daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Enhanced Piezoelectricity and Excellent Thermal Stability in Sm3+-Doped BiFeO3-PbTiO3 Ceramics Enhanced Piezoelectricity and Excellent Thermal Stability in Sm3+-Doped BiFeO3-PbTiO3 Ceramics AITranslate

Harbin Institute of Technology; Harbin Institute of Technology; Harbin Institute of Technology; Université Paris-Saclay; Harbin Institute of Technology; Harbin Institute of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Piezoelectric ceramics with combined high piezoelectric performance and excellent thermal stability are important and urgently needed for actuation and sensor applications in harsh environments, such as aerospace, automotive, oil, and gas exploration industries. However, the development of such piezoceramics is still a highly challenging task because an enhanced piezoelectric response is generally accompanied by a decrease in thermal stability. Here, we report that 0.55Bi1–xSmxFeO3–0.45PbTiO3 piezoceramics exhibit a balanced trade-off between piezoelectric response and thermal stability near the morphotropic phase boundary (MPB), where piezoelectric coefficient d33 (275 pC N–1) barely changes even at a temperature as high as 320 °C and the well-squared shape P–E hysteresis loop persists even at a high temperature of 220 °C. Compared with La3+, Sm3+ has a smaller ionic radius than Bi3+ or Pb2+ and thus could be more effectively to induce MPB at a relatively low substitution level (x = 0.16–0.21). In turn, the thermal stability of the piezoceramics does not degrade significantly. Our results further demonstrate that Sm substitution induces a strong relaxor behavior in the ceramics. These results suggest that the Sm3+-doped BiFeO3-PbTiO3 ceramics hold great promise for high temperature piezoelectric applications.

KeyWords AITranslate

piezoelectricity thermal stability morphotropic phase boundary (MPB) ceramics relaxor
No data

Basic Information:

DOI:https://doi.org/10.1021/acsaelm.1c01166

Chinese Library Classification Number:

Citation Information:

Piezoelectric ceramics with combined high piezoelectric performance and excellent thermal stability are important and urgently needed for actuation and sensor applications in harsh environments, such as aerospace, automotive, oil, and gas exploration industries. However, the development of such piezoceramics is still a highly challenging task because an enhanced piezoelectric response is generally accompanied by a decrease in thermal stability. Here, we report that 0.55Bi1–xSmxFeO3–0.45PbTiO3 piezoceramics exhibit a balanced trade-off between piezoelectric response and thermal stability near the morphotropic phase boundary (MPB), where piezoelectric coefficient d33 (275 pC N–1) barely changes even at a temperature as high as 320 °C and the well-squared shape P–E hysteresis loop persists even at a high temperature of 220 °C. Compared with La3+, Sm3+ has a smaller ionic radius than Bi3+ or Pb2+ and thus could be more effectively to induce MPB at a relatively low substitution level (x = 0.16–0.21). In turn, the thermal stability of the piezoceramics does not degrade significantly. Our results further demonstrate that Sm substitution induces a strong relaxor behavior in the ceramics. These results suggest that the Sm3+-doped BiFeO3-PbTiO3 ceramics hold great promise for high temperature piezoelectric applications.

quote

GB/T 7714-2015 [1] Xinyu He, Tao Wang, Xudong Li, et al. ACS Applied Electronic Materials, 2022(4). DOI:10.1021/acsaelm.1c01166.
MLA [1] Xinyu He, et al., ACS Applied Electronic Materials, no. 4, 2022, https://doi.org/10.1021/acsaelm.1c01166.
APA [1] Xinyu He, Tao Wang, Xudong Li, Sujit Das, Xingjun Liu, & Zuhuang Chen. (2022). ACS Applied Electronic Materials(4). https://doi.org/10.1021/acsaelm.1c01166