daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Properties of Micro-Arc Oxides of 7075 Aluminum Alloys Prepared with Different pH AITranslate

Xi'an Rare Metal Materials Institute Co,Ltd,Xi'an 710016,China
AITranslate
Publisher: Youke Publishing Co., Ltd
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

7075 Al alloy is a kind of alloy material with high strength and excellent wear resistance,which is widely used in aerospace,automotive and other fields. In recent years,the application of 7075 aluminum alloy in marine vessels has gradually increased with the proposal of marine energy strategy. However,despite its good mechanical properties and strength,its corrosion resistance in marine environment is unsatisfactory and susceptible to corrosion,which seriously affects its safety and service life,and limits its large-scale application in the field of 7075 Al alloy in the field of marine engineering,national defense industry and others. In order to solve this problem,researchers are constantly searching for ways to improve the alloy,such as alloy surface coating technology,alloy formulation optimization,etc.,to improve the corrosion resistance of 7075 Al alloy in marine environment. Micro arc oxidation (MAO) technology is one of the effective ways to improve the surface properties of aluminum alloys by combining the electrolyte and appropriate electrical parameters so that the metal on the surface of the substrate interacts with the electrolyte solution,forming a ceramic film layer on the surface of the substrate,which is dominated by the metal oxides of the substrate. This technique can significantly improve the surface hardness,wear resistance,corrosion resistance and other properties of the material,which is of great importance in improving the overall performance of aluminum alloys. The pH of the electrolyte is a key parameter affecting the microstructure,mechanical properties and physical and chemical properties of the micro-arc oxidation film layer. Different pH leads to changes in the composition and structure of the film layer,which in turn affects its hardness,wear and corrosion resistance,and other properties. Therefore,in the micro-arc oxidation process,proper control of the pH of the electrolyte is essential to achieve the desired performance of the film layer. The film layer was prepared on the surface of 7075 aluminum alloy by using micro-arc oxidation technology in this paper. By adjusting pH of the electrolyte,the effects of different pH on the microstructure and corrosion resistance of the micro-arc oxidized film layer were investigated. Aiming to understand the influence mechanism of pH change on the performance of the film layer during the micro-arc oxidation process,and to provide theoretical support and experimental basis for the optimization of the micro-arc oxidation process. The surface morphology of the membrane layers prepared with different pH electrolytes was observed using scanning electron microscope (SEM),and the changes in micropore distribution,pore size,and porosity of the membrane layers were analyzed using Image-J software. Meanwhile,an eddy current thickness gauge was used to check the thickness variation of the membrane layer. Vickers microhardness tester was used to evaluate the hardness of the membrane layer. In addition,the corrosion resistance was tested in 3.5% NaCl (mass fraction) solution using an electrochemical workstation. Tafel fitting method was used to obtain the corresponding electrochemical parameters to quantitatively analyze the changes in corrosion performance of 7075 aluminum alloy before and after micro-arc oxidation treatment. And the effects of pH changes on the microstructure,thickness,hardness,and corrosion resistance of the membrane layer were systematically analyzed.The results showed that the micro-arc oxidation treatment could significantly improve the corrosion resistance of 7075 aluminum alloy. As pH of the electrolyte increased,the breakdown voltage during the micro-arc oxidation process decreased,resulting in the generation of finer discharge sparks,the number of large-size micropores (diameter larger than 2.5 μm) or the total number of micropores decreased and then increased,and the porosity of the film layer showed a tendency to decrease and then increase,while the hardness and thickness of the film layer showed the opposite tendency. Moreover,the corrosion resistance of the samples was improved. The self-corrosion current and corrosion rate of the micro-arc oxidized film layer showed a trend of decreasing and then increasing with the increase of pH,and the trend of self-corrosion voltage was opposite. When pH of the electrolyte was 12.7,the surface film layer of 7075 aluminum alloy showed the best corrosion resistance,with self-corrosion potential of -0.6 V,self-corrosion current of 4.74×10−7 A·cm−2,corrosion rate of 0.0056 mm·a−1 and polarization resistance value of 18.7×103 Ω·cm2,which was about one order of magnitude lower than that of 7075 aluminum alloy. However,when pH of the electrolyte was too high,the growth rate of the coating slowed down,the film layer became thinner and the corrosion resistance decreased.

KeyWords AITranslate

7075 aluminum alloy pH micro-arc oxidation (MAO) corrosion resistance

[1]朱炳耀,贾小波. 超声振动原位Al2O3(p)/7075汽车零件合金组织与耐腐蚀性能研究 [J].有色金属科学与工程,2023,14(4):511.

