Unraveling role of double-exchange interaction in electrochemical water oxidation by external magnetic field AITranslate

National Laboratory of Solid State Microstructures and Jiangsu Provincial Key Laboratory for Nanotechnology;National Laboratory of Solid State Microstructures and Jiangsu Provincial Key Laboratory for Nanotechnology;National Laboratory of Solid State Microstructures and Jiangsu Provincial Key Laboratory for Nanotechnology;National Laboratory of Solid State Microstructures and Jiangsu Provincial Key Laboratory for Nanotechnology;National Laboratory of Solid State Microstructures and Jiangsu Provincial Key Laboratory for Nanotechnology;National Laboratory of Solid State Microstructures and Jiangsu Provincial Key Laboratory for Nanotechnology
AITranslate
Publisher: Youke Publish Co., Ltd.
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Double-exchange(DE) interaction plays an important role in electrocatalytic oxygen evolution reaction(OER).However,precise achievement of DE interaction often requires foreign dopants or vacancy engineering,leading to destabilization of the catalysts and deterioration of performance.By contrast,the utilization of environmentally friendly,contactless,and continuously adjustable magnetic fields to study the OER process is profitable to avoid aforementioned interference factors and further elucidate the direct relationship0.5between DE interaction and OER activity.Here,by using cobalt hydroxide carbonate(Co(OH)(CO3)·xH2O,CoHC) nanostructures as a proof-of-concept study,external magnetic fields are carefully implemented to verify the role of DE interaction during water oxidation reaction.Detailed studies reveal that external magnetic fields effectively enhance the reaction rate of the catalyst,the overpotential decreases from 386 to 355 mV(100 mA·cm-2),while Tafel slopes drastically decline from 93 to 67 mV·dec-1(1.0 T).Moreover,magnetic field increment exhibits robust durability.Through in situ Raman and impedance measurements under external field,it can be found that magnetic field promotes the electron migration between Co2+ and Co3+ in the CoHC catalysts with the assistance of DE interactions,thus boosting the OER efficiency.

KeyWords AITranslate

Magnetic field Double-exchange(DE)interaction ELECTROCATALYSIS Oxygen evolution reaction(OER) Cobalt hydroxide carbonate

1Zeng-Xi Wei,Ya-Ting Zhu,Jin-Yuan Liu,Zhi-Cheng Zhang,Wen-Ping Hu,Hui Xu,Yue-Zhan Feng,Jian-Min Ma.Recent advance in single-atom catalysis[J].Rare Metals,2021,40(4):767-789. 被引量:8

2李丽,石永霞,侯曼,张志成.铜基材料电催化二氧化碳还原反应的研究进展[J].稀有金属,2022,46(6):681-694. 被引量:9

3Zheng-Xuan Yang,Xiu-Gang Li,Qi-Lu Yao,Zhang-Hui Lu,Ning Zhang,Jun Xia,Kai Yang,Yu-Qing Wang,Kan Zhang,Hai-Zhen Liu,Liu-Ting Zhang,Huai-Jun Lin,Qing-Jun Zhou,Fang Wang,Zhi-Ming Yu,Jian-Min Ma.2022 roadmap on hydrogen energy from production to utilizations[J].Rare Metals,2022,41(10):3251-3267. 被引量:4

4Li-Hua Liu,Ning Li,Mei Han,Jing-Rui Han,Hong-Yan Liang.Scalable synthesis of nanoporous high entropy alloys for electrocatalytic oxygen evolution[J].Rare Metals,2022,41(1):125-131. 被引量:7

5刘淖泽,熊时健,彭祥.钒酸钴纳米片的析氧性能研究[J].稀有金属,2022,46(6):839-845. 被引量:3

1Xinyu Zhang,Yiwen Dong,Huiying Wang,Ziyi Zhao,Wenchun Jiang,Bin Dong,Han Hu,Chenguang Liu,Yongming Chai.Iron adsorption engineering facilitated by Cu doping on cobalt hydroxide host with enhanced oxygen evolution reaction[J].Nano Research,2023,16(2):2111-2118.

2韩长峰,钱若曦,向超宇,钱磊.Materials and device engineering to achieve high-performance quantum dots light emitting diodes for display applications[J].Chinese Physics B,2023,32(12):1-13.

