Process Design of Oxygen-enriched Side-blown Molten Pool Smelting of Heavy Metal-containing Sludge AITranslate
Abstract AITranslate
The process of recovering valuable metals such as copper and zinc from heavy metal-containing sludge by oxygen-enriched side-blown molten pool smelting is introduced from the aspects of process selection and design,main equipment selection and main technical indicators,to provide a reference for the comprehensive utilization of heavy metal-containing sludge.
KeyWords AITranslate
1张海亮,梁冬云,刘勇.电镀污泥处理现状及进展[J].再生资源与循环经济,2017,10(7):25-30. 被引量:13
2陈永松,周少奇.电镀污泥的基本理化特性研究[J].中国资源综合利用,2007,25(5):2-6. 被引量:42
3王静,叶海明.含铜电镀污泥中铜的资源化回收技术[J].化学工程与装备,2010(8):197-199. 被引量:11
4刘生长.富氧侧吹炉处理含铜渣料的工艺设计[J].铜业工程,2018(2):57-59. 被引量:2
1林炳丞,吴广龙,郑明辉,刘国瑞.再生铜冶炼过程中重金属排放特征和控制[J].环境科学,2023,44(3):1678-1685.
2郑瑞立,吕建芳,宋卫锋,刘牡丹,刘勇,吕先谨.含铜电镀污泥熔炼过程中主要元素的迁移转化行为研究[J].中南大学学报:自然科学版,2023,54(7):2563-2575.
1刘忠平.提升高铅黑铜吹炼品质的生产实践[J].世界有色金属,2019,0(23):9-10.
2谢祥添,左东平,韩义忠,余华清.铋在双旋浮铜冶炼过程中的分布及回收[J].有色金属:冶炼部分,2020,0(5):36-38.
3左东平,谢祥添,余华清.废电解液处理工艺优化与生产实践[J].中国金属通报,2020,0(3):4-4.
4黄晟,梁治安,陈水波,张兴勋,叶志勇.从某氧化铜浮选尾矿中回收铜、钴的试验研究[J].有色金属:选矿部分,2020(3):29-34. 被引量:6
5刘泉洲,张楌,王志刚.浅析天然气净化工艺中的设备选择[J].南北桥,2018(6):183-183.
6薛飞,林丽华,王亮,杨蕾.海洋疏浚泥资源化综合利用成果转化推广“瓶颈”及其对策建议[J].海洋开发与管理,2020,37(6):25-29. 被引量:3
7刘影,邱陆明,迟崇哲,降向正.某焙烧冶炼企业酸性废水综合治理回收试验研究[J].黄金,2020,41(6):69-71.
8刘凯,苏迎,屠国伟,罗哲.心源性休克时机械循环辅助设备的应用[J].中华重症医学电子杂志,2020,6(2):151-155. 被引量:2
9罗文灵.浅谈北疆供水工程老旧干渠改造快速一体化施工工法[J].中国标准化,2019(24):94-95. 被引量:1
10李漪锦,肖力,徐梦玮,刘德明,董新荣,朱池明.葛根淀粉提取工艺优化与同时富集回收总异黄酮的方法[J].江苏农业科学,2020,48(12):192-196. 被引量:1
Basic Information:
DOI:
Chinese Library Classification Number:X758[环境科学与工程—环境工程]
Citation Information:
The process of recovering valuable metals such as copper and zinc from heavy metal-containing sludge by oxygen-enriched side-blown molten pool smelting is introduced from the aspects of process selection and design,main equipment selection and main technical indicators,to provide a reference for the comprehensive utilization of heavy metal-containing sludge.
quote
| GB/T 7714-2015 | [1] YANG Lun-zhuang, TANG Zhao-hui, WANG Yong-zhou, et al. Process Design of Oxygen-enriched Side-blown Molten Pool Smelting of Heavy Metal-containing Sludge[J]. Rare Metals and Cemented Carbides, 2020(3): 25-28. |
| MLA | [1] YANG Lun-zhuang, et al., "Process Design of Oxygen-enriched Side-blown Molten Pool Smelting of Heavy Metal-containing Sludge." Rare Metals and Cemented Carbides, no. 3, 2020, pp. 25-28. |
| APA | [1] YANG Lun-zhuang, TANG Zhao-hui, WANG Yong-zhou, & ZHANG Ling. (2020). Process Design of Oxygen-enriched Side-blown Molten Pool Smelting of Heavy Metal-containing Sludge. Rare Metals and Cemented Carbides(3), 25-28. |
| IEEE | [1] YANG Lun-zhuang, TANG Zhao-hui, WANG Yong-zhou, and ZHANG Ling, "Process Design of Oxygen-enriched Side-blown Molten Pool Smelting of Heavy Metal-containing Sludge," Rare Metals and Cemented Carbides, no. 3, pp. 25-28, 2020. keywords: {heavy metal-containing sludge;oxygen-enriched side-blown molten pool smelting;black copper;zinc-rich smoke dust;comprehensive recovery;process design} |