B Y Zhu,X B Jia. Study on microstructure and corrosion resistance of an in situ Al2O3(p)/7075 alloy for automotive parts prepared by ultrasonic vibration [J].Nonferrous Metals Science and Engineering,2023,14(4):511.

[2]李晓含,贺嘉宁,苏睿明,杨玉萍,聂赛男,谭兵. 双级时效对7075合金应力腐蚀性能影响 [J].有色金属科学与工程,2022,13(3):69.

X H Li,J N He,R M Su,Y P Yang,S N Nie,B Tan. Effect on stress corrosion cracking of alloy 7075 with two-step aging [J].Nonferrous Metals Science and Engineering,2022,13(3):69.

[3](刘立博,乔及森,许佳敏,夏宗辉,李琦伦. 稀土Y对挤压态7075铝合金微观组织和力学性能的影响[J].有色金属工程,2022,12(3):47.)

L B Liu,J S Qiao,J M Xu,Z H Xia,Q L Li. Effect of rare earth yttrium on mechanical properties and microstructure of extruded 7075 aluminum alloy[J].Nonferrous Metals Engineering,2022,12(3):47.

[4]Songur F,Arslan E,Dikici B. Taguchi optimization of PEO process parameters for corrosion protection of AA7075 alloy [J].Surface and Coatings Technology,2022,434:128202.

[5]Wang S N,Gu Y H,Geng Y L,Liang J,Zhao J,Kang J. Investigating local corrosion behavior and mechanism of MAO coated 7075 aluminum alloy [J].Journal of Alloys and Compounds,2020,826:153976.

[6]吕晓丹,刘斌,刘岩,刘蔚,田华阳. 铝合金在海洋环境中的腐蚀行为研究进展 [J].中国材料进展,2022,41(6):477.

X D Lv,B Liu,Y Liu,Y Liu,H Y Tian. Research progress on the corrosion behavior of aluminum alloys under marine environment [J].Materials China,2022,41(6):477.

[7]刘建,朱新河,马春生,尚少伟. 稀土添加剂对微弧氧化膜层影响的研究进展 [J].稀有金属,2022,46(8):1073.

J Liu,X H Zhu,C S Ma,S W Shang. Research progress on micro-arc oxide film with rare earth additives [J].Chinese Journal of Rare Metals,2022,46(8):1073.

[8]雍家惠,李宏战,李争显,王毅飞,耿娟娟. 微纳米颗粒添加剂在镁合金微弧氧化涂层中的应用研究现状 [J].稀有金属,2021,45(10):1230.

J H Yong,H Z Li,Z X Li,Y F Wang,J J Geng. Research status of application of micro-nano additives in micro-arc oxidation coatings formed on magnesium alloys [J].Chinese Journal of Rare Metals,2021,45(10):1230.

[9]赵华星,孙晓峰,宋巍,李占明,李德民. 微弧氧化技术在铝合金腐蚀防护中的应用研究与发展 [J].材料导报,2021,35(21):21236.

H X Zhao,X F Sun,W Song,Z M Li,D M Li. Application research and development of micro-arc oxidation technology in corrosion protection of aluminum alloy equipment [J].Materials Reports,2021,35(21):21236.

[10]彭振军. 基础电解液中金属表面微弧氧化膜生长行为与性能关系研究[D].兰州:兰州理工大学,2022. 1.

Z J Peng. Correlations between the Growth Behavior and Properties of the Micro-Arc Oxidation Coatings on Metal Surface in Basic Electolyte[D].Lanzhou:Lanzhou University of Technology,2022. 1.

[11]陈庚,苗景国,方琴,苗骁,王正云. 铝酸钠对铝合金微弧氧化膜层组织性能的影响 [J].兵器材料科学与工程,2022,45(5):42.

G Chen,J G Miao,Q Fang,X Miao,Z Y Wang. Effect of sodium aluminate on microstructure and properties of micro-arc oxidation coatings on aluminum alloy [J].Ordnance Material Science and Engineering,2022,45(5):42.

[12]Rakoch A G,Gladkova A A,Linn Z,Strekalina D M. The evidence of cathodic micro-discharges during plasma electrolytic oxidation of light metallic alloys and micro-discharge intensity depending on pH of the electrolyte [J].Surface and Coatings Technology,2015,269:138.

[13]Rocca E,Veys-Renaux D,Guessoum K. Electrochemical behavior of zinc in KOH media at high voltage:micro-arc oxidation of zinc [J].Journal of Electroanalytical Chemistry,2015,754:125.

[14]Mojtaba V A,Arash F A,Mohsen K K. Optimizing the electrolyte chemistry parameters of PEO coating on 6061 Al alloy by corrosion rate measurement:response surface methodology [J].Measurement,2018,124:252.

