daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Hierarchical Silver Network Transparent Conducting Electrodes for Thin-Film Solar Cells Hierarchical Silver Network Transparent Conducting Electrodes for Thin-Film Solar Cells AITranslate

Hanbat National University; Hanbat National University; Hanbat National University; Hanbat National University; Hanbat National University; Hanbat National University; Princeton University; Korea Institute of Energy Research (KIER); University of Science and Technology (UST); University of Science and Technology (UST); University of Science and Technology (UST); University of Science and Technology (UST); University of Science and Technology (UST); Hanbat National University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Flexible metal network transparent conducting electrodes (TCEs) are expected to be the most promising candidates to replace indium tin oxide (ITO) due to their excellent electro-optical performance and mechanical flexibility. However, to successfully replace ITO with the metal network TCEs, more studies on their suitability for integration with real devices are needed. In this study, we developed a hierarchical silver network simultaneously meeting the requirements of (i) low sheet resistance, (ii) high optical transmittance, (iii) excellent mechanical flexibility, and (iv) good integration into a thin-film solar cell. The hierarchical silver network consists of a silver micromesh as the main framework and silver nanowires as the secondary framework. The hierarchical network provides a figure of merit similar to that of the individual micromesh and much higher than those of silver nanowires and ITO. When applied to Cu(In, Ga)Se2 thin-film solar cells, the hierarchical network achieved better device performance than the micromesh. In the hierarchical network, the micromesh enables low sheet resistance and the silver nanowires enable excellent integration with the device while maintaining high optical transmittance. Thus, considering the aforementioned requirements, the hierarchical network could be one of the best candidates as a TCE for Cu(In, Ga)Se2 thin-film solar cells.

KeyWords AITranslate

hierarchical network transparent conducting electrode solar cells micromesh silver nanowire
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c01176

Chinese Library Classification Number:

Citation Information:

Flexible metal network transparent conducting electrodes (TCEs) are expected to be the most promising candidates to replace indium tin oxide (ITO) due to their excellent electro-optical performance and mechanical flexibility. However, to successfully replace ITO with the metal network TCEs, more studies on their suitability for integration with real devices are needed. In this study, we developed a hierarchical silver network simultaneously meeting the requirements of (i) low sheet resistance, (ii) high optical transmittance, (iii) excellent mechanical flexibility, and (iv) good integration into a thin-film solar cell. The hierarchical silver network consists of a silver micromesh as the main framework and silver nanowires as the secondary framework. The hierarchical network provides a figure of merit similar to that of the individual micromesh and much higher than those of silver nanowires and ITO. When applied to Cu(In, Ga)Se2 thin-film solar cells, the hierarchical network achieved better device performance than the micromesh. In the hierarchical network, the micromesh enables low sheet resistance and the silver nanowires enable excellent integration with the device while maintaining high optical transmittance. Thus, considering the aforementioned requirements, the hierarchical network could be one of the best candidates as a TCE for Cu(In, Ga)Se2 thin-film solar cells.

quote

GB/T 7714-2015 [1] Kyung Soo Cho, Seoin Kang, YongJun Oh, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01176.
MLA [1] Kyung Soo Cho, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01176.
APA [1] Kyung Soo Cho, Seoin Kang, YongJun Oh, Joon Sik Park, Sangyeob Lee, JungSub Wi, JeungHun Park, Soomin Song, Kihwan Kim, YoungJoo Eo, Jae Ho Yun, Jihye Gwak, JunSik Cho, & ChoongHeui Chung. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01176
IEEE [1] Kyung Soo Cho, Seoin Kang, YongJun Oh, Joon Sik Park, Sangyeob Lee, JungSub Wi, JeungHun Park, Soomin Song, Kihwan Kim, YoungJoo Eo, Jae Ho Yun, Jihye Gwak, JunSik Cho, and ChoongHeui Chung, ACS Applied Electronic Materials, no. 4, 2022, doi: 10.1021/acsaelm.1c01176. keywords: {hierarchical network transparent conducting electrode solar cells micromesh silver nanowire}