Effect of Al Content upon TiB_2 SHS Process AITranslate

New Materials Research Institute of Wuhan University of Technology;New Materials Research Institute of Wuhan University of Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Tde particles in Al matrix were prepared successfully from powders of Ti, B andAl by means of SHS technique. The effect of aluminium content and the temperature of synthesison the SHS process, phase comPOsition and microstructure of the reaction products have beenstudied. The mechanism involved in the synthesis of TiB2 in Al matrix has been discussed. Theresults show that TiB2 particles may form in Al matrix at temperatures even about 800 t owingto the exothermic reaction between Ti and Al POwders. The presence of Al may hinder thereaction between Ti and B powders. The size of TiB2 particles is 5. 0 to 0. 5 pm, according to theAl content of the system.

KeyWords AITranslate

TiB_2 Al content Ti-B system SHS

1A. R. C. Westwood. Materials for advanced studies and devices[J] 1988,Metallurgical Transactions A(4):749~758

1蔡利芳,张永忠,席明哲,石力开.原位合成法在材料制备中的应用及进展[J].金属热处理,2005,30(10):1-6. 被引量:32

1刘志明,谢成,王海英,吴鹏,孟围.纳米纤维素/磁性纳米球的原位合成及表征[J].功能材料,2012,43(12):1627-1631. 被引量:9

2缪燕平,何柏林.金属间化合物/陶瓷基复合材料的制备及发展[J].华东交通大学学报,2007,24(2):131-134. 被引量:4

3黄铭刚,鲁世强,肖璇,胡平,李鑫.球磨时间对软第二相韧化Cr_2Nb基复合材料组织与性能的影响[J].热加工工艺,2008,37(16):7-10.

4牛立斌,许云华,蔡美,张夏妮.原位合成WC_p/W丝增强铁基复合材料的组织与性能[J].金属热处理,2009,34(6):49-52. 被引量:1

5王亚娟,史楷歧,邵双喜,单志华.原位协同聚合反应在制革中的应用[J].皮革科学与工程,2009,19(4):28-32. 被引量:1

6于秀平,沈以赴,顾冬冬.激光烧结法制备原位增强型多孔镍基复合材料[J].稀有金属与硬质合金,2009,37(4):11-14. 被引量:7

7李少峰,刘维良,彭牛生,张小锋.金属陶瓷刀具材料研究进展[J].陶瓷学报,2010,31(1):140-144. 被引量:14

8卜蕾,林同伟,熊宁,陈飞雄,周武平.Ti_3AlC_2陶瓷材料制备工艺研究进展[J].粉末冶金工业,2012,22(1):48-52. 被引量:2

9陈颢,李剑波,羊建高.硬质合金回收研究进展及发展趋势[J].有色金属科学与工程,2012,3(5):18-22. 被引量:17

10樊宁霞,王芬,朱建锋.Al_2O_3-NbAl/TiAl基高温复合材料的研究[J].陕西科技大学学报:自然科学版,2012,30(6):32-35. 被引量:1

1刘永合,殷声,赖和怡.自蔓燃高温合成碳化物陶瓷[J].粉末冶金技术,1999,17(2):130-137. 被引量:7

2孙晓冬,傅正义,袁润章.TiH_2对TiB_2自蔓延高温合成过程的影响[J].粉末冶金技术,1998,16(1):17-20. 被引量:1

3宋文杰,钟晖,袁艳,杨建文,戴艳阳,钟海云.真空碳热还原法制备高纯TiB_2粉末[J].稀有金属与硬质合金,2006,34(1):9-13. 被引量:1

4周书助,彭卫珍.硼热/碳热还原TiO_2合成高纯TiB_2粉末[J].硬质合金,2004,21(1):27-31. 被引量:1

5孙天康,汪成刚,卢一鸣.自蔓燃高温合成CrB2[J].粉末冶金技术,1998,16(4):254-255. 被引量:4

6殷声,赖和怡.自蔓燃高温合成法(SHS)的发展[J].粉末冶金技术,1992,10(3):223-227. 被引量:27

7缪曙霞,殷声,李建勇,赖和怡.自蔓燃高温合成法(SHS)制备碳化钨[J].中国有色金属学报,1994,4(2):79-81. 被引量:6

8赵昆渝,严丙勇,李智东,李莉,朱心昆,段云彪,刘国玺,马秋花,葛伟萍.机械合金化制备TiB_2粉末的机理研究[J].机械工程材料,2004,28(3):25-27. 被引量:4

9亓家钟.粉末冶金文摘[J].粉末冶金技术,2008,26(1):73-73.

10黄铁枢,黄腾政,崔玉梅,步丰满.自蔓燃-离心法制造陶瓷内衬钢管技术[J].新技术新工艺,1996(5):35-37. 被引量:14

Basic Information:

DOI:

Chinese Library Classification Number:TF123.32[冶金工程—粉末冶金]

Citation Information:

Tde particles in Al matrix were prepared successfully from powders of Ti, B andAl by means of SHS technique. The effect of aluminium content and the temperature of synthesison the SHS process, phase comPOsition and microstructure of the reaction products have beenstudied. The mechanism involved in the synthesis of TiB2 in Al matrix has been discussed. Theresults show that TiB2 particles may form in Al matrix at temperatures even about 800 t owingto the exothermic reaction between Ti and Al POwders. The presence of Al may hinder thereaction between Ti and B powders. The size of TiB2 particles is 5. 0 to 0. 5 pm, according to theAl content of the system.

quote

GB/T 7714-2015 [1] SUN Xiao-dong, YUAN Run-zhang. Effect of Al Content upon TiB_2 SHS Process[J]. Rare Metals and Cemented Carbides, 1998(2): 27-31.
MLA [1] SUN Xiao-dong, and YUAN Run-zhang. "Effect of Al Content upon TiB_2 SHS Process." Rare Metals and Cemented Carbides, no. 2, 1998, pp. 27-31.
APA [1] SUN Xiao-dong, & YUAN Run-zhang. (1998). Effect of Al Content upon TiB_2 SHS Process. Rare Metals and Cemented Carbides(2), 27-31.
IEEE [1] SUN Xiao-dong and YUAN Run-zhang, "Effect of Al Content upon TiB_2 SHS Process," Rare Metals and Cemented Carbides, no. 2, pp. 27-31, 1998. keywords: {TiB_2;Al content ,Ti-B system ,SHS}