[15]李均明. 铝合金微弧氧化陶瓷层的形成机制及其磨损性能[D].西安:西安理工大学,2008. 37.

J M Li. Formation Mechanism and Abrasion Tests of Micro-Arc Oxidation Ceramic Layers on Aluminum Alloy[D].Xi'an:Xi'an University of Technology,2008. 37.

[16]Kaseem M,Lee Y H,Ko Y G. Incorporation of MoO2 and ZrO2 particles into the oxide film formed on 7075 Al alloy via micro-arc oxidation [J].Materials Letters,2016,182:260.

[17]Arash F A,Mojtaba V A,Mohsen K K. Influence of concentrations of KOH and Na2SiO3 electrolytes on the electrochemical behavior of ceramic coatings on 6061 Al alloy processed by plasma electrolytic oxidation [J].Acta Metallurgica Sinica (English Letters),2016,29(3):274.

[18]吴国瑞. 铝及铝合金表面微弧氧化膜层微观结构及耐蚀性能研究[D].秦皇岛:燕山大学,2022. 1.

G R Wu. Microstructure and Corrosion Resistance of Micro Arc Oxidationcoatings on Aluminium and Aluminium Alloy[D].Qinhuangdao:Yanshan University,2022. 1.

[19]童澍. 基于微弧氧化技术铝合金表面复合氧化膜的制备及耐蚀性能研究[D].青岛:青岛理工大学,2022. 27.

S Tong. Preparation and Corrosion Resistance of Composite Oxide Film on Aluminum Alloy Surface Based on Micro-Arc Oxidation Technology[D].Qingdao:Qingdao University of Technology,2022. 27.

[20]赵华星,宋巍,孙晓峰,李占明,邱骥,史玉鹏. 铝合金表面微弧氧化制备陶瓷层的最佳工艺优化及耐腐蚀性能研究 [J].材料保护,2022,55(2):88.

H X Zhao,W Song,X F Sun,Z M Li,J Qiu,Y P Shi. Study on optimum process optimization and corrosion resistance of ceramic layer prepared by micro-arc oxidation on surface of aluminum alloy [J].Materials Protection,2022,55(2):88.

[21]Mahshid S J,Arash F A. Effect of KOH concentration on the electrochemical behavior of coatings formed by pulsed DC micro-arc oxidation (MAO) on AZ31B Mg alloy [J].Journal of Alloys and Compounds,2016,661:237.

[22]苗景国. 超硬铝合金7075微弧氧化陶瓷层的微结构及性能研究[D].武汉:武汉科技大学,2013. 69.

J G Miao. Study of the Microstructure and Properties of Ceramic Coatings Prepared by Micro-Arc Oxidation on Surface of 7075 Super-Hard Aluminum Alloy[D].Wuhan:Wuhan University of Science and Technology,2013. 69.

[23]Peng C,Liu Y W,Guo M X,Gu T Z,Wang C,Wang Z Y,Sun C. Corrosion and pitting behavior of pure aluminum 1060 exposed to Nansha Islands tropical marine atmosphere [J].Transactions of Nonferrous Metals Society of China,2022,32(2):448.

[24]Qi X,Li J,He Y F,Liu Y T,Liu R,Song R G. Study on the wear resistance and corrosion behaviour of self-sealed MAO/ZrO2 coatings prepared on 7075 aluminium alloy [J].Journal of Alloys and Compounds,2023,969:172436.

Basic Information:

DOI:10.13373/j.cnki.cjrm.XY23120003

Chinese Library Classification Number:TG174.4

Citation Information:

