Research Progress in Vanadium Recovery by Hydrometallurgical Acid Leaching from Stone Coal AITranslate

State Key Laboratory of Organic Geochemistry,Guangzhou Institute of Geochemisty.Chinese Academy of Sciences;State Key Laboratory of Organic Geochemistry,Guangzhou Institute of Geochemisty.Chinese Academy of Sciences;State Key Laboratory of Organic Geochemistry,Guangzhou Institute of Geochemisty.Chinese Academy of Sciences;State Key Laboratory of Organic Geochemistry,Guangzhou Institute of Geochemisty.Chinese Academy of Sciences;State Key Laboratory of Organic Geochemistry,Guangzhou Institute of Geochemisty.Chinese Academy of Sciences;State Key Laboratory of Organic Geochemistry,Guangzhou Institute of Geochemisty.Chinese Academy of Sciences
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The resource characteristics and recovery process status of vanadium in stone coal were reviewed.Focusing on the recovery process of vanadium in stone coal by hydrometallurgical acid leaching,and combined with the control factors and kinetics of vanadium leaching reaction process under different process conditions,the influences of vanadium occurrence state,leaching aid and leaching process on the vanadium recovery process by hydrometallurgical acid leaching were analyzed.The promotion effect of fluorine-containing leaching aid,oxidant and their compound on the hydrometallurgical leaching of vanadium was expounded.Based on the occurrence state of vanadium in stone coal,it is pointed out that the development of environmentally friendly and high-efficiency leaching aid and the in-depth analysis of its leaching kinetics to improve the leaching and recovery efficiency of vanadium,and the development of the recovery and recycling technology of leaching waste liquid and slag are the focus of future research and the key to realize the high-efficiency and clean recovery of vanadium in stone coal.

KeyWords AITranslate

stone coal vanadium recovery hydrometallurgical acid leaching leaching aid kinetics

1王丽,张庆鹏,孙伟.陕西商洛石煤中钒的赋存状态与工艺矿物学研究[J].矿物学报,2017,37(1):29-35. 被引量:16

2冀成庆,沈明伟,朱昌洛,惠博,杨常艳,蔡旺.黑色页岩型黏土钒矿的硫酸直接湿法浸出试验研究[J].钢铁钒钛,2014,35(1):11-15. 被引量:3

3LI Haoran,FENG Yali,LIANG Jianglong,LUO Xiaobing,DU Zhuwei.Vanadium recovery from clay vanadium mineral using an acid leaching method[J].稀有金属:英文版,2008,27(2):116-120. 被引量:23

4邢学永,宁顺明,佘宗华,赵强.甘肃酒泉某石煤矿中钒的赋存状态与提钒过程研究[J].稀有金属,2013,37(1):135-139. 被引量:8

5WANG Mingyu XIANG Xiaoyan ZHANG Liping XIAO Liansheng.Effect of vanadium occurrence state on the choice of extracting vanadium technology from stone coal[J].稀有金属:英文版,2008,27(2):112-115. 被引量:32

6邓志敢,魏昶,樊刚,李旻廷,李存兄,李兴彬.Extracting vanadium from stone-coal by oxygen pressure acid leaching and solvent extraction[J].中国有色金属学报:英文版,2010,0(S1):118-122. 被引量:15

7张卫国,侯恩科,杨建业,李焕同,桓斌斌.石煤中钒-钼-硒等伴生元素研究[J].稀有金属,2019,43(10):1092-1102. 被引量:14

8叶国华,张爽,何伟,童雄,吴宁.石煤的工艺矿物学特性及其与提钒的关系[J].稀有金属,2014,38(1):146-157. 被引量:28

9杨晓,张一敏,刘涛,赵杰,黄晶.含氟助浸剂对石煤提钒酸浸动力学的影响[J].化学工程,2013,41(5):59-63. 被引量:13

10余文轩,梁冬云,戴子林.贵州省石煤型钒矿的工艺矿物学及钒的赋存状态研究[J].矿冶工程,2013,33(1):79-82. 被引量:16

1陈健,李洋,江佩君,李秀丽,齐啸威,刘文中,陈萍.煤型关键元素矿床的资源综合利用与潜在环境风险——以云南临沧某锗提炼厂为例[J].煤炭学报,2022,47(5):1885-1894.

