Investigation on Lowering of Fe,Ni and Cr Impurities Content in Na-reduced Ta Powder AITranslate

Zhuzhou Cemented Carbide Factory Tantalum Niobium Products Branch
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Investigation is made on lowering of Fe,Ni and Cr impurities content in K 2TaF 7 and sodium reduced Ta Powder.The results showed the basic way to lower Fe,Ni and Cr content is by reducing the fusion salt corrosion of the reduction equipment Fe;Ni,and Cr content can be distinctly lowered by the selection of proper fusion salt system and composition,the lowering of initial reduction temperature as well as the melting of given amount of sodium and diluent in the reactor followed by addition of K 2TaF 7 for melting.

KeyWords AITranslate

K 2TaF 7 NaCl liquid-liquid Na reduction Fe Ni and Cr impurlties

1王肇信.钽铌冶金学[M].稀有金属冶金学会、钽铌冶金专业委员会,1998..

1胡小锋,许茜,吴艳.钽粉制备工艺研究进展[J].材料导报,2005,19(10):97-99. 被引量:11

2李丽君,雒国清,刘建伟,纪保军.降低钠还原钽粉中铁、镍质量分数的工艺探讨[J].宁夏工程技术,2020,19(3):223-225. 被引量:1

1蒋柏泉,黄庆荣,郑典模,全水清,曾庆芳.溶剂浸取法制备低氟高纯氧化钽研究[J].南昌大学学报:工科版,2008,30(2):120-122. 被引量:1

2梁栋,侯击波,殷涛,尚福军,史洪刚,黄伟,史文璐.感应等离子工艺参数对制备电容器级钽粉性能的影响[J].兵器材料科学与工程,2010,33(3):46-50. 被引量:5

3王东新,李军义,孙本双,任晓,何季麟.钽粉制备新工艺研究进展[J].湖南有色金属,2011,27(3):34-37. 被引量:19

4王东新,李军义,孙本双,任晓,何季麟.还原氧化钽制备钽粉工艺研究进展[J].中国材料进展,2011,30(10):54-58. 被引量:1

5杨国启,何季麟,郑爱国,罗文,周小军,李军义.电容器级高比容钽粉制备工艺研究进展[J].湖南有色金属,2014,30(1):48-52. 被引量:17

6杨国启,孙宇,李仲香,陈学清,林辅坤,程越伟,雒国清.高压高比容钽粉的制备及性能表征[J].湖南有色金属,2017,33(2):43-47. 被引量:3

7杨国启,李仲香,李慧,马海燕,雒国清,赵春霞.高氮含量电容器级钽粉末的制备工艺研究[J].湖南有色金属,2018,34(5):50-52. 被引量:2

8月日辉,周丽.添加细化剂对FTB-48电容器钽粉粒度及电性能的影响[J].稀有金属与硬质合金,2020,48(2):18-21.

9苏龙兴,颜晓勇.金属钽粉的生产及提纯工艺进展[J].粉末冶金工业,2021,31(1):91-97. 被引量:2

10刘建迪,王静静,李伟,刘平,马凤仓,张柯,陈小红.钽的提取研究进展[J].矿产保护与利用,2021,41(2):163-173.

1潘伦桃,李荣德,张巧元.FTW300钽粉的制取及性能[J].电子元件与材料,1996,15(3):44-48.

2陈伟文.专利信息[J].上海有色金属,2013,34(2):91-91.

3许文江,潘伦桃,王向东,舒永春,毛襄萍,施文峰.氟钽酸钾及其相关熔盐体系的密度[J].稀有金属,1999,23(5):349-352. 被引量:6

4史鹏飞,尹鸽平,夏保佳.三瓦铝—空气电池的研究[J].电池,1992,22(4):152-154. 被引量:7

5蒋铁军.高纯铝铸锭质量缺陷及预防措施[J].新疆有色金属,2008,31(2):43-44. 被引量:2

6唐华.维修空调如何准确加氟[J].家电检修技术,2003(7):33-33.

7小型、大容量氟钽酸钾电容器[J].机电工程技术,2005,34(7):6-6.

8Sugio ōTANI,任少锋.由离子交换炭纤维和NaCl水溶液组成的二次电池[J].河北化工,1991(2):63-64.

9高飞.废催化剂熟料溶出粗液提钒工艺技术研究[J].轻金属,2013(7):22-25.

10蒋铁军.高纯铝铸锭冶金质量对电解电容器用铝箔生产的影响浅析[J].新疆有色金属,2009,32(1):48-49.

Basic Information:

DOI:

Chinese Library Classification Number:TM535.1[电气工程—电器];TF125.242[冶金工程—粉末冶金]

Citation Information:

Investigation is made on lowering of Fe,Ni and Cr impurities content in K 2TaF 7 and sodium reduced Ta Powder.The results showed the basic way to lower Fe,Ni and Cr content is by reducing the fusion salt corrosion of the reduction equipment Fe;Ni,and Cr content can be distinctly lowered by the selection of proper fusion salt system and composition,the lowering of initial reduction temperature as well as the melting of given amount of sodium and diluent in the reactor followed by addition of K 2TaF 7 for melting.

quote

GB/T 7714-2015 [1] LI Shi-lin. Investigation on Lowering of Fe,Ni and Cr Impurities Content in Na-reduced Ta Powder[J]. Rare Metals and Cemented Carbides, 2001(3): 10-13.
MLA [1] LI Shi-lin. "Investigation on Lowering of Fe,Ni and Cr Impurities Content in Na-reduced Ta Powder." Rare Metals and Cemented Carbides, no. 3, 2001, pp. 10-13.
APA [1] LI Shi-lin. (2001). Investigation on Lowering of Fe,Ni and Cr Impurities Content in Na-reduced Ta Powder. Rare Metals and Cemented Carbides(3), 10-13.
IEEE [1] LI Shi-lin, "Investigation on Lowering of Fe,Ni and Cr Impurities Content in Na-reduced Ta Powder," Rare Metals and Cemented Carbides, no. 3, pp. 10-13, 2001. keywords: {K 2TaF 7;NaCl;liquid-liquid Na reduction;Fe Ni and Cr impurlties}