Study on a New Process for the Wet Preparation of Ammonium Heptamolybdate from Ammonium Dimolybdate AITranslate

Metallurgical Separation Science and Engineering Laboratory,School of Metallurgy and Environment,Central South University;Metallurgical Separation Science and Engineering Laboratory,School of Metallurgy and Environment,Central South University;Metallurgical Separation Science and Engineering Laboratory,School of Metallurgy and Environment,Central South University;Metallurgical Separation Science and Engineering Laboratory,School of Metallurgy and Environment,Central South University;Metallurgical Separation Science and Engineering Laboratory,School of Metallurgy and Environment,Central South University;Metallurgical Separation Science and Engineering Laboratory,School of Metallurgy and Environment,Central South University;Metallurgical Separation Science and Engineering Laboratory,School of Metallurgy and Environment,Central South University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Ammonium heptamolybdate was prepared by water dissolving-evaporation concentration removal of ammonia-cooling crystallization method using ammonium dimolybdate as raw material.The effects of concentration degree on crystallization product were investigated,and the effects of concentrated liquid density,cooling rate,crystal growing time,and stirring rate on the particle size and morphology of ammonium heptamolybdate were also studied.The results show that ammonium heptamolybdate crystals with a single phase can be prepared by the evaporation concentration-cooling crystallization method after the water dissolution of ammonium dimolybdate.With a concentrated liquid density of about 1.38 g/cm3,a cooling rate of 30℃/h,a crystal growing time of 1 h,a stirring rate of 150 r/min,and a final cooling temperature of 22℃,the crystals of ammonium heptamolybdate are complete in morphology and prismatic with an average particle size of 337.649μm in a controlled cooling crystallization process.

KeyWords AITranslate

ammonium heptamolybdate ammonium dimolybdate evaporation concentration cooling crystallization morphology particle size

1曹璇,张宝.七钼酸铵的制备及进展[J].铜业工程,2008(4):29-31. 被引量:7

2李莉.焙烧钼精矿制备七钼酸铵新工艺试验研究[J].中国钼业,2015,39(2):41-45. 被引量:3

3唐军利,唐利侠,李辉.二钼酸铵蒸发结晶过程控制[J].中国钼业,2002,26(4):25-27. 被引量:11

4徐芳苓,田建荣.钼酸铵生产废水废气回收利用及综合处理[J].中国钼业,2017,41(5):6-9. 被引量:2

5张宝,夏晓梅,李倩.单相仲钼酸铵制备与表征[J].稀有金属材料与工程,2012,41(S2):781-785. 被引量:2

6李冠军,鲁兴武.铜钼精矿制取钼酸铵试验研究[J].甘肃冶金,2014,36(6):49-50. 被引量:3

7郭军刚,白佩,崔玉青.七钼酸铵连续式结晶工艺优化研究[J].中国钼业,2018,42(1):34-39. 被引量:2

8张旭,郭军刚,白佩,员汝娜,李冬,李稳宏.七钼酸铵制备工艺优化及热力学分析研究[J].西北大学学报:自然科学版,2017,47(6):852-858. 被引量:2

1杨伟,易建,刘锦锐.超低钾低钨二钼酸铵制备工艺研究[J].福建冶金,2023,52(3):44-47.

2冀酉.结晶工艺条件对二钼酸铵产量的影响[J].中国钼业,2023,47(2):56-59.

3段守保,韩平,刘彩霞.多效蒸发工艺处理火电厂脱硫废水的影响研究[J].东北电力技术,2023,44(3):40-44.

4胡义华.利用铬酸酐副产的废酸泥湿法制备无水晶体硫酸氢钠的方法研究[J].当代化工研究,2023(8):182-184.

5徐豪,王琨,樊丽然,吴明君.新型沥青混合料掺加料玉米秸秆纤维的制备工艺及改性方法[J].山东交通学院学报,2023,31(2):102-108.

6李玉萌,程彬瑶,吴秋珏,王玉琴,马岩.铅致蛋鸡卵泡颗粒细胞凋亡及茶多酚的保护作用[J].中国家禽,2023,45(5):65-71.

7李娜,王占忠.离子液体对溶菌酶晶体形态和活性的影响[J].化学工业与工程,2023,40(1):112-119.

8刘慧妮,曾俊杰,伍青龙,胡松,李涛,金会心.异丙醇铝水解制备高纯氧化铝[J].广州化工,2023,51(4):86-90.

9高彦梅,周江平.语义密度、句法复杂度与学科知识编码[J].当代外语研究,2022(6):55-67. 被引量:1

10张益民.有些尿常规异常不用慌[J].保健与生活,2023(5):59-59.

Basic Information:

DOI:

Chinese Library Classification Number:TF841.2[冶金工程—有色金属冶金]

Citation Information:

Ammonium heptamolybdate was prepared by water dissolving-evaporation concentration removal of ammonia-cooling crystallization method using ammonium dimolybdate as raw material.The effects of concentration degree on crystallization product were investigated,and the effects of concentrated liquid density,cooling rate,crystal growing time,and stirring rate on the particle size and morphology of ammonium heptamolybdate were also studied.The results show that ammonium heptamolybdate crystals with a single phase can be prepared by the evaporation concentration-cooling crystallization method after the water dissolution of ammonium dimolybdate.With a concentrated liquid density of about 1.38 g/cm3,a cooling rate of 30℃/h,a crystal growing time of 1 h,a stirring rate of 150 r/min,and a final cooling temperature of 22℃,the crystals of ammonium heptamolybdate are complete in morphology and prismatic with an average particle size of 337.649μm in a controlled cooling crystallization process.

quote

GB/T 7714-2015 [1] CHEN Chao, ZHANG Gui-qing, GUAN Wen-juan, et al. Study on a New Process for the Wet Preparation of Ammonium Heptamolybdate from Ammonium Dimolybdate[J]. Rare Metals and Cemented Carbides, 2023(2): 13-19.
MLA [1] CHEN Chao, et al., "Study on a New Process for the Wet Preparation of Ammonium Heptamolybdate from Ammonium Dimolybdate." Rare Metals and Cemented Carbides, no. 2, 2023, pp. 13-19.
APA [1] CHEN Chao, ZHANG Gui-qing, GUAN Wen-juan, WU Xin-sheng, WU Sheng-xi, LI Qing-gang, & CAO Zuo-ying. (2023). Study on a New Process for the Wet Preparation of Ammonium Heptamolybdate from Ammonium Dimolybdate. Rare Metals and Cemented Carbides(2), 13-19.
IEEE [1] CHEN Chao, ZHANG Gui-qing, GUAN Wen-juan, WU Xin-sheng, WU Sheng-xi, LI Qing-gang, and CAO Zuo-ying, "Study on a New Process for the Wet Preparation of Ammonium Heptamolybdate from Ammonium Dimolybdate," Rare Metals and Cemented Carbides, no. 2, pp. 13-19, 2023. keywords: {ammonium heptamolybdate;ammonium dimolybdate;evaporation concentration;cooling crystallization;morphology;particle size}