Ion Plating of Cu-Al-In Alloy on the Surface of NdFeB Permanent Magnetism Alloy AITranslate
Abstract AITranslate
The principle of ion plating has been analyzed in this paper, And a noveltechnology for ion plating of imitation gold Cu-Al-in alloy on the surface of NdFeB permanentmagnetism alloy has been studied. The reasonable technical conditions for obtaining homogeneousbeautiful coating layer with tiny crystal particles were as follows: workpiece bias voltage: 200 V,main arc current: 5 A 2 0. 25 A, optimum workpiece height: 120 mm, evaporation heating power:11 kW, PAr: 1. 33 Pa~0. 0133 Pa, time: 30 min.
KeyWords AITranslate
1贺琦军,李卫.钕铁硼永磁材料防腐蚀研究发展[J].金属功能材料,2001,8(5):8-13. 被引量:33
1岳晓岱,郭志猛,罗骥.烧结NdFeB磁体的热浸镀铝工艺研究[J].粉末冶金工业,2008,18(6):23-26. 被引量:2
2马宗耀,谢发勤,刘道新.NdFeB永磁体阳极电泳新工艺[J].电镀与环保,2004,24(6):33-34. 被引量:1
3胡艳峰,申宏,王岱林.旋进旋涡流量计计量误差分析[J].工业计量,2005,15(3):33-34. 被引量:1
4于升学,陈玲.烧结型NdFeB永磁体锌铬膜处理工艺及性能研究[J].中国稀土学报,2006,24(1):65-69. 被引量:5
5王文光,柴立民,刘小平,黄可淼.铁氧体/NdFeB压合型柔性磁体的耐腐蚀性能[J].磁性材料及器件,2007,38(5):39-41. 被引量:1
6唐杰,魏成富,赵导文,林红,徐伟.4种涂层对NdFeB磁体耐腐蚀性能和磁性能的影响[J].材料保护,2009,42(5):17-19. 被引量:2
7李广宇,孟瑶,娄桂艳.水溶性缓蚀剂对钕铁硼永磁材料的防腐蚀性能[J].材料保护,2009,42(12):49-51. 被引量:2
8陈焕铭,王冬玲,高亚红,郝旭暖,谷玉丹,付鹏.NdFeB磁性材料化学镀非晶态Ni-W-P合金及其相转变行为[J].宁夏大学学报:自然科学版,2010,31(1):49-51. 被引量:3
9岳晓岱,王效光.烧结NdFeB永磁体的热浸镀铝工艺研究[J].失效分析与预防,2010,5(2):82-84.
10付鹏,王憨鹰,王冬玲,高亚红,高作宁,陈焕铭.NdFeB磁性材料化学镀Ni-W-P合金及其电化学行为研究[J].宁夏工程技术,2010,9(4):349-352.
1唐多光,周自强,葛建生,陆庆桃.抗变色仿金合金的研究[J].金属科学与工艺,1991,10(1):77-82. 被引量:18
2朱安印,陈景林,李周,罗利阳,雷前,张良,张婉.新型仿金铜合金的热变形行为(英文)[J].中国有色金属学报:英文版,2013,23(5):1349-1355. 被引量:7
3陆原,沈燕.FJ18仿金合金材料的研究[J].广西冶金,1992(1):37-43.
4华宏慈,王葛亚,徐庆镇,金慧娟,许桂琴.NdFeB永磁材料氧化行为的研究[J].金属学报,1991,27(1). 被引量:2
5郑国桢,林庆文.NdFeB永磁材料表面防护技术研究[J].广东机械学院学报,1996,14(4):49-54.
6黄刚.NdFeB永磁防锈处理的新工艺[J].新技术新工艺,1993(5):38-38.
7廖秋慧,王伟.纳米复合NdFeB永磁材料的研究进展[J].热加工工艺,2005,34(10):62-64. 被引量:4
8李维清,陈志勇,王兴华.电动自行车用无刷直流电动机及其驱动系统[J].微电机,2003,36(1):10-11. 被引量:3
9刘颖,张然,李军,徐建川,高升吉,涂铭旌.粘结NdFeB永磁的应用与发展[J].新材料产业,2006(7):46-48.
10周寿增,唐伟忠,王润.烧结NdFeB永磁合金的边界显微结构与磁硬化[J].金属学报,1990,26(4). 被引量:18
Basic Information:
DOI:
Chinese Library Classification Number:TG174.442[金属学及工艺—金属表面处理];TM273.051[一般工业技术—材料科学与工程]
Citation Information:
The principle of ion plating has been analyzed in this paper, And a noveltechnology for ion plating of imitation gold Cu-Al-in alloy on the surface of NdFeB permanentmagnetism alloy has been studied. The reasonable technical conditions for obtaining homogeneousbeautiful coating layer with tiny crystal particles were as follows: workpiece bias voltage: 200 V,main arc current: 5 A 2 0. 25 A, optimum workpiece height: 120 mm, evaporation heating power:11 kW, PAr: 1. 33 Pa~0. 0133 Pa, time: 30 min.
quote
| GB/T 7714-2015 | [1] LIU Fei-long, WU Li-jue, CHAI Li-yuan, et al. Ion Plating of Cu-Al-In Alloy on the Surface of NdFeB Permanent Magnetism Alloy[J]. Rare Metals and Cemented Carbides, 1998(2): 23-26. |
| MLA | [1] LIU Fei-long, et al., "Ion Plating of Cu-Al-In Alloy on the Surface of NdFeB Permanent Magnetism Alloy." Rare Metals and Cemented Carbides, no. 2, 1998, pp. 23-26. |
| APA | [1] LIU Fei-long, WU Li-jue, CHAI Li-yuan, & ZHONG Hai-yun. (1998). Ion Plating of Cu-Al-In Alloy on the Surface of NdFeB Permanent Magnetism Alloy. Rare Metals and Cemented Carbides(2), 23-26. |
| IEEE | [1] LIU Fei-long, WU Li-jue, CHAI Li-yuan, and ZHONG Hai-yun, "Ion Plating of Cu-Al-In Alloy on the Surface of NdFeB Permanent Magnetism Alloy," Rare Metals and Cemented Carbides, no. 2, pp. 23-26, 1998. keywords: {ion plating;NdFeB permanent magnetism alloy;imitation gold Cu-Al-in alloy} |