Investigation on Expansion Mechanism of Tungsten Alloy AITranslate
Abstract AITranslate
Investigation is made on the improvement of the expansion coefficient of W-Ni-Cu alloy.The results showed that the alloys expansion coefficient varies directly as the binding phase (Ni Cu) and basically conforms with the law of addition.The expansion coefficient of the said alloy has been improved from 5.6×10 -6 /K to 8×10 -6 /K on the prerequisite of ensuring good properties of tungsten alloys by controlling the alloy component,optimum technical conditions.
KeyWords AITranslate
1王伏生,赵慕岳.高密度钨合金及其在军事工业中的应用[J].粉末冶金材料科学与工程,1997,2(2):114-120. 被引量:19
2曾昭论(译).苏联化学手册(Ⅱ)[M].北京:科学出版社,1959,8..
3王伏生,梁容海,赵慕岳.高密度钨合金在民用工业中的应用与开发[J].粉末冶金材料科学与工程,1997,2(4):279-284. 被引量:9
4GTRMAN R M.高比重合金结构的局限性[J].稀有金属材料与工程,1986,(1):54-54.
1杨宗辉,沈以赴,孟氢钡.浸渗法合金化纯钨表层的研究[J].材料工程,2012,40(7):86-91. 被引量:1
2杨宗辉,沈以赴,李晓泉.纯钨表面含镍涂层的浸渗法制备[J].稀有金属与硬质合金,2012,40(4):26-29.
3王玲,秦颖楠,单东栋,吕思键,熊宁.Ni、Cu比对钨镍铜合金性能及金相组织的影响规律研究[J].粉末冶金工业,2022,32(4):106-109. 被引量:2
4秦颖楠,王玲,单东栋,熊宁.不同镍铜比对65WNiCu合金力学性能及热膨胀系数影响规律[J].粉末冶金工业,2022,32(4):110-112. 被引量:2
1徐振钦,杨宗辉.异种材料焊接接头热应力缓冲中间层的研究现状[J].机械工程材料,2013,37(12):6-10. 被引量:4
2李昌伟,张勇.铜含量对CoCrFeNi高熵合金组织结构和性能的影响[J].精密成形工程,2022,14(12):1-9.
3韩俊峰,马越超,姜子明.液相烧结制备电力开关用W-7Cu-xNi合金微观组织及性能分析[J].粉末冶金工业,2023,33(1):84-88.
4李宗强,张廷瑜,杨跃标,张盛华.节镍型铜磷系耐候钢薄板带的质量控制工艺[J].金属功能材料,2023,30(3):62-70.
1华丽,徐宏,朱奎龙,王琼琦,王志文.2.25Cr-1Mo钢回火脆化对氢脆的影响[J].机械工程材料,2004,28(2):17-20. 被引量:7
2梁伟文,孙卫和.金属板材的激光弯曲成形技术及其应用[J].深圳职业技术学院学报,2005,4(1):21-25. 被引量:1
3孔小钧.偏心工件的加工方法及车削技巧[J].中国机械,2013(10):123-124. 被引量:1
4王才德,汪建昌.Fe-Cu粉末压坯烧结膨胀机理[J].粉末冶金材料科学与工程,1996,1(1):25-29. 被引量:6
5刘东星,陶华,薛红前,唐兴龄.超高强度钢超高周循环下疲劳裂纹扩展寿命研究[J].组合机床与自动化加工技术,2011(1):5-8. 被引量:5
6熊良勇,史占彪.新疆什可布台铁矿还原膨胀机理[J].东北工学院学报,1991,12(4):348-355.
7晏祥树,陈春林.富氧顶吹炼铅炉炉龄探讨[J].冶金能源,2012,31(4):47-50. 被引量:3
8陈刚,王宁,孙琴.硅颗粒对AlSi合金显微组织的影响[J].农业机械学报,2006,37(6):144-147.
9王涛,丁跃华,夏海英,张品贵.自焙炭砖侵蚀试验研究[J].钢铁研究,2010,38(2):1-4. 被引量:1
10袁国洲.镍铜总量对液相烧结Mo-W-Ni-Cu合金性能的影响[J].稀有金属与硬质合金,1999(2):7-10. 被引量:5
Basic Information:
DOI:
Chinese Library Classification Number:TG146.411[金属学及工艺—金属材料];TF125.241[冶金工程—粉末冶金]
Citation Information:
Investigation is made on the improvement of the expansion coefficient of W-Ni-Cu alloy.The results showed that the alloys expansion coefficient varies directly as the binding phase (Ni Cu) and basically conforms with the law of addition.The expansion coefficient of the said alloy has been improved from 5.6×10 -6 /K to 8×10 -6 /K on the prerequisite of ensuring good properties of tungsten alloys by controlling the alloy component,optimum technical conditions.
quote
| GB/T 7714-2015 | [1] YIN Xiang-chu, XIONG Xiang-jun. Investigation on Expansion Mechanism of Tungsten Alloy[J]. Rare Metals and Cemented Carbides, 2001(3): 14-16. |
| MLA | [1] YIN Xiang-chu, and XIONG Xiang-jun. "Investigation on Expansion Mechanism of Tungsten Alloy." Rare Metals and Cemented Carbides, no. 3, 2001, pp. 14-16. |
| APA | [1] YIN Xiang-chu, & XIONG Xiang-jun. (2001). Investigation on Expansion Mechanism of Tungsten Alloy. Rare Metals and Cemented Carbides(3), 14-16. |
| IEEE | [1] YIN Xiang-chu and XIONG Xiang-jun, "Investigation on Expansion Mechanism of Tungsten Alloy," Rare Metals and Cemented Carbides, no. 3, pp. 14-16, 2001. keywords: {W-Ni-Cu alloy;expansion coefficient;the law of addition;binding phase} |