7075 Al alloy is a kind of alloy material with high strength and excellent wear resistance,which is widely used in aerospace,automotive and other fields. In recent years,the application of 7075 aluminum alloy in marine vessels has gradually increased with the proposal of marine energy strategy. However,despite its good mechanical properties and strength,its corrosion resistance in marine environment is unsatisfactory and susceptible to corrosion,which seriously affects its safety and service life,and limits its large-scale application in the field of 7075 Al alloy in the field of marine engineering,national defense industry and others. In order to solve this problem,researchers are constantly searching for ways to improve the alloy,such as alloy surface coating technology,alloy formulation optimization,etc.,to improve the corrosion resistance of 7075 Al alloy in marine environment. Micro arc oxidation (MAO) technology is one of the effective ways to improve the surface properties of aluminum alloys by combining the electrolyte and appropriate electrical parameters so that the metal on the surface of the substrate interacts with the electrolyte solution,forming a ceramic film layer on the surface of the substrate,which is dominated by the metal oxides of the substrate. This technique can significantly improve the surface hardness,wear resistance,corrosion resistance and other properties of the material,which is of great importance in improving the overall performance of aluminum alloys. The pH of the electrolyte is a key parameter affecting the microstructure,mechanical properties and physical and chemical properties of the micro-arc oxidation film layer. Different pH leads to changes in the composition and structure of the film layer,which in turn affects its hardness,wear and corrosion resistance,and other properties. Therefore,in the micro-arc oxidation process,proper control of the pH of the electrolyte is essential to achieve the desired performance of the film layer. The film layer was prepared on the surface of 7075 aluminum alloy by using micro-arc oxidation technology in this paper. By adjusting pH of the electrolyte,the effects of different pH on the microstructure and corrosion resistance of the micro-arc oxidized film layer were investigated. Aiming to understand the influence mechanism of pH change on the performance of the film layer during the micro-arc oxidation process,and to provide theoretical support and experimental basis for the optimization of the micro-arc oxidation process. The surface morphology of the membrane layers prepared with different pH electrolytes was observed using scanning electron microscope (SEM),and the changes in micropore distribution,pore size,and porosity of the membrane layers were analyzed using Image-J software. Meanwhile,an eddy current thickness gauge was used to check the thickness variation of the membrane layer. Vickers microhardness tester was used to evaluate the hardness of the membrane layer. In addition,the corrosion resistance was tested in 3.5% NaCl (mass fraction) solution using an electrochemical workstation. Tafel fitting method was used to obtain the corresponding electrochemical parameters to quantitatively analyze the changes in corrosion performance of 7075 aluminum alloy before and after micro-arc oxidation treatment. And the effects of pH changes on the microstructure,thickness,hardness,and corrosion resistance of the membrane layer were systematically analyzed.The results showed that the micro-arc oxidation treatment could significantly improve the corrosion resistance of 7075 aluminum alloy. As pH of the electrolyte increased,the breakdown voltage during the micro-arc oxidation process decreased,resulting in the generation of finer discharge sparks,the number of large-size micropores (diameter larger than 2.5 μm) or the total number of micropores decreased and then increased,and the porosity of the film layer showed a tendency to decrease and then increase,while the hardness and thickness of the film layer showed the opposite tendency. Moreover,the corrosion resistance of the samples was improved. The self-corrosion current and corrosion rate of the micro-arc oxidized film layer showed a trend of decreasing and then increasing with the increase of pH,and the trend of self-corrosion voltage was opposite. When pH of the electrolyte was 12.7,the surface film layer of 7075 aluminum alloy showed the best corrosion resistance,with self-corrosion potential of -0.6 V,self-corrosion current of 4.74×10−7 A·cm−2,corrosion rate of 0.0056 mm·a−1 and polarization resistance value of 18.7×103 Ω·cm2,which was about one order of magnitude lower than that of 7075 aluminum alloy. However,when pH of the electrolyte was too high,the growth rate of the coating slowed down,the film layer became thinner and the corrosion resistance decreased.

quote

GB/T 7714-2015 [1] Haixia Jiang, Liman Chen, Dong Han, et al. Properties of Micro-Arc Oxides of 7075 Aluminum Alloys Prepared with Different pH[J]. Chinese Journal of Rare Metals, 2024, 48(12): 1692-1701. DOI:10.13373/j.cnki.cjrm.XY23120003.
MLA [1] Haixia Jiang, et al., "Properties of Micro-Arc Oxides of 7075 Aluminum Alloys Prepared with Different pH." Chinese Journal of Rare Metals, vol. 48, no. 12, 2024, pp. 1692-1701, https://doi.org/10.13373/j.cnki.cjrm.XY23120003.
APA [1] Haixia Jiang, Liman Chen, Dong Han, Bo Zhou, Gang Liu, Xiaogang Hu, & Longshi Qiu. (2024). Properties of Micro-Arc Oxides of 7075 Aluminum Alloys Prepared with Different pH. Chinese Journal of Rare Metals, 48(12), 1692-1701. https://doi.org/10.13373/j.cnki.cjrm.XY23120003
IEEE [1] Haixia Jiang, Liman Chen, Dong Han, Bo Zhou, Gang Liu, Xiaogang Hu, and Longshi Qiu, "Properties of Micro-Arc Oxides of 7075 Aluminum Alloys Prepared with Different pH," Chinese Journal of Rare Metals, vol. 48, no. 12, pp. 1692-1701, 2024, doi: 10.13373/j.cnki.cjrm.XY23120003. keywords: {7075 aluminum alloy;pH;micro-arc oxidation (MAO);corrosion resistance}