daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study on Electrochemical Performance of Cu(Ⅰ)Ions in Choline Chloride-Urea Deep Eutectic Solvent AITranslate

School of Metallurgy and Environment,Central South University;Faculty of Metallurgical and Energy Engineering,Kunming University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The electrochemical performance was studied of Cu(Ⅰ)ions in CuCl-containing choline chloride-urea(ChCl-Urea)deep eutectic solvent as the electrolyte.The results show that the conductivity of ChCl-Urea-CuCl electrolyte increases with the increase of temperature,but increases at first and then decreases with the increase of CuCl concentration.The variation of its viscosity is opposite to its conductivity.In addition,the reduction reaction of Cu(Ⅰ)ions in ChCl-Urea-CuCl electrolyte is quasi-reversible and controlled by diffusion.The diffusion coefficient of Cu(Ⅰ)ions increases with the increase of temperature,but increases firstly and then decreases with the increase of CuCl concentration,which is mainly related to the existence form of Cu(Ⅰ)ions in ChCl-Urea deep eutectic solvent.

KeyWords AITranslate

Cu(Ⅰ)ion choline chloride-urea deep eutectic solvent conductivity viscosity diffusion coefficient metallurgical electrochemistry

1王喜然,华一新,赵秋凝,李艳.AlCl_3-BMIC离子液体的电导率[J].中国有色金属学报,2006,16(12):2138-2141. 被引量:18

2M.Rostom Ali,Md.Ziaur Rahman,S.SankarSaha.基于氯化胆碱离子液体的铜电沉积研究(英文)[J].电化学,2014,20(2):139-145. 被引量:3

1姚海威,MA Han,MAO Rui,QIU Jiayong,CHEN Chunyu,居殿春.Preparation of ZnO Nanoparticles from Zn-containing Rotary Hearth Furnace Dust[J].武汉理工大学学报:材料科学英文版,2022,37(1):32-37. 被引量:1

2竹源,齐本坤,梁欣泉,万印华.有机酸及多元醇类低共熔溶剂预处理木质纤维素研究进展[J].应用化工,2021,50(10):2786-2790. 被引量:4

3曹雪辰,周东杰,姚海威,居殿春.氯化胆碱-草酸低共熔溶剂处理含铁尘泥制备纳米氧化铁及动力学研究[J].无机盐工业,2021,53(11):100-106. 被引量:1

1徐春燕,熊凤,陈德明,单玉蓉,张林,王挥.低共熔溶剂协同酸性二氧六环预处理杨木及其酶水解特性的探究[J].应用化工,2022,51(9):2558-2564. 被引量:1

2贾昭炎,王成成,曹春晖,刘洋,奚永兰,刘明庆.深度共熔溶剂预处理木质纤维素研究进展[J].江苏农业科学,2022,50(20):77-85.

3姚海威,毛瑞,王飞,朱祚峤.转底炉氧化锌粉高值化利用研究[J].无机盐工业,2022,54(12):119-125.

4左金龙,张迎停,夏至,谭冲,穆德颖,马雪薇,李俊生.生物质预处理技术研究进展[J].应用化工,2023,52(5):1569-1575.

5洪元芳,雷永伟,安艳霞,赵阳,张剑.不同类型低共熔溶剂预处理对玉米秸秆酶解效率的影响[J].现代食品科技,2023,39(7):162-169.

1蒋建方,冯章语,宋清新,刘秋均,初振钰,何琛,金玲.酮醛胺缩合物高温缓蚀剂制备方法的优化[J].油田化学,2020,37(2):330-334. 被引量:2

2于竞翔,刘国宏,任丽君,刘萌,黄志平,李建,李丹萍,肖艳华.新型便携式RGB色度传感器定量检测水中路易氏剂[J].分析化学,2020,48(7):962-968. 被引量:3

3韩晔华,欧阳萍,张艳芬,黄凌,张睿,史权,孟祥海,刘植昌,徐春明.基于实时直接分析质谱技术的氯铝酸及其复合离子液体分析[J].中国科学:化学,2020,50(6):720-728. 被引量:5

Basic Information:

DOI:

Chinese Library Classification Number:TF811[冶金工程—有色金属冶金]

Citation Information:

The electrochemical performance was studied of Cu(Ⅰ)ions in CuCl-containing choline chloride-urea(ChCl-Urea)deep eutectic solvent as the electrolyte.The results show that the conductivity of ChCl-Urea-CuCl electrolyte increases with the increase of temperature,but increases at first and then decreases with the increase of CuCl concentration.The variation of its viscosity is opposite to its conductivity.In addition,the reduction reaction of Cu(Ⅰ)ions in ChCl-Urea-CuCl electrolyte is quasi-reversible and controlled by diffusion.The diffusion coefficient of Cu(Ⅰ)ions increases with the increase of temperature,but increases firstly and then decreases with the increase of CuCl concentration,which is mainly related to the existence form of Cu(Ⅰ)ions in ChCl-Urea deep eutectic solvent.

quote

GB/T 7714-2015 [1] TANG Jie, XU Cun-ying. Study on Electrochemical Performance of Cu(Ⅰ)Ions in Choline Chloride-Urea Deep Eutectic Solvent[J]. Rare Metals and Cemented Carbides, 2020(3): 18-24.
MLA [1] TANG Jie, and XU Cun-ying. "Study on Electrochemical Performance of Cu(Ⅰ)Ions in Choline Chloride-Urea Deep Eutectic Solvent." Rare Metals and Cemented Carbides, no. 3, 2020, pp. 18-24.
APA [1] TANG Jie, & XU Cun-ying. (2020). Study on Electrochemical Performance of Cu(Ⅰ)Ions in Choline Chloride-Urea Deep Eutectic Solvent. Rare Metals and Cemented Carbides(3), 18-24.
IEEE [1] TANG Jie and XU Cun-ying, "Study on Electrochemical Performance of Cu(Ⅰ)Ions in Choline Chloride-Urea Deep Eutectic Solvent," Rare Metals and Cemented Carbides, no. 3, pp. 18-24, 2020. keywords: {Cu(Ⅰ)ion;choline chloride-urea;deep eutectic solvent;conductivity;viscosity;diffusion coefficient;metallurgical electrochemistry}