2赖永传,杨鑫龙,孙建之,尚鹤,莫晓兰,温建康.石煤含氟酸浸液中V(Ⅴ)-Fe(Ⅲ)-F-H_(2)O系钒铁分离热力学研究[J].中南大学学报:自然科学版,2023,54(5):1703-1712.

3王淼,温建康,李文娟,杨鑫龙,赖永传,杨洪英.选冶联合回收石煤中伴生战略金属钒镍钼的研究进展[J].稀有金属,2023,47(6):881-892.

1郑淑芳,吕琪,冯青.全湿法从锰钴镍渣中回收钴、镍的试验研究[J].科教导刊:电子版,2020(7):287-287.

2汪虎,左恒,陈超.石煤钒矿中钒高效浸出新技术研究[J].石油石化物资采购,2020(8):59-60.

3李彬彬.废弃SCR脱硝催化剂资源化制备再生钛钨粉的研究[J].化学工业与工程,2020,37(3):60-66. 被引量:3

4熊以俊,许用华,张骏南,王元华.废锂电三元正极材料和铝镍钴废磁钢混合物酸浸技术研究[J].有色金属:冶炼部分,2020,0(6):19-23.

5陈浩,董廷旭,李勇,文星跃.涪江上游下切深度、速率及它们对下切过程控制因素的约束[J].重庆师范大学学报:自然科学版,2019,36(6):53-57. 被引量:1

6宁继来,郑永兴,胡盘金,庞杰.锌冶炼渣选冶联合技术研究进展[J].矿冶,2020,29(3):18-24. 被引量:5

7张贺.退役光伏组件资源化利用工艺及经济效益分析[J].经济管理文摘,2019(16):6-7. 被引量:1

8葛永睿,王大寿,龚朝兵,李海华.原油清罐污油膜强化传质技术的应用[J].中外能源,2020,0(2):77-80. 被引量:2

9何文龙,兰玮锋,吴世发.含钴黄铁矿硫酸化焙烧浸出研究[J].中国资源综合利用,2020,38(6):10-12. 被引量:1

10李猛.化工制药工程中工艺优化方法探析[J].今天,2020,0(14):0292-0292.

Basic Information:

DOI:

Chinese Library Classification Number:TF841.3[冶金工程—有色金属冶金]

Citation Information:

The resource characteristics and recovery process status of vanadium in stone coal were reviewed.Focusing on the recovery process of vanadium in stone coal by hydrometallurgical acid leaching,and combined with the control factors and kinetics of vanadium leaching reaction process under different process conditions,the influences of vanadium occurrence state,leaching aid and leaching process on the vanadium recovery process by hydrometallurgical acid leaching were analyzed.The promotion effect of fluorine-containing leaching aid,oxidant and their compound on the hydrometallurgical leaching of vanadium was expounded.Based on the occurrence state of vanadium in stone coal,it is pointed out that the development of environmentally friendly and high-efficiency leaching aid and the in-depth analysis of its leaching kinetics to improve the leaching and recovery efficiency of vanadium,and the development of the recovery and recycling technology of leaching waste liquid and slag are the focus of future research and the key to realize the high-efficiency and clean recovery of vanadium in stone coal.

quote

GB/T 7714-2015 [1] HUANG Zu-lv, CHEN Tao, LIN Han-zhi, et al. Research Progress in Vanadium Recovery by Hydrometallurgical Acid Leaching from Stone Coal[J]. Rare Metals and Cemented Carbides, 2020(3): 11-17.
MLA [1] HUANG Zu-lv, et al., "Research Progress in Vanadium Recovery by Hydrometallurgical Acid Leaching from Stone Coal." Rare Metals and Cemented Carbides, no. 3, 2020, pp. 11-17.
APA [1] HUANG Zu-lv, CHEN Tao, LIN Han-zhi, ZHOU Yang, YAN Bo, & TIAN Hui. (2020). Research Progress in Vanadium Recovery by Hydrometallurgical Acid Leaching from Stone Coal. Rare Metals and Cemented Carbides(3), 11-17.
IEEE [1] HUANG Zu-lv, CHEN Tao, LIN Han-zhi, ZHOU Yang, YAN Bo, and TIAN Hui, "Research Progress in Vanadium Recovery by Hydrometallurgical Acid Leaching from Stone Coal," Rare Metals and Cemented Carbides, no. 3, pp. 11-17, 2020. keywords: {stone coal;vanadium recovery;hydrometallurgical acid leaching;leaching aid;kinetics}