Granulating Mechanism of Mixing Drum and Drum Lining Selection AITranslate

Changsha Nonferrous Metallurgical Design Research Institute
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Detailed analysis is made of the granulating mechanism of sintering material and drum liners. Based on comparison of lining materials for engineering purpose and its application, the paper indicated that during production, the ideal liner will adsorb a thin layer of mixed material at its surface, which will not be bonded and thickened gradually, resulting in better mixing and granulation and longer service life. The selection of proper liner is important for higher filling rate of the drum, and better permeability of the mixed material as well as larger output of the sintered ore.

KeyWords AITranslate

mixing granulation sintering material mixing drum lining material

1曾平生.韶冶烧结制粒技术改造与生产实践[J].有色冶金设计与研究,2007,28(4):1-4. 被引量:1

2曾平生.韶冶铅锌硫化矿高料层烧结焙烧应用研究[J].有色冶金设计与研究,2007,28(5):4-6. 被引量:1

1戴孟良.提高韶冶烧结小矿山矿处理能力的研究与应用[J].有色冶金设计与研究,2011,32(6):17-19.

1从锆英石和二氧化锆生产烧结物料[J].化工矿物与加工,2002,31(9):42-42.

2祁忠.酒钢烧结厂强化制粒及燃料分加工艺的探讨[J].烧结球团,2002,27(1):15-16.

3刘金庭,张立华.湘钢烧结机(105m^2)主要工艺及设备特点[J].钢铁,2000,35(1):1-3. 被引量:1

4查国才.湿法混合制粒的特点与高速混合制粒机的制造要求[J].机电信息,2005(8):44-46. 被引量:5

5范韶梅,陈一忠.430m^2烧结机二混选型分析[J].浙江冶金,2005(2):5-7.

6邵俊,孟君,桑蓉栎,刘建朋.论节能降耗型烧结工序的设计要点及发展趋势[J].中国冶金,2015,25(2):58-61. 被引量:8

7刘金庭.韶关冶炼厂Ⅱ系统烧结工序挖潜改造设计[J].中国有色冶金,2009,38(1):18-21.

8陈永兴.迦南科技湿法混合制粒机获好评[J].机电信息,2009(32):58-58.

9贺建峰.烧结配料计算新方法[J].山东冶金,1995,17(1):25-29. 被引量:1

10彭兵,宋海琛,王佳,柴立元,王云燕,闵小波.Cr_2O_3含碳球团的还原过程[J].中南大学学报:自然科学版,2005,36(4):571-575. 被引量:4

Basic Information:

DOI:

Chinese Library Classification Number:TF3[冶金工程—冶金机械及自动化];TF046.4[冶金工程—冶金物理化学]

Citation Information:

Detailed analysis is made of the granulating mechanism of sintering material and drum liners. Based on comparison of lining materials for engineering purpose and its application, the paper indicated that during production, the ideal liner will adsorb a thin layer of mixed material at its surface, which will not be bonded and thickened gradually, resulting in better mixing and granulation and longer service life. The selection of proper liner is important for higher filling rate of the drum, and better permeability of the mixed material as well as larger output of the sintered ore.

quote

GB/T 7714-2015 [1] YUAN Xue-min. Granulating Mechanism of Mixing Drum and Drum Lining Selection[J]. Rare Metals and Cemented Carbides, 1999(4): 27-30.
MLA [1] YUAN Xue-min. "Granulating Mechanism of Mixing Drum and Drum Lining Selection." Rare Metals and Cemented Carbides, no. 4, 1999, pp. 27-30.
APA [1] YUAN Xue-min. (1999). Granulating Mechanism of Mixing Drum and Drum Lining Selection. Rare Metals and Cemented Carbides(4), 27-30.
IEEE [1] YUAN Xue-min, "Granulating Mechanism of Mixing Drum and Drum Lining Selection," Rare Metals and Cemented Carbides, no. 4, pp. 27-30, 1999. keywords: {mixing granulation;sintering material;mixing drum;lining material}