Precise Measurement of Lattice Constant S in Tungsten and Cobalt AITranslate
Abstract AITranslate
Lattice constants in tungsten and cobalt were precisely measured by X ray diffraction. The results of measurement are that the lattice constant S in tugnsten is a=0.316468nm, and in cobalt is a=0.354410nm. The crystal structure of fcc is dominant in cobalt powder, and hcp only a few.
KeyWords AITranslate
1Yuan-zhi Zhu,Zhe Zhu,Zhi-min Yin,Zhi-dong Xiang.Evolution of carbides and carbon content in matrix of an ultra-high carbon sintered steel during heat treatment process[J].矿物冶金与材料学报:英文版,2009,16(3):299-303. 被引量:2
2晋勇.X射线衍射分析技术课程的实验教学研究[J].实验科学与技术,2014,12(6):172-174. 被引量:6
3何耿煌.碳化物添加剂对硬质合金刀具综合性能的影响[J].稀有金属与硬质合金,2019,47(2):87-92. 被引量:5
1刘敏,夏艳芳,丁晓彤,胡盛礼,彭安国,王孟.关于XRD的开放性实验教学的探讨[J].广东化工,2020,0(3):222-222.
2Yuan-zhi Zhu,Zhe Zhu,Jian-ping Xu.Grain boundary segregation of minor arsenic and nitrogen at elevated temperatures in a microalloyed steel[J].矿物冶金与材料学报:英文版,2012,19(5):399-403. 被引量:2
3Yu Fu,Hao Yu,Pan Tao.On-line spheroidization process of medium-carbon low-alloyed cold heading steel[J].矿物冶金与材料学报:英文版,2014,21(1):26-35.
4韦岩松,黄燕祥,韦联强,李胜英.X射线衍射和能谱联用技术用于锌冶炼废渣的物相分析[J].冶金分析,2016,36(4):52-56. 被引量:2
5孙桂芳,叶杰,刘思彤,韩杰,郝锐.X射线衍射仪在实验教学中的应用[J].课程教育研究,2016,0(32):235-235.
6晋勇.研究型XRD实验教学模式的优化与实践[J].实验科学与技术,2016,14(6):151-153. 被引量:2
7郭智兴,罗天友,鲜广,熊计,陈诚.难熔过渡金属碳化物晶格缺陷演化研究型实验[J].实验室研究与探索,2018,37(12):68-71. 被引量:4
8马宏伟,李晖.本科生X射线结构分析实验教学探索[J].大学化学,2019,34(5):73-79. 被引量:1
9祁志旭,陈兴媚.硬质合金刀具研究进展[J].材料研究与应用,2019,13(4):347-354. 被引量:7
10陈艺聪.CVD涂层α-Al2O3织构制备技术研究[J].工具技术,2020,54(2):71-73.
1魏志全,罗云,王宜金,张晓磊.钎焊工艺对点阵结构残余应力的影响规律研究[J].焊接技术,2016,45(11):17-21.
2刘宁,黄新民,周杰,宫晨利,石敏,张庶元.Ti(C,N)基金属陶瓷中陶瓷相芯/壳组织的观察与分析[J].硅酸盐学报,2000,28(4):381-384. 被引量:9
3罗治平,张少卿,汤亚力.稀土镁合金中的W相及其有序结构W'相的TEM研究[J].中国有色金属学报,1993,3(2):62-66. 被引量:1
4杨晓红,彭丽梅,杨晨辉,贾波,安建.固溶时效Mg-4Y-3Nd合金析出相与基体的微观结构[J].材料热处理学报,2015,36(4):39-43. 被引量:7
5朱祖昌.马氏体转变(十六)[J].热处理技术与装备,2014,35(2):65-70. 被引量:1
6赵伟,李付国,孙燚,杨根林.铸、锻两种状态下TiNiNb合金的热加工性能[J].稀有金属材料与工程,2011,40(5):892-896. 被引量:3
7赵冰,李志强,侯红亮,韩秀全,廖金华,谭谆礼.钛合金三维点阵结构制备工艺与压缩性能研究[J].稀有金属,2017,41(3):258-266. 被引量:9
8高度抗腐蚀及耐磨的冷硬铸件[J].现代铸铁,2002(4):68-68.
9陈大钦,郑子樵,李世晨,刘祖耀,李剑,周明,陈志国.共格沉淀析出过程的模拟Ⅰ——微观结构演化[J].中国有色金属学报,2005,15(12):1945-1952. 被引量:9
10孙丽,陈厚文,王蓉.氩离子轰击感生Ni_2Al_3和NiAl_3成分变化的TEM/EDS研究[J].金属学报,2003,39(2):113-119. 被引量:3
Basic Information:
DOI:
Chinese Library Classification Number:TG146.411[金属学及工艺—金属材料];TG146.412[金属学及工艺—金属材料]
Citation Information:
Lattice constants in tungsten and cobalt were precisely measured by X ray diffraction. The results of measurement are that the lattice constant S in tugnsten is a=0.316468nm, and in cobalt is a=0.354410nm. The crystal structure of fcc is dominant in cobalt powder, and hcp only a few.
quote
| GB/T 7714-2015 | [1] WU Chong-hu, CHEN Shi-ren, ZHANG Shou-quan. Precise Measurement of Lattice Constant S in Tungsten and Cobalt[J]. Rare Metals and Cemented Carbides, 1999(4): 30-36. |
| MLA | [1] WU Chong-hu, et al., "Precise Measurement of Lattice Constant S in Tungsten and Cobalt." Rare Metals and Cemented Carbides, no. 4, 1999, pp. 30-36. |
| APA | [1] WU Chong-hu, CHEN Shi-ren, & ZHANG Shou-quan. (1999). Precise Measurement of Lattice Constant S in Tungsten and Cobalt. Rare Metals and Cemented Carbides(4), 30-36. |
| IEEE | [1] WU Chong-hu, CHEN Shi-ren, and ZHANG Shou-quan, "Precise Measurement of Lattice Constant S in Tungsten and Cobalt," Rare Metals and Cemented Carbides, no. 4, pp. 30-36, 1999. keywords: {tungsten;cobalt;lattice constant;x ray diffraction} |