtis R V. Blow molding of bulk metallic glass[J].Scripta Materialia,2007,57(4):341.

[59]Sarac B,Kumar G,Hodges T,Ding S,Desai A,Schroers J. Three-dimensional shell fabrication using blow molding of bulk metallic glass[J].Journal of Microelectromechanical Systems,2011,20(1):28.

[60]Hasan M,Schroers J,Kumar G. Functionalization of metallic glasses through hierarchical patterning[J].Nano Letters,2015,15(2):963.

[61]Chen Z,Xie Y,Datye A,Thornton J,Schroers J,Cha J J,Schwarz U D. Angstrom-scale replication of surfaces with crystallized bulk metallic glasses[J].Materials Today Nano,2021,16:100145.

[62]Xiang J X,Wang Y X,Wu Y P,Peng Q,Shui L Q,Ouyang W G,Ding T,Liu, Z. Superplastic nanomolding of highly ordered metallic sub-micrometer pillars arrays for surface enhanced Raman scattering[J].Advanced Materials Technologies,2022,7(3),2100891.

[63]Cox L M,Martinez A M,Blevins A K,Sowan N,Ding Y,Bowman C N. Nanoimprint lithography:emergent materials and methods of actuation[J].Nano Today,2020,31,100838.

[64]Chu J P,Wijaya H,Wu C W,Tsai T R,Wei C S,Nieh T G,Wadsworth J. Nanoimprint of gratings on a bulk metallic glass[J].Applied Physics Letters,2007,90(3):034101.

[65]Saotome Y,Fukuda Y,Yamaguchi I,Inoue A. Superplastic nanoforming of optical components of Pt-based metallic glass[J].Journal of Alloys and Compounds,2007,434:97.

[66]Ma J,Yi J,Zhao D Q,Pan M X,Wang W H. Large size metallic glass gratings by embossing[J].Journal of Applied Physics,2012,112(6):064505.

[67]Yashiro W,Noda D,Hattori T,Hayashi K,Momose A,Kato H. A metallic glass grating for X-ray grating interferometers fabricated by imprinting[J].Applied Physics Express,2014,7(3):032521.

[68]Sadeghilaridjani M,Kato K,Shinohara T,Yashiro W,Momose A,Kato H. High aspect ratio grating by isochronal imprinting of less viscous workable Gd-based metallic glass for neutron phase imaging[J].Intermetallics,2016,78:55.

[69]Seki Y,Shinohara T,Parker J D,Yashiro W,Momose A,Kato K,Kato H,Sadeghilaridjani M,Otake Y,Kiyanagi Y. Development of multi-colored neutron talbot–lau interferometer with absorption grating fabricated by imprinting method of metallic glass[J].Journal of the Physical Society of Japan,2017,86(4):044001.

[70]Yang C,Lu L M,Zhao Z W,Li J.H,Gong F,Ma J. Micro thermoplastic forming of a Pd-based metallic glass:theory and applications[J].Journal of Iron and Steel Research International,2017,24(4):378.

[71]Sun F,Yang J,Fu J N,Wang B,Ma J,Shen J. Hierarchical macro to nano press molding of optical glasses by using metallic glasses [J].Journal of Non-Crystalline Solids,2022,594:121821.

[72]Sarac B,Eckert J. Thermoplasticity of metallic glasses:processing and applications[J].Progress in Materials Science,2022,127:100941.

Basic Information:

DOI:10.13373/j.cnki.cjrm.XY23010007

Chinese Library Classification Number:TG139+.8

Citation Information:

