Ln_2O_3/Al_2O_3 As Catalyst for Synthesizing of Internal Plasticizer DOM AITranslate
Abstract AITranslate
The supported catalyst Ln 2O 3/Al 2O 3 prepared by coprecipitation calcination has remarkable effect on the catalytic synthesis of DOM to larger specific surface and high dispersion.
KeyWords AITranslate
1陈其瑞.-[J].催化学报,1991,12(6):494-494.
2陈其瑞,张凤美,罗明润,焦肇林.Ln_2O_3/Al_2O_3催化酯化合成邻苯二甲酸二辛酯[J].催化学报(英文),1994,15(3):236-238. 被引量:20
3陈其瑞.-[J].化学试剂,1995,17(3):187-187.
4陈其瑞.-[J].稀有金属与硬质合金,1997,(4):11-11.
5陈其瑞,张凤美,罗明润,焦肇林.混合镨钕氧化物催化合成DOP、DOM和DOA[J].稀有金属与硬质合金,1994,22(2):1-4. 被引量:5
1陈其瑞,邵明霞.Ln_2O_3/ZrO_2催化合成DOP、DOM和DOA[J].稀有金属与硬质合金,2001,29(3):23-26. 被引量:1
1陈其瑞.Ln_2O_3/MgO催化合成增塑剂IOP的研究[J].稀有金属与硬质合金,2003,31(4):16-17.
1陈其瑞,邵明霞.Ln_2O_3/ZrO_2催化合成DOP、DOM和DOA[J].稀有金属与硬质合金,2001,29(3):23-26. 被引量:1
2陈其瑞.内增塑剂DOM的稀土催化合成[J].安徽化工,2000,26(3):13-14.
3邹长君.内增塑剂DOM制备方法改进[J].化学世界,1998,39(1):17-18. 被引量:1
4陈其瑞,邵明霞.Ln_2O_3/MgO(Ln=Nd、Sm、Er)催化合成DOP、DOM和DOA[J].稀土,1998,19(4):8-10. 被引量:3
5陈其瑞,孟菁,张凤美,焦肇林.内增塑剂DOM制备方法的改进[J].化学试剂,1995,17(3):187-188. 被引量:5
6吕布,吴培云.Ln_2O_3/x-13分子筛担载型催化剂在合成DOP中的催化活性[J].安徽化工,2000,26(2):21-22.
7国内增塑剂相关的文献题录[J].增塑剂,2011(3):58-60.
8陶建宁.DOP替代趋势逐渐明朗[J].苯酐工业,2010(2):12-13.
9剑尾.Bayer推出新型聚氯酯内增塑剂[J].化学推进剂与高分子材料,2005,3(3):50-50. 被引量:1
10关玉德.制备催化剂的新方法——醇盐法[J].天然气化工—C1化学与化工,1993,18(4):39-41. 被引量:2
Basic Information:
DOI:
Chinese Library Classification Number:TQ414[化学工程];TQ426[化学工程]
Citation Information:
The supported catalyst Ln 2O 3/Al 2O 3 prepared by coprecipitation calcination has remarkable effect on the catalytic synthesis of DOM to larger specific surface and high dispersion.
quote
| GB/T 7714-2015 | [1] CHEN Qi-rui. Ln_2O_3/Al_2O_3 As Catalyst for Synthesizing of Internal Plasticizer DOM[J]. Rare Metals and Cemented Carbides, 1999(4): 24-26. |
| MLA | [1] CHEN Qi-rui. "Ln_2O_3/Al_2O_3 As Catalyst for Synthesizing of Internal Plasticizer DOM." Rare Metals and Cemented Carbides, no. 4, 1999, pp. 24-26. |
| APA | [1] CHEN Qi-rui. (1999). Ln_2O_3/Al_2O_3 As Catalyst for Synthesizing of Internal Plasticizer DOM. Rare Metals and Cemented Carbides(4), 24-26. |
| IEEE | [1] CHEN Qi-rui, "Ln_2O_3/Al_2O_3 As Catalyst for Synthesizing of Internal Plasticizer DOM," Rare Metals and Cemented Carbides, no. 4, pp. 24-26, 1999. keywords: {rare earth oxides;supported cartalyst;catalytic esterification} |