daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Study on Reduction Roast and Magnetic Separation Process of Mixed Rare Earth Concentrate AITranslate

Key Laboratories of the Ministry of Education of Light Rare Earth Resources Green Extraction and Efficient Use,Inner Mongolia University of Science and Technology;Key Laboratories of the Ministry of Education of Light Rare Earth Resources Green Extraction and Efficient Use,Inner Mongolia University of Science and Technology;Key Laboratories of the Ministry of Education of Light Rare Earth Resources Green Extraction and Efficient Use,Inner Mongolia University of Science and Technology;Key Laboratories of the Ministry of Education of Light Rare Earth Resources Green Extraction and Efficient Use,Inner Mongolia University of Science and Technology;Key Laboratories of the Ministry of Education of Light Rare Earth Resources Green Extraction and Efficient Use,Inner Mongolia University of Science and Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The reduction roasting technology was used to reduce the iron minerals in a mixed rare earth concentrate from Inner Mongolia to elemental metals,and then the magnetic separation technology was used for high efficient separation and enrichment of iron,rare earth,niobium and other elements.The effects of reduction temperature,roasting time and carbon content on the reduction roasting were investigated by single factor experiments,as well as the enrichment and recovery of rare earth and niobium at different roasting temperatures.Under the optimized conditions of roasting temperature of 1175℃,roasting time of 90 min and C/O ratio of 1.5,the iron metallization rate reaches 92.52%,the iron grade and recovery rate in magnetic materials are 89.71%and 92.12%,the niobium grade and recovery rate in non-magnetic materia-ls are 3.85%and 87.92%,and the rare earth grade and recovery rate are 7.15%and 88.23%,respectively.

KeyWords AITranslate

mixed rare earth concentrate reduction roasting metallization rate magnetic separation activated carbon

1沈慧庭,周波,黄晓毅,张延军,林乡伟.难选鲕状赤铁矿焙烧-磁选和直接还原工艺的探讨[J].矿冶工程,2008,28(5):30-34. 被引量:36

2高鹏,韩跃新,李艳军,孙永升.白云鄂博氧化矿石深度还原-磁选试验研究[J].东北大学学报:自然科学版,2010,31(6):886-889. 被引量:38

3郭保万.高铁铌中矿浸出除铁试验研究[J].矿产保护与利用,2010,30(6):30-32. 被引量:1

4刘勇,刘牡丹,刘珍珍.复杂稀有金属伴生矿富集渣提取稀土和铌的工艺研究[J].稀有金属与硬质合金,2015,43(1):21-25. 被引量:10

5姬俊梅,欧俊英.白云鄂博氧化矿反浮尾矿综合回收稀土和铁的选矿新工艺研究[J].四川稀土,2012(2):18-20. 被引量:1

6李春龙,李小钢,徐广尧.白云鄂博共伴生矿资源综合利用技术开发与产业化[J].稀土,2015,36(5):151-158. 被引量:51

7余永富.白云鄂博矿稀土、铌资源综合利用研究意义重大[J].稀土信息,2007,13(8):8-9. 被引量:28

8张清岑,白国华.影响含铁原料直接还原的若干因素[J].烧结球团,1996,21(3):43-46. 被引量:6

1田杰,李梅,张宇旭,李凯,高凯.稀有多金属混合精矿焙烧过程形貌及物相研究[J].稀有金属与硬质合金,2021,49(2):15-19.

2孙亮,李玉虎,宋健清,张敏.焙烧制度对稀土精矿中铁、铝等杂质浸出行为的影响[J].有色金属科学与工程,2021,12(4):27-32. 被引量:1

3钟荣海,耿志强,曾令明,左鸿山,谷雪涛.磁化焙烧-磁选含铁氟碳铈粗精矿研究[J].铜业工程,2022(6):57-62.

1郭志强,燕可洲,张吉元,柳丹丹,高阳艳,郭彦霞.煤矸石/粉煤灰对赤泥钠化还原焙烧反应的影响机制[J].化工学报,2022,73(5):2194-2205. 被引量:5

1梁祖祯.某黄金冶炼渣还原焙烧磁选工艺研究[J].冶金与材料,2020,40(2):36-36.

2Health Phys. Abstracts,Volume 118,Number 5[J].辐射防护,2020,40(3):262-264.

3伏彩萍.铋精矿加压氧化氨浸高效分离铜、硫和铋[J].矿冶工程,2020,40(2):111-113.

4张登高,蒋训雄,范艳青,汪胜东,冯林永,刘巍.铜阳极泥加压浸出液中硒碲分离研究[J].有色金属:冶炼部分,2020(7):65-68. 被引量:3

5张敏敏,程素盼,赵志国,刘倩,刘伟,王晓,赵恒强.UPLC-DPPH-PAD-ESI-TOF/MS在线联用技术快速筛选丹参中的抗氧化成分[J].中草药,2020,51(11):2908-2913. 被引量:11

Basic Information:

DOI:

Chinese Library Classification Number:TF111[冶金工程—冶金物理化学]

Citation Information:

The reduction roasting technology was used to reduce the iron minerals in a mixed rare earth concentrate from Inner Mongolia to elemental metals,and then the magnetic separation technology was used for high efficient separation and enrichment of iron,rare earth,niobium and other elements.The effects of reduction temperature,roasting time and carbon content on the reduction roasting were investigated by single factor experiments,as well as the enrichment and recovery of rare earth and niobium at different roasting temperatures.Under the optimized conditions of roasting temperature of 1175℃,roasting time of 90 min and C/O ratio of 1.5,the iron metallization rate reaches 92.52%,the iron grade and recovery rate in magnetic materials are 89.71%and 92.12%,the niobium grade and recovery rate in non-magnetic materia-ls are 3.85%and 87.92%,and the rare earth grade and recovery rate are 7.15%and 88.23%,respectively.

quote

GB/T 7714-2015 [1] LI Kai, TIAN Jie, LI Mei, et al. Study on Reduction Roast and Magnetic Separation Process of Mixed Rare Earth Concentrate[J]. Rare Metals and Cemented Carbides, 2020(3): 5-10.
MLA [1] LI Kai, et al., "Study on Reduction Roast and Magnetic Separation Process of Mixed Rare Earth Concentrate." Rare Metals and Cemented Carbides, no. 3, 2020, pp. 5-10.
APA [1] LI Kai, TIAN Jie, LI Mei, GAO Kai, & ZHANG Dong-liang. (2020). Study on Reduction Roast and Magnetic Separation Process of Mixed Rare Earth Concentrate. Rare Metals and Cemented Carbides(3), 5-10.
IEEE [1] LI Kai, TIAN Jie, LI Mei, GAO Kai, and ZHANG Dong-liang, "Study on Reduction Roast and Magnetic Separation Process of Mixed Rare Earth Concentrate," Rare Metals and Cemented Carbides, no. 3, pp. 5-10, 2020. keywords: {mixed rare earth concentrate;reduction roasting;metallization rate;magnetic separation;activated carbon}