Determination and Correlation of Solubility of Yttrium Oxalate in Oxalic Acid Solution AITranslate
Abstract AITranslate
The solubility of yttrium oxalate in oxalic acid solution with different concentration(0.6~1.0 mol/L) was determined by FBRM combined with dynamic method at atmospheric pressure and 318.15~343.15 K.The experimental results show that the solubility of yttrium oxalate in oxalic acid solution with different concentration decreases with the increase of temperature and increases with the increase of oxalic acid concentration.Apelblat equation and polynomial empirical equation are used to fit and correlate the experimental data, and the correlation results are good.When the concentration of oxalic acid is low, the effects of the two models are similar.When the concentration of oxalic acid is high, Apelblat equation is slightly better than polynomial empirical equation.The solution enthalpy and entropy of yttrium oxalate in different oxalic acid solution calculated by Van′t Hoff equation are negative, the dissolution process is a non-spontaneous exothermic process, and the main driving force of this process is entropy driving.
KeyWords AITranslate
1鲍卫民,公锡泰.稀土沉淀条件及形态控制研究[J].稀土,1995,16(2):33-37. 被引量:26
2赵儒铭,王桂玲,周百斌.不同温度和酸度条件下稀土草酸盐溶解度的研究[J].稀土,1995,16(3):12-16. 被引量:4
3赵永志,郝先库,张瑞祥,胡珊珊,马显东,许宗泽.钆元素在碳酸钠、碳酸氢铵溶液中溶解性研究[J].稀土,2013,34(1):37-40. 被引量:2
4柳召刚,李梅,胡艳宏,王觅堂,史振学.Preparation of large particle rare earth oxides by precipitation with oxalic acid[J].稀土学报:英文版,2008,26(2):158-162. 被引量:16
5梅燕,韩业斌,聂祚仁.草酸二甲酯均相沉淀法制备超细CeO_2的研究[J].人工晶体学报,2006,35(4):893-896. 被引量:4
6曾青云,肖培南,赵娟刚,李青,邬鹏,王冬冬.大颗粒氧化钆的沉淀法合成及其合成条件控制的研究[J].有色金属科学与工程,2015,6(5):119-123. 被引量:3
7杨明,吴迪,叶信宇,焦芸芬,吴龙,黄昕,李琴.草酸沉淀反萃余液制备大粒度氧化钕工艺研究[J].有色金属科学与工程,2015,6(1):106-110. 被引量:6
8马莹,李莉娜,王宝荣,乔军,苏允兰,王晶晶.草酸沉淀法制备大颗粒氧化钇工艺研究[J].稀有金属,2010,34(6):950-954. 被引量:9
9马莹,王宝荣,李莉娜,乔军,苏允兰,王晶晶.大粒度氧化钕制备工艺研究[J].稀土,2011,32(5):56-59. 被引量:7
10马莹,王宝荣,李莉娜,乔军,苏允兰,王笃金,王晶晶.Study on the preparation process of large particle cerium oxide[J].稀土学报:英文版,2010(S1):136-138. 被引量:2
1冀旭,孙芳云,赵勤,张晓英,李岩松.藏药中有效成分与功能蛋白的相互作用与相互识别[J].中国民族民间医药,2021,30(12):54-60. 被引量:1
2杨忠勇,钱门亮,纪道斌,周哲轩,姚仕明,范中亚.香溪河初冬降温过程中垂向混合结构特征分析[J].中国环境科学,2021,41(6):2862-2870. 被引量:2
3张君松,廖京京,韦天国,龙冲生.锆合金氧化膜在真空退火过程中的氧扩散行为[J].稀有金属材料与工程,2021,50(5):1590-1595.
4程春祖,徐中凯,张东,徐纪刚,刘聘.溶解温度及NMMO溶剂浓度对纤维素溶解的影响[J].纺织高校基础科学学报,2021,34(2):1-6. 被引量:3
5熊晨辰,刘叠,纪天鸿,王皓宇,郑建友,任付伟,赵骧,白静.Ni-Mn-Sn合金缺陷稳定性和磁性能的第一性原理研究[J].中国科学:物理学、力学、天文学,2021,51(6):140-147.
6罗垒,高永,刘晓达.基于西安咸阳机场近20年降水特征及一次短时强降水的分析[J].地球科学前沿(汉斯),2021,11(6):892-902.
7马旭,常森,王涛,陆佳春,姜楠.修正等时试井资料解释改进方法对比[J].钻采工艺,2021,44(3):67-71. 被引量:1
8吴迪迪,李舢,David CHEW,刘铁翊,郭东海.中亚造山带东南缘二叠纪-三叠纪花岗质岩浆演化对增生-碰撞过程的制约[J].中国科学:地球科学,2021,51(6):906-926. 被引量:8
Basic Information:
DOI:
Chinese Library Classification Number:O645.12[理学—物理化学]
Citation Information:
The solubility of yttrium oxalate in oxalic acid solution with different concentration(0.6~1.0 mol/L) was determined by FBRM combined with dynamic method at atmospheric pressure and 318.15~343.15 K.The experimental results show that the solubility of yttrium oxalate in oxalic acid solution with different concentration decreases with the increase of temperature and increases with the increase of oxalic acid concentration.Apelblat equation and polynomial empirical equation are used to fit and correlate the experimental data, and the correlation results are good.When the concentration of oxalic acid is low, the effects of the two models are similar.When the concentration of oxalic acid is high, Apelblat equation is slightly better than polynomial empirical equation.The solution enthalpy and entropy of yttrium oxalate in different oxalic acid solution calculated by Van′t Hoff equation are negative, the dissolution process is a non-spontaneous exothermic process, and the main driving force of this process is entropy driving.
quote
| GB/T 7714-2015 | [1] LIU Qing-sheng, CHENG Hua-jin, WANG Xue-zhong, et al. Determination and Correlation of Solubility of Yttrium Oxalate in Oxalic Acid Solution[J]. Rare Metals and Cemented Carbides, 2021(3): 9-15. |
| MLA | [1] LIU Qing-sheng, et al., "Determination and Correlation of Solubility of Yttrium Oxalate in Oxalic Acid Solution." Rare Metals and Cemented Carbides, no. 3, 2021, pp. 9-15. |
| APA | [1] LIU Qing-sheng, CHENG Hua-jin, WANG Xue-zhong, & LI Hua-jie. (2021). Determination and Correlation of Solubility of Yttrium Oxalate in Oxalic Acid Solution. Rare Metals and Cemented Carbides(3), 9-15. |
| IEEE | [1] LIU Qing-sheng, CHENG Hua-jin, WANG Xue-zhong, and LI Hua-jie, "Determination and Correlation of Solubility of Yttrium Oxalate in Oxalic Acid Solution," Rare Metals and Cemented Carbides, no. 3, pp. 9-15, 2021. keywords: {yttrium oxalate;solubility;Apelblat equation;polynomial empirical equation;thermodynamics} |