Study on Electrochemical Behavior of Y(Ⅲ) in Molten YF3-LiF AITranslate
Abstract AITranslate
The electrochemical reduction process of Y(Ⅲ) and the cathode behavior of Y2O3 in YF3-LiF molten salt system were studied by cyclic voltammetry.The results indicate that the reduction potential of Y(Ⅲ) on molybdenum electrode is-0.95 V(vs.Pt) in YF3-LiF molten salt system, and the reaction is a quasi reversible reaction that transfers three electrons in one step.The redox peak does not change with the scanning speed, which indicates that the reaction is a quasi reversible reaction with great reversibility.The peak current Ip is linearly related to v1/2,so the reaction is controlled by diffusion with diffusion coefficient of 3.626 4×10-8 cm2/s.The addition of Y2O3 into molten salt contributes to reducing reduction potential of Y(Ⅲ) and has a certain depolarization effect.There are three different reduction current peaks in the reduction process of Y(Ⅲ) on the iron electrode.Yttrium-iron alloy phase is formed by underpotential deposition and yttrium metal is formed by electroreduction.
KeyWords AITranslate
1陈甲斌.稀土资源产业发展前景分析[J].世界有色金属,2004(5):9-10. 被引量:3
2杨绮琴,丘开容,刘冠昆,郑锡光.氯化物熔体中钇的电还原和合金化[J].中国稀土学报,1994,12(2):116-119. 被引量:3
3段淑贞,周春根,乔芝郁,翟清,武世民.循环伏安法用于钇在钼和镍电极上的电极过程研究[J].中国稀土学报,1992,10(2):116-119. 被引量:3
4赵立忠,段淑贞,魏寿昆,李国勋.钇离子在氟化物体系中的电化学还原[J].中国稀土学报,1993,11(3):271-273. 被引量:4
5尹祖平,郝占云,陈文亮,蔡安洪.氟盐体系电解制备钇铁合金几种原料的比较[J].稀土,1991,12(3):70-72. 被引量:4
6韩伟,赵强,王季,李梅,刘文凯,张密林,杨晓光,孙杨.Electrochemical behavior of Y(Ⅲ) and preparation of Y-Ni intermetallic compounds in molten LiCl-KCl salts[J].稀土学报:英文版,2017,35(1):90-97. 被引量:4
7颜永得,杨晓南,黄莹,薛云,张密林,韩伟,张志俭.LiCl-KCl熔盐中共沉积直接电化学形成不同相Al-Y合金(英文)[J].稀有金属材料与工程,2016,45(2):272-276. 被引量:1
8张常在,李国栋,云月厚.电化学脱氧提纯稀土金属钇(Y)的物理化学问题[J].稀有金属材料与工程,2006,35(5):736-739. 被引量:5
9薛云,颜永得,张密林,韩伟,张志俭.Electrochemical formation of Mg-Li-Y alloys by co-deposition of magnesium, lithium and yttrium ions in molten chlorides[J].稀土学报:英文版,2012,30(10):1048-1054. 被引量:5
10李斌川,李师居,孔亚鹏,陈建设,刘奎仁,韩庆.CeO2在CeF3-LiF-BaF2熔盐中的溶解过程及电化学行为[J].稀有金属材料与工程,2020,49(3):749-754. 被引量:1
1赵雪静,孙晓君,魏金枝,张婷,刘欣然.电化学法原位合成Zn/Co-ZIF材料及电容性能[J].复合材料学报,2021,38(5):1543-1550. 被引量:1
2童孟良,唐淑贞,王罗强.锌铝水滑石作为锌负极材料的电化学性能研究[J].电源技术,2021,45(6):753-755. 被引量:1
3赵菲,靳东.模拟沿海工业大气环境中2A12铝合金的加速腐蚀行为[J].腐蚀与防护,2021,42(4):19-23. 被引量:5
4无.韩国科学技术研究院开发电还原CO_(2)制乙烯的电极与催化剂[J].石油炼制与化工,2021,52(7):95-95.
5杨程,朱媚柔,龚现玲,高爱英,许新胜.乙腈-水和乙二醇-水均相溶液中光诱导杜醌激发三重态与色氨酸、酪氨酸的氢原子转移反应[J].化学物理学报(英文),2021,34(3):256-262.
6何登武,李冠超,李小燕,王杨,王昱莹,付晓辉.CuInS_(2)光催化材料制备及光催化还原溶液中U(Ⅵ)的性能[J].有色金属工程,2021,11(7):18-24.
7李人骏,张玲,张晓序,王志刚,胡於江.TiO_(2)的添加对铝铬固溶体烧结动力学的影响[J].硅酸盐通报,2021,40(6):2104-2109.
8谢凡,时凯华,顾金宝.传统方法制备超细WC粉末的质量控制研究进展[J].稀有金属与硬质合金,2021,49(3):31-36. 被引量:2
9杨泽胜,陈国俊,张相杰,程宽,龙明亮,刘同旭.微生物介导硝酸盐还原耦合亚铁氧化过程的动力学及其影响因素[J].微生物学报,2021,61(6):1536-1550.
Basic Information:
DOI:
Chinese Library Classification Number:O646.541[理学—物理化学]
Citation Information:
The electrochemical reduction process of Y(Ⅲ) and the cathode behavior of Y2O3 in YF3-LiF molten salt system were studied by cyclic voltammetry.The results indicate that the reduction potential of Y(Ⅲ) on molybdenum electrode is-0.95 V(vs.Pt) in YF3-LiF molten salt system, and the reaction is a quasi reversible reaction that transfers three electrons in one step.The redox peak does not change with the scanning speed, which indicates that the reaction is a quasi reversible reaction with great reversibility.The peak current Ip is linearly related to v1/2,so the reaction is controlled by diffusion with diffusion coefficient of 3.626 4×10-8 cm2/s.The addition of Y2O3 into molten salt contributes to reducing reduction potential of Y(Ⅲ) and has a certain depolarization effect.There are three different reduction current peaks in the reduction process of Y(Ⅲ) on the iron electrode.Yttrium-iron alloy phase is formed by underpotential deposition and yttrium metal is formed by electroreduction.
quote
| GB/T 7714-2015 | [1] HUANG Hai-tao, YU Bing, YAN Qi-cao, et al. Study on Electrochemical Behavior of Y(Ⅲ) in Molten YF3-LiF[J]. Rare Metals and Cemented Carbides, 2021(3): 5-8. |
| MLA | [1] HUANG Hai-tao, et al., "Study on Electrochemical Behavior of Y(Ⅲ) in Molten YF3-LiF." Rare Metals and Cemented Carbides, no. 3, 2021, pp. 5-8. |
| APA | [1] HUANG Hai-tao, YU Bing, YAN Qi-cao, CHEN Guo-hua, ZHANG Quan-jun, & LIU Yu-bao. (2021). Study on Electrochemical Behavior of Y(Ⅲ) in Molten YF3-LiF. Rare Metals and Cemented Carbides(3), 5-8. |
| IEEE | [1] HUANG Hai-tao, YU Bing, YAN Qi-cao, CHEN Guo-hua, ZHANG Quan-jun, and LIU Yu-bao, "Study on Electrochemical Behavior of Y(Ⅲ) in Molten YF3-LiF," Rare Metals and Cemented Carbides, no. 3, pp. 5-8, 2021. keywords: {yttrium oxide;oxidoreduction;yttrium-iron alloy;cyclic voltammetry;diffusion control} |