Study of Ge Recovery with H Extractant from H_2SO_4-leached Solution of Zinc Oxide AITranslate

Zhuzhou Switching Factory Rare and Words Plant
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Study is made on Ge recovery from H2SO4-leached supernatant (0. 02 ~0' 03 g/lGe), using 'H' kerosene and butyl octano TBP as extractant. Resljlts show that the said processfeatures lower reagent consumption and over 22% Ge content in concentrate.

KeyWords AITranslate

H_2SO_4-leached zinc oxide solution ' H' extractant butyl octanol TBP Gerecovery

1肖华利.“B”试剂回收锗新工艺在我厂的应用及改进[J].稀有金属与硬质合金,1996,24(1):11-14. 被引量:2

1周智华,莫红兵.稀散金属锗富集回收技术的研究进展[J].中国矿业,2006,15(2):64-67. 被引量:10

1普世坤,严云南,兰尧中.氢氧化钠预处理-盐酸蒸馏法回收锗的工艺研究[J].昆明理工大学学报:自然科学版,2012,37(2):19-22. 被引量:4

2王晓华,陶龙政,郑永萍.燃煤飞灰氯化浸出提取锗的研究[J].内蒙古石油化工,2007,33(8):11-12. 被引量:3

3普世坤,严云南,陈代凤.硅-锗合金废料中锗的回收研究[J].中国有色冶金,2011,40(4):57-59. 被引量:9

4周虹,刘建,吴书凤.泡沫塑料法在高浓度盐酸溶液中吸附回收锗[J].应用化工,2011,40(11):1871-1874. 被引量:2

5普世坤,何贵.太阳能电池用锗单晶片加工废料综合回收利用研究[J].云南冶金,2011,40(6):31-34. 被引量:1

6普世坤,兰尧中.从粉煤灰中回收锗的湿法工艺研究[J].稀有金属与硬质合金,2012,40(5):15-17. 被引量:10

7何静,王小能,刘明海,王继民,唐谟堂,鲁君乐,王涛,罗超,郭瑞,蓝明艳.含锗真空炉渣在HCl-CaCl_2-H_2O体系中浸出锗的动力学研究[J].稀有金属材料与工程,2013,42(6):1258-1263. 被引量:2

8刘爽,鲁力,柳德华,康健,黄鹏.我国稀有及稀散金属综合利用技术综述[J].矿产综合利用,2013(5):10-12. 被引量:6

9彭伟校.氯化蒸馏残渣回收锗工艺研究[J].有色金属:冶炼部分,2017(1):53-56. 被引量:1

10李长林,杨再磊,谢高,薛丹,窦辉,张弦,滕文,普世坤.氟化焙烧预处理提取低品位锗精矿中锗的工艺研究[J].稀有金属与硬质合金,2017,45(5):22-26. 被引量:2

1车文婷,肖金娥,王少雄.采用离心萃取从氧化锌酸浸液中回收铟的实践[J].湖南有色金属,1994,10(6):366-369.

2肖华利.株冶回收锗技术的变革与展望[J].有色冶炼,1996,25(6):54-57. 被引量:7

3肖金娥,陈春祥,车文婷.离心萃取氧化锌酸浸液中铟锗新工艺的研究[J].湖南有色金属,1992(6):358-362.

4张秀莉.环烷酸中异辛醇的简便测定方法[J].吉林工学院学报:自然科学版,1999,20(1):37-39. 被引量:1

5郑顺德,陈世民,林兴铭,李裕后,李俊红.从锌渣浸渣中综合回收铟锗铅银的试验研究[J].有色冶炼,2001,30(2):34-35. 被引量:25

6童长仁,武金朋,李俊朝,张鹏,刘秀.TBP与N1923协同萃取铜电解液中的砷锑铋[J].有色金属:冶炼部分,2012(5):17-20. 被引量:20

7李亮星,黄茜琳,廖春发,童长仁,黄金堤,姜平国.N235-硫酸-助萃体系锑萃取性能研究[J].中南大学学报:自然科学版,2014,45(7):2151-2156. 被引量:1

8邹小平,张邦胜,张磊,王海北.酸性加压浸出液中钼的萃取分离[J].中国资源综合利用,2014,32(4):13-16. 被引量:2

9凌克奇,刘一宁.长链烷基羟肟酸离心萃锗试验[J].有色金属:冶炼部分,1998(5):37-38. 被引量:1

10包福毅,朱大和,方军,杨明德,张志庚.氯化浸出镍溶液中钴的分离和回收[J].有色金属,1995,47(1):57-61. 被引量:6

Basic Information:

DOI:

Chinese Library Classification Number:TF840.52[冶金工程—有色金属冶金]

Citation Information:

Study is made on Ge recovery from H2SO4-leached supernatant (0. 02 ~0' 03 g/lGe), using 'H' kerosene and butyl octano TBP as extractant. Resljlts show that the said processfeatures lower reagent consumption and over 22% Ge content in concentrate.

quote

GB/T 7714-2015 [1] XIAO Hua-li. Study of Ge Recovery with H Extractant from H_2SO_4-leached Solution of Zinc Oxide[J]. Rare Metals and Cemented Carbides, 1998(2): 19-22.
MLA [1] XIAO Hua-li. "Study of Ge Recovery with H Extractant from H_2SO_4-leached Solution of Zinc Oxide." Rare Metals and Cemented Carbides, no. 2, 1998, pp. 19-22.
APA [1] XIAO Hua-li. (1998). Study of Ge Recovery with H Extractant from H_2SO_4-leached Solution of Zinc Oxide. Rare Metals and Cemented Carbides(2), 19-22.
IEEE [1] XIAO Hua-li, "Study of Ge Recovery with H Extractant from H_2SO_4-leached Solution of Zinc Oxide," Rare Metals and Cemented Carbides, no. 2, pp. 19-22, 1998. keywords: {H_2SO_4-leached zinc oxide solution,' H' extractant, butyl octanol, TBP, Gerecovery}