The feature size of micro-optical elements is typically on the order of microns or nanometers. Due to the development of micro- and nano-detection and test systems for industrial,commercial and civil applications in the last decade,researchers have conducted detailed and in-depth studies on increasingly miniaturized and integrated micro-optical components and systems,and the rapidly developing microelectronic manufacturing processes have contributed to the design,fabrication and application of micro-optical components. As a used basic optical element,optical grating consists of a large number of equal-width,equally spaced slits arranged periodically,and has four basic functions of dispersion,beam splitting,polarization and phase matching. Although the classical concept of diffraction grating is simple,its connotation is extremely rich. Over the years,gratings have been used for much more than their traditional applications,becoming irreplaceable and important components in many fields of technology. For example,gratings are used in integrated optics,optical holography,spectral analysis,fuzzy processing,digital-to-analog conversion correlation storage,beam coupling,beam sampling,beam splitting,data storage optical testing,bit-phase co-choking,mode-locking,signal processing,solar focused spatial light modulation,optical switching,diagnostic measurements,image recognition,and many more,while gratings continue to be used in new areas. With the development of science and technology,the requirements for grating are constantly improving. At present,many micro-opto-mechanical systems containing optical components are developing toward miniaturization,integration and arraying,so the size of many optical components is also reduced,such as micro-lens arrays,micro-nano gratings,etc. Therefore,the use of new materials for grating preparation and the development of new grating preparation techniques are crucial. Metallic glass has generated a great deal of research,while creating an increasing number of new opportunities for various basic research and commercial applications. Metallic glasses,also known as amorphous alloys,are new metallic materials in which atoms lose their long-range order and maintain their short-range order in three-dimensional space. The inherent structure and properties of metallic glasses further broaden their development field. Compared to crystalline materials,metallic glasses have a unique structure,which gives them many unique physical,chemical and mechanical properties and is one of the most active areas of research in the materials and physics communities today. Metallic glasses possess an amazing property that is not found in traditional metallic materials,which greatly compensates for the lack of mechanical properties of metallic glasses at room temperature and allows us to process this material more easily than traditional metals. This amazing property of metallic glass is its ability to soften after heating to a certain temperature,like glass or plastic,and is called the thermoplastic nature of metallic glass. The viscosity of metallic glass decreases significantly with increasing temperature,so that after heating to a certain temperature (also known as the supercooled liquid region),it can be molded at temperatures and stresses much lower than those required for conventional metal processing. In addition,metallic glass has no dislocations,grain boundaries and other crystalline defects,and its low coefficient of thermal expansion ensures excellent dimensional accuracy in thermoplastic molding,which makes it possible to produce precise microstructures on its surface by thermoplastic molding technology. At the same time,the researchers found that metallic glass has the advantages of high preparation efficiency (molding cycle in seconds,usually less than 30 s),good molding accuracy (dimensional error of about 2%),excellent surface quality (surface roughness of about 10 nm or less),simple process and low cost,etc.,so it has a very broad application prospect in the field of medicine,precision instruments and especially the emerging microelectromechanical systems. Based on this,metallic glasses have injected new blood into the preparation of gratings. Metallic glass has an exceptional surface finish after thermoplastic forming and is significantly more productive than conventional methods. Compared to crystalline glasses,metallic glasses have a smooth and glossy surface,which makes them promising for preparing grating structures with higher performance than common metals (e.g.,pure nickel,etc.). Compared to conventional materials such as polydimethylsiloxane and polymethyl methacrylate,the unique mechanical and physical properties of metallic glasses improve the grating quality. In summary,the selection of materials and preparation processes for grating at the micro and nano scale are of particular importance as the quality requirements for optical devices continue to increase. Metallic glasses are ideal materials for grating preparation,but related research is still in its infancy. In this paper,the definition,classification and application of grating were reviewed. And the research status and unsolved scientific problems of the fabrication technology for traditional grating technology and amorphous alloy grating were presented,and the development opportunities and challenges of amorphous alloy grating in the future were prospected. The discussion in this paper provided a theoretical basis for micro-electro-mechanical (MEMS) system,which showed important theoretical and practical significance to promote the engineering application of amorphous alloy as a new material.

quote

GB/T 7714-2015 [1] Chunyan Li, Yishu Zhang, Shaojie Hou, et al. Research Progress of Traditional Grating Preparation Technology and Amorphous Alloy Grating Preparation[J]. Chinese Journal of Rare Metals, 2024, 48(12): 1766-1780. DOI:10.13373/j.cnki.cjrm.XY23010007.
MLA [1] Chunyan Li, et al., "Research Progress of Traditional Grating Preparation Technology and Amorphous Alloy Grating Preparation." Chinese Journal of Rare Metals, vol. 48, no. 12, 2024, pp. 1766-1780, https://doi.org/10.13373/j.cnki.cjrm.XY23010007.
APA [1] Chunyan Li, Yishu Zhang, Shaojie Hou, Chunling Li, Xiaocheng Li, & Shengzhong Kou. (2024). Research Progress of Traditional Grating Preparation Technology and Amorphous Alloy Grating Preparation. Chinese Journal of Rare Metals, 48(12), 1766-1780. https://doi.org/10.13373/j.cnki.cjrm.XY23010007
IEEE [1] Chunyan Li, Yishu Zhang, Shaojie Hou, Chunling Li, Xiaocheng Li, and Shengzhong Kou, "Research Progress of Traditional Grating Preparation Technology and Amorphous Alloy Grating Preparation," Chinese Journal of Rare Metals, vol. 48, no. 12, pp. 1766-1780, 2024, doi: 10.13373/j.cnki.cjrm.XY23010007. keywords: {grating;metallic glass;surface patterning;diffraction efficiency}