Large-Scale Production of Electrothermal Films with GNSs/CNTs/CB Three-Dimensional Structure Ink by Screen Printing Large-Scale Production of Electrothermal Films with GNSs/CNTs/CB Three-Dimensional Structure Ink by Screen Printing AITranslate
Abstract AITranslate
With the development of flexible electronic technology, there is a growing demand for electrothermal materials that are environmentally friendly, safe, low-cost, and large-scale producible for efficiently solving thermal management issues. In this study, low-cost water-based carbon series electrothermal ink is prepared by a dispersion and grinding method, and the electrothermal films with various areas can be prepared on a large scale by screen printing. Simultaneously, the three-dimensional (3D) conductive network structure of graphene nanosheets (GNSs)/multiwalled carbon nanotubes (MWCNTs)/carbon black (CB) is built by the ball milling dispersion process. Due to the low percolation threshold network formed by GNSs/CNTs/CB, the prepared ink has excellent conductivity, and the square resistance (Rsq) reaches 4.3 Ω sq–1 with a thickness of 25 μm. Moreover, the saturation temperature (Ts) of the screen-printed electrothermal film (4 cm × 4 cm) can reach 165 °C with an input voltage of 10 V, and it has extremely low power consumption (444.75 cm2 W–1). The electrothermal film also maintains relatively stable electrical properties in a bending test of 115 000 cycles. When the heating device (9 cm × 31 cm) is applied to the expanded polypropylene (EPP) box, the food temperature can be kept around 60 °C and the flavor can be well preserved.
KeyWords AITranslate
Basic Information:
DOI:https://doi.org/10.1021/acsaelm.1c01172
Chinese Library Classification Number:
Citation Information:
With the development of flexible electronic technology, there is a growing demand for electrothermal materials that are environmentally friendly, safe, low-cost, and large-scale producible for efficiently solving thermal management issues. In this study, low-cost water-based carbon series electrothermal ink is prepared by a dispersion and grinding method, and the electrothermal films with various areas can be prepared on a large scale by screen printing. Simultaneously, the three-dimensional (3D) conductive network structure of graphene nanosheets (GNSs)/multiwalled carbon nanotubes (MWCNTs)/carbon black (CB) is built by the ball milling dispersion process. Due to the low percolation threshold network formed by GNSs/CNTs/CB, the prepared ink has excellent conductivity, and the square resistance (Rsq) reaches 4.3 Ω sq–1 with a thickness of 25 μm. Moreover, the saturation temperature (Ts) of the screen-printed electrothermal film (4 cm × 4 cm) can reach 165 °C with an input voltage of 10 V, and it has extremely low power consumption (444.75 cm2 W–1). The electrothermal film also maintains relatively stable electrical properties in a bending test of 115 000 cycles. When the heating device (9 cm × 31 cm) is applied to the expanded polypropylene (EPP) box, the food temperature can be kept around 60 °C and the flavor can be well preserved.
quote
| GB/T 7714-2015 | [1] Yunhao Liu, Xiaohua Ma, Haizhai Zhang, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01172. |
| MLA | [1] Yunhao Liu, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01172. |
| APA | [1] Yunhao Liu, Xiaohua Ma, Haizhai Zhang, Jitai Sun, Jun Qian, & Xin Wang. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01172 |
| IEEE | [1] Yunhao Liu, Xiaohua Ma, Haizhai Zhang, Jitai Sun, Jun Qian, and Xin Wang, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01172. keywords: {electrothermal ink low percolation threshold waterbased temperature control largescale} |