3Yuhe ZHAO,Xu WANG,Dingshan GAO,Jianji DONG,Xinliang ZHANG.On-chip programmable pulse processor employing cascaded MZI-MRR structure[J].Frontiers of Optoelectronics,2019,12(2):148-156. 被引量:11

4Liming Wang,Yaping Zhang,Weibing Li,Lei Wang.Recent advances in elaborate interface regulation of BiVO_(4)photoanode for photoelectrochemical water splitting[J].Materials Reports(Energy),2023,3(4):3-18.

5Lingshuang Qin,Wei Zhang,Rui Cao.Hydrophilic MnO_(2) nanowires coating with o-fluoroaniline for electrocatalytic water oxidation[J].Chinese Journal of Structural Chemistry,2023,42(8):31-36.

6Quazi T.H.Shubhra.Iron oxide nanoparticles in magnetic drug targeting and ferroptosis-based cancer therapy[J].Medical Review,2023,3(5):444-447.

7Minghong Huang,Changsheng Cao,Li Liu,Wenbo Wei,Qi-Long Zhu,Zhenguo Huang.Controlled synthesis of MOF-derived hollow and yolk–shell nanocages for improved water oxidation and selective ethylene glycol reformation[J].eScience,2023,3(5):69-76.

8Tianshu Chu,Lei Zhou,Bowei Zhang,Fu-Zhen Xuan.Accurate atomic scanning transmission electron microscopy analysis enabled by deep learning[J].Nano Research,2024,17(4):2971-2980.

9Lu Chen,Junfeng Wang,Xiaojing Li,Jiayu Zhang,Chunran Zhao,Xin Hu,Hongjun Lin,Leihong Zhao,Ying Wu,Yiming He.Facile preparation of Ag_(2)S/KTa_(0.5)Nb_(0.5)O_(3) heterojunction for enhanced performance in catalytic nitrogen fixation via photocatalysis and piezo-photocatalysis[J].Green Energy & Environment,2023,8(6):1630-1643. 被引量:1

10Xiao-Yan Li,Manyi Duan,Pengfei Ou.High-throughput screening of single-atom catalysts confined in monolayer black phosphorus for efficient nitrogen reduction reaction[J].Nano Research,2024,17(4):2360-2367.

Basic Information:

DOI:

Chinese Library Classification Number:O646.542[理学—物理化学]

Citation Information:

Double-exchange(DE) interaction plays an important role in electrocatalytic oxygen evolution reaction(OER).However,precise achievement of DE interaction often requires foreign dopants or vacancy engineering,leading to destabilization of the catalysts and deterioration of performance.By contrast,the utilization of environmentally friendly,contactless,and continuously adjustable magnetic fields to study the OER process is profitable to avoid aforementioned interference factors and further elucidate the direct relationship0.5between DE interaction and OER activity.Here,by using cobalt hydroxide carbonate(Co(OH)(CO3)·xH2O,CoHC) nanostructures as a proof-of-concept study,external magnetic fields are carefully implemented to verify the role of DE interaction during water oxidation reaction.Detailed studies reveal that external magnetic fields effectively enhance the reaction rate of the catalyst,the overpotential decreases from 386 to 355 mV(100 mA·cm-2),while Tafel slopes drastically decline from 93 to 67 mV·dec-1(1.0 T).Moreover,magnetic field increment exhibits robust durability.Through in situ Raman and impedance measurements under external field,it can be found that magnetic field promotes the electron migration between Co2+ and Co3+ in the CoHC catalysts with the assistance of DE interactions,thus boosting the OER efficiency.

quote

GB/T 7714-2015 [1] Jun Li, Jun-Ming Li, Hong Hong, et al. Rare Metals, 2024(1): 289-297.
MLA [1] Jun Li, et al., Rare Metals, no. 1, 2024, pp. 289-297.
APA [1] Jun Li, Jun-Ming Li, Hong Hong, Dong-Xue Liu, Qing-Qi Cao, & Dun-Hui Wang. (2024). Rare Metals(1), 289-297.
IEEE [1] Jun Li, Jun-Ming Li, Hong Hong, Dong-Xue Liu, Qing-Qi Cao, and Dun-Hui Wang, Rare Metals, no. 1, pp. 289-297, 2024.