Study on Preparation of Ferrosilicon Alloy Containing Titanium by Carbothermal Reduction of Polymetallic Ore AITranslate

School of Metallurgy,Northeastern University;School of Metallurgy,Northeastern University;School of Metallurgy,Northeastern University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Ferrosilicon alloy containing titanium was prepared by carbothermal reduction and induction melting with a polymetallic ore from Xinjiang as raw material.The effects of carbothermal reduction temperature, carbon content and holding time on metal recovery, alloy composition and slag phase were studied by single factor experiment.The experimental results show that under the optimum single factor conditions of 2 073 K carbothermal temperature, 0.8 times of theoretical carbon content and 0.5 h holding time, the highest metal recovery is 52%.The contents(mass fraction) of Al, Si, Fe, Ti and C in alloy are 0.338%,39.74%,45.54%,6.84% and 0.058%,respectively, and the main phase of reduced slag is MgAl2O4.

KeyWords AITranslate

polymetallic ore carbothermal reduction induction smelting ferrosilicon alloy high-value utilization

1杨合群,艾宁,毛自力,武丹.宁夏硅石利用之二:生产硅铁[J].西北地质,2015,48(4):87-87. 被引量:1

2尤晶,王耀武.皮江法炼镁还原机理[J].过程工程学报,2019,19(3):560-566. 被引量:9

3卢学峰,南雪丽,郭鑫.利用废渣冶炼回收硅铁的研究[J].铁合金,2009,40(5):42-44. 被引量:2

4鲁慧慧,张朝晖,刘佰龙,宋世雄.冶金焦粉压块制备硅铁合金的工艺分析[J].科技创新与应用,2012,2(10Z):111-112. 被引量:1

5李云海.感应电炉冶炼75%硅铁的试验生产[J].甘肃冶金,2007,29(6):58-59. 被引量:1

6李雪琴,潘飞飞,贺文超,邱杰,吕学伟.硅铁合金离心粒化工艺[J].中国冶金,2018,28(9):77-82. 被引量:6

7袁建军,马美荣,徐佳卉.浅述硅铁合金生产产量与单耗及成本的关系[J].铁合金,2017,48(4):7-13. 被引量:4

8袁建军.制备复合熔剂球重熔生产精炼硅铁合金技术研究[J].铁合金,2017,48(8):17-20. 被引量:3

9于志辉,刘丹丹,寇艳娜.锂离子电池负极材料多孔硅/硅铁合金的制备及性能[J].北京工业大学学报,2017,43(2):278-284. 被引量:4

10周文娟.矿热炉生产超低碳硅铁合金工艺技术的研究与应用[J].甘肃冶金,2015,37(2):44-45. 被引量:4

1郭子洋,钱永芳,孙永丰.沥青和PAN的静电纺碳纳米级纤维膜的制备及表征[J].产业用纺织品,2021,39(3):15-23. 被引量:2

2吴军,郑锋华,文春海,谭春雷,王红强,李庆余.三相碳改性磷酸铁锂复合材料的制备及其电化学性能研究[J].矿冶工程,2021,41(3):138-142. 被引量:4

3张禛,郑鑫,张小联.钙热还原氧化铪制备铪粉的研究[J].稀有金属与硬质合金,2021,49(3):58-63.

4邓杰,宋新莉,孙新军,贾涓,梁小凯,范丽霞.含钛中锰钢淬火-配分组织及力学性能[J].钢铁,2021,56(6):103-111. 被引量:16

5龙平勇,杜浪.有色金属真空冶金技术研究[J].科学大众:科技创新,2021(6):164-164.

6刘芳辰.铸态钇锆合金组织结构及硬度研究[J].有色金属与稀土应用,2020(4):1-9.

7邓超群,王海北,刘三平,周起帆,李强.废三元锂电池碳热还原焙烧热解研究[J].有色金属:冶炼部分,2021(7):98-104. 被引量:3

8张金池,张福元,赵卓,徐亮.铜阳极泥分铜液高效分离稀散金属碲[J].稀有金属,2021,45(3):312-321. 被引量:2

9张国华,潘辉,陈先友,陆开臣,刘洪嶂.焙砂下料槽喷淋管在湿法炼锌中的应用[J].装备维修技术,2021(16):0203-0203.

10陶成,戴曦.铁矾渣富氧强化还原挥发熔炼工艺研究[J].冶金工程,2021,8(2):76-86.

Basic Information:

DOI:

Chinese Library Classification Number:TF111[冶金工程—冶金物理化学]

Citation Information:

Ferrosilicon alloy containing titanium was prepared by carbothermal reduction and induction melting with a polymetallic ore from Xinjiang as raw material.The effects of carbothermal reduction temperature, carbon content and holding time on metal recovery, alloy composition and slag phase were studied by single factor experiment.The experimental results show that under the optimum single factor conditions of 2 073 K carbothermal temperature, 0.8 times of theoretical carbon content and 0.5 h holding time, the highest metal recovery is 52%.The contents(mass fraction) of Al, Si, Fe, Ti and C in alloy are 0.338%,39.74%,45.54%,6.84% and 0.058%,respectively, and the main phase of reduced slag is MgAl2O4.

quote

GB/T 7714-2015 [1] HAO Jun, WANG Kun, ZHANG Ting-an. Study on Preparation of Ferrosilicon Alloy Containing Titanium by Carbothermal Reduction of Polymetallic Ore[J]. Rare Metals and Cemented Carbides, 2021(3): 16-23.
MLA [1] HAO Jun, et al., "Study on Preparation of Ferrosilicon Alloy Containing Titanium by Carbothermal Reduction of Polymetallic Ore." Rare Metals and Cemented Carbides, no. 3, 2021, pp. 16-23.
APA [1] HAO Jun, WANG Kun, & ZHANG Ting-an. (2021). Study on Preparation of Ferrosilicon Alloy Containing Titanium by Carbothermal Reduction of Polymetallic Ore. Rare Metals and Cemented Carbides(3), 16-23.
IEEE [1] HAO Jun, WANG Kun, and ZHANG Ting-an, "Study on Preparation of Ferrosilicon Alloy Containing Titanium by Carbothermal Reduction of Polymetallic Ore," Rare Metals and Cemented Carbides, no. 3, pp. 16-23, 2021. keywords: {polymetallic ore;carbothermal reduction;induction smelting;ferrosilicon alloy;high-value utilization}