Effects of Electromagnetic Action on Melting and Separation of Niobium Concentrate AITranslate

College of Materials and Metallurgy,Inner Mongolia University of Science and Technology;College of Materials and Metallurgy,Inner Mongolia University of Science and Technology;College of Materials and Metallurgy,Inner Mongolia University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

In view of the characteristics and actuality of unbalanced utilization of Bayan Obo niobium concentrate,the electromagnetic action is introduced to realize the dual objectives of efficient separation of metallic iron resources and comprehensive utilization of niobium carbide in Bayan Obo niobium concentrate.In this research,the effect of electromagnetic action on the melting and separation of the niobium concentrate was studied by using self-designed electromagnetic melting and separation device.The results indicate that the electromagnetic action can promote the separation of slag and iron after the reduction of niobium concentrate to reduce the residual iron in the slag.When the current frequency is fixed,the yield of metallic iron increases significantly with the increase of the current intensity.When the current intensity is fixed,the iron yield decreases with the increase of the current frequency.The electromagnetic action promotes the contact between niobium carbide and iron.Under the same current frequency,the content of niobium carbide in iron increases significantly with the increase of the current intensity,while it decreases obviously with the increase of the current frequency under the same current intensity.The magnetic field produced by low frequency and high intensity current can improve the dispersion effect of niobium carbide in iron phase,and the niobium carbide particles in iron are obviously dispersed.

KeyWords AITranslate

electromagnetic action niobium concentrate melting and separation iron niobium carbide current frequency current intensity

1张殿彬,安东,张艳国.电磁搅拌在铝熔铸行业中的应用[J].世界有色金属,2005(1):39-40. 被引量:1

2石瑞.电磁搅拌技术在冶金方面的应用[J].机械研究与应用,2012,25(2):5-7. 被引量:8

3赵君文,郭安,徐超,李微,戴光泽,吴树森.弱电磁搅拌制备Al-Zn-Mg-Cu大体积铝合金半固态浆料[J].中国有色金属学报,2016,26(12):2499-2505. 被引量:9

4陈刚,郑顺奇,王岩,王斌锋.镁合金半固态浆料制备与成形技术研究进展[J].兵器材料科学与工程,2018,41(3):116-120. 被引量:8

5王海花.铌矿资源及其选矿工艺[J].有色矿冶,2011,27(6):21-23. 被引量:14

6王维维,杨占峰,候少春,张立锋,魏威.白云鄂博铌资源特征及开发利用新进展[J].矿产保护与利用,2020,40(5):49-53. 被引量:7

7张勇.我国铌资源开发利用现状调查[J].现代矿业,2022,38(2):32-34. 被引量:3

8陈太生.浅析铌微合金化在高强度钢筋生产中的应用[J].天津冶金,2005(6):30-32. 被引量:3

9于秀兰,王之昌.铌的光度分析试剂及其在光度分析中的应用[J].稀有金属,2006,30(6):863-869. 被引量:3

10董汉鹏,张威.半导体乙醇传感器的湿度影响与氧化铌的应用[J].传感器与微系统,2008,27(3):49-51. 被引量:3

1姚承.比较PKP术中运用侧方开口和前方开口骨水泥注射器治疗胸腰椎OVCF的疗效[J].中文科技期刊数据库(全文版)医药卫生,2023(3):0037-0039.

2王福新.土木工程施工安全管理模式的创新思考[J].中文科技期刊数据库(全文版)工程技术,2020(11):0263-0264.

3许静.以学生为中心的初中英语阅读有效教学研究[J].中文科技期刊数据库(全文版)教育科学,2023(4):0127-0130.

4冯超,赵力,张书熠,张义龙.椎体后凸成形术治骨质疏松性椎体压缩骨折的临床效果分析[J].中文科技期刊数据库(全文版)医药卫生,2021(5):0005-0006.

5陈伟文.一种铌锆碳合金铸锭的制备方法[J].有色金属材料与工程,2023,44(2):85-85.

6柴鑫,杨俊松,徐辉,刘团江,郝定均.经横突上缘椎弓根外侧入路单侧PKP治疗伴椎弓根狭窄骨质疏松性腰椎骨折[J].实用骨科杂志,2023,29(4):296-302.

7陈昆.饮食对肠镜检查肠道准备的影响[J].中文科技期刊数据库(引文版)医药卫生,2021(5):0213-0213.

8龚剑.基于Nvivo11质性分析的我国冰雪运动发展影响因素研究[J].四川体育科学,2023,42(3):11-17.

9范振宁,何小凡,巩艳明.计件工资制与现代农业企业用工[J].中文科技期刊数据库(全文版)经济管理,2022(2):0247-0250.

10鲜科.企业财务风险管控创新策略研究[J].中国民商,2023(4):154-156.

Basic Information:

DOI:

Chinese Library Classification Number:TF649[冶金工程—钢铁冶金]

Citation Information:

In view of the characteristics and actuality of unbalanced utilization of Bayan Obo niobium concentrate,the electromagnetic action is introduced to realize the dual objectives of efficient separation of metallic iron resources and comprehensive utilization of niobium carbide in Bayan Obo niobium concentrate.In this research,the effect of electromagnetic action on the melting and separation of the niobium concentrate was studied by using self-designed electromagnetic melting and separation device.The results indicate that the electromagnetic action can promote the separation of slag and iron after the reduction of niobium concentrate to reduce the residual iron in the slag.When the current frequency is fixed,the yield of metallic iron increases significantly with the increase of the current intensity.When the current intensity is fixed,the iron yield decreases with the increase of the current frequency.The electromagnetic action promotes the contact between niobium carbide and iron.Under the same current frequency,the content of niobium carbide in iron increases significantly with the increase of the current intensity,while it decreases obviously with the increase of the current frequency under the same current intensity.The magnetic field produced by low frequency and high intensity current can improve the dispersion effect of niobium carbide in iron phase,and the niobium carbide particles in iron are obviously dispersed.

quote

GB/T 7714-2015 [1] WEN Ming, WANG Xiao-nan, LIU Ya-qi. Effects of Electromagnetic Action on Melting and Separation of Niobium Concentrate[J]. Rare Metals and Cemented Carbides, 2023(2): 26-29.
MLA [1] WEN Ming, et al., "Effects of Electromagnetic Action on Melting and Separation of Niobium Concentrate." Rare Metals and Cemented Carbides, no. 2, 2023, pp. 26-29.
APA [1] WEN Ming, WANG Xiao-nan, & LIU Ya-qi. (2023). Effects of Electromagnetic Action on Melting and Separation of Niobium Concentrate. Rare Metals and Cemented Carbides(2), 26-29.
IEEE [1] WEN Ming, WANG Xiao-nan, and LIU Ya-qi, "Effects of Electromagnetic Action on Melting and Separation of Niobium Concentrate," Rare Metals and Cemented Carbides, no. 2, pp. 26-29, 2023. keywords: {electromagnetic action;niobium concentrate;melting and separation;iron;niobium carbide;current frequency;current intensity}