daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Present Situation and Prospect of Rare Earth Molten Salt Electrolytic Slag Recovery and Utilization Technology AITranslate

Faculty of Materials Metallurgy and Chemistry,Jiangxi University of Science and Technology;Faculty of Materials Metallurgy and Chemistry,Jiangxi University of Science and Technology;Faculty of Materials Metallurgy and Chemistry,Jiangxi University of Science and Technology;Faculty of Materials Metallurgy and Chemistry,Jiangxi University of Science and Technology;Faculty of Materials Metallurgy and Chemistry,Jiangxi University of Science and Technology;Faculty of Materials Metallurgy and Chemistry,Jiangxi University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Rare earth molten salt electrolytic slag is a rare-earth-based solid waste generated during the preparation of rare earth metals and their alloys by molten salt electrolysis,containing abundant rare earth metals,fluorine,and lithium resources.This paper reviews the present situation of valuable metal recovery and reuse from rare earth molten salt electrolytic slag,and introduces the technical advantages and problems of physical,acid,and alkali processes.The paper also focuses on the existing issues and future development trends of industrialized technologies of concentrated sulfuric acid roasting and sodium hydroxide roasting,hoping to provide reference for resource recycling of rare earth molten salt electrolytic slag.

KeyWords AITranslate

rare earth molten salt electrolytic slag fluoride concentrated sulfuric acid roasting sodium hydroxide roasting development trend

1邝海,谭敦强,何文,王晓茹,邹志航,易志强,白杜娟.稀土元素对硬质合金影响的研究进展[J].稀有金属与硬质合金,2018,46(3):69-74. 被引量:8

2李国玲,李星国.稀土金属及其金属间化合物的研究与应用[J].中国稀土学报,2016,34(6):748-763. 被引量:13

3肖敏,邱小英,蓝桥发.稀土冶炼中氟转化及资源化探究[J].世界有色金属,2019,0(15):1-3. 被引量:2

4徐家聪,喻小强,吴选高,龚傲,徐志峰,田磊.氟化稀土熔盐电解渣硫酸浸出脱氟研究[J].有色金属科学与工程,2020,11(6):1-9. 被引量:5

5肖勇,陈月华,崔小震.稀土熔盐电解废料回收工艺研究[J].世界有色金属,2016,0(3):26-28. 被引量:5

6龚傲,李子良,吴选高,田磊.稀土熔盐电解渣中铁的分布状态与磁选除铁的工艺研究[J].江西冶金,2019,39(6):21-28. 被引量:6

7陈冬英,欧阳红,刘莲翠,谢亘.稀土电解废熔盐的综合利用研究[J].江西冶金,2005,25(1):4-8. 被引量:11

8杨幼明,李柳,肖敏,牛飞.稀土熔盐渣碳酸钠焙烧转型机理及浸出规律[J].中南大学学报:自然科学版,2019,50(5):1035-1041. 被引量:7

9Zhifang Tong,Xiaofei Hu,Hao Wen.Effect of roasting activation of rare earth molten salt slag on extraction of rare earth,lithium and fluorine[J].稀土学报:英文版,2023,41(2):300-308. 被引量:1

10刘木根.一种稀土电解废石墨制品回收稀土熔盐工艺研究[J].有色矿冶,2018,34(4):41-44. 被引量:3

1周黎,万新屏.绿色制造与生态文明建设的关系[J].中文科技期刊数据库(全文版)农业科学,2022(5):0222-0224.

2郝朋.试论煤矿智能化开采技术研究现状及展望[J].中国科技期刊数据库 工业A,2022(11):0137-0140.

3闫荣伟,李会泉,邢鹏,叶春林,王晨晔,朱干宇,钟立钦.熔盐电解渣磁选—焙烧—浸出提取稀土元素[J].有色金属:冶炼部分,2023(5):43-51.

4宋书宇,荣涛,左海滨.熔盐电化学还原CO_(2)制备先进碳材的研究进展[J].江西冶金,2023,43(2):128-134.

5林堂茂,刘小多,孙雪婷.石化行业面对“双碳”目标的应对措施[J].现代化工,2023,43(3):1-5. 被引量:2

6阳国军,刘会友.我国石化行业耦合绿氢降碳发展现状及展望[J].中国石化,2023(5):38-41.

7于国军,韩振斌,赵昭.聚合物复合铜箔生产技术研究现状及展望[J].铜业工程,2023(2):101-107.

8罗世兰.论中药临床药学发展现状及展望[J].中国科技期刊数据库 医药,2021(6):0214-0214.

9张金宇,林如山,张磊,唐洪彬,叶国安.干法后处理流程中电解精炼设备研发进展[J].核化学与放射化学,2023,45(2):93-101.

10罗磊磊,刘宇婧,孙小虎.废旧三元锂离子电池正极材料资源化技术研究进展[J].广州化工,2023,51(2):13-18.

Basic Information:

DOI:

Chinese Library Classification Number:TF845[冶金工程—有色金属冶金]

Citation Information:

Rare earth molten salt electrolytic slag is a rare-earth-based solid waste generated during the preparation of rare earth metals and their alloys by molten salt electrolysis,containing abundant rare earth metals,fluorine,and lithium resources.This paper reviews the present situation of valuable metal recovery and reuse from rare earth molten salt electrolytic slag,and introduces the technical advantages and problems of physical,acid,and alkali processes.The paper also focuses on the existing issues and future development trends of industrialized technologies of concentrated sulfuric acid roasting and sodium hydroxide roasting,hoping to provide reference for resource recycling of rare earth molten salt electrolytic slag.

quote

GB/T 7714-2015 [1] ZHONG Li-qin, YE Chun-lin, LIAO Liang-fang, et al. Present Situation and Prospect of Rare Earth Molten Salt Electrolytic Slag Recovery and Utilization Technology[J]. Rare Metals and Cemented Carbides, 2023(2): 20-25.
MLA [1] ZHONG Li-qin, et al., "Present Situation and Prospect of Rare Earth Molten Salt Electrolytic Slag Recovery and Utilization Technology." Rare Metals and Cemented Carbides, no. 2, 2023, pp. 20-25.
APA [1] ZHONG Li-qin, YE Chun-lin, LIAO Liang-fang, CAO Lei, XIONG Shi-xian, & LIAO Chun-fa. (2023). Present Situation and Prospect of Rare Earth Molten Salt Electrolytic Slag Recovery and Utilization Technology. Rare Metals and Cemented Carbides(2), 20-25.
IEEE [1] ZHONG Li-qin, YE Chun-lin, LIAO Liang-fang, CAO Lei, XIONG Shi-xian, and LIAO Chun-fa, "Present Situation and Prospect of Rare Earth Molten Salt Electrolytic Slag Recovery and Utilization Technology," Rare Metals and Cemented Carbides, no. 2, pp. 20-25, 2023. keywords: {rare earth;molten salt electrolytic slag;fluoride;concentrated sulfuric acid roasting;sodium hydroxide roasting;development trend}