Simulation of Three-roll Spiral Rolling Process of TC17 Titanium Alloy Rod Based on DEFORM-3D and its Application AITranslate
Abstract AITranslate
The three-roll spiral rolling model of TC17 titanium alloy rod was established by using the finite element analysis software DEFORM-3D.The whole rolling process was numerically simulated and the change laws were analyzed of equivalent stress and strain of the rod with 30 mm or 50 mm reduction.And then the experimental study was carried out.The results show that it is feasible to simulate three-roll spiral rolling process of the titanium alloy rod.Controlling reduction can improve the forming quality of the rod,and the metal flow in the rod mainly occurs on the surface during rolling.
KeyWords AITranslate
1王亚芹,刘欣玉,潘露.平三角-圆孔型钛合金棒材轧制过程的三维有限元模拟及应用[J].稀有金属与硬质合金,2014,42(6):38-41. 被引量:2
2何伟,郭征,杜小平,马红征,杨军红.TC6钛合金棒材黑条纹缺陷分析[J].钢铁钒钛,2014,35(6):27-30. 被引量:1
3陈国定,王涛,程凤军.TB6钛合金材料本构关系的试验研究[J].机械科学与技术,2013,32(2):157-159. 被引量:6
4王耀奇,白雪飘,侯红亮.Ti-6Al-4V钛合金热拉伸变形行为与本构方程[J].塑性工程学报,2013,20(5):82-86. 被引量:4
5王晓森,高行山,孙贤,韩鹍,岳珠峰.冷挤压对钛合金紧固结构件的耐久性影响研究[J].机械科学与技术,2012,31(10):1601-1604. 被引量:3
6LOPATIN N V. Effect of hot rolling microstructure of a Ti-6Al-4V titaniu Forming by screw mill on m alloy[J]. Inter- ,2013,6 (4) : 459-465.
7王路,孙宝寿,彭文飞,束学道.钛合金棒材三辊斜轧的数值模拟研究[J].热加工工艺,2015,44(1):116-119. 被引量:3
8张文明,高硕,曹振鹏.硬质合金组合式轧辊在棒材切分轧制中的应用[J].稀有金属与硬质合金,2014,42(3):69-71. 被引量:2
9GALIYEV A, SITDIKOV O, KAIBYSHEV R. Deform- ation behavior and controlling mechanisms for plastic flow of magnesium and magnesium alloy[J]. Materials Transactions, 2003,44 (4) : 426-435.
1袁思波,程军,韩建业,于振涛,皇甫强,牛金龙,余森.一种新型钛合金无缝管轧制过程中应力应变有限元模拟分析[J].广东化工,2017,44(8):62-64. 被引量:2
2苏春民,范茂艳,钟仁智,徐文帅,黄常勋,葛波,邹吉猛.有限元模拟验证TC17钛合金前轴颈精密成形过程中变形和微观结构的关系[J].锻压技术,2021,46(9):224-229.
3常彬彬,帅美荣,刘鑫.棒材三辊孔型自由宽展流动模型[J].锻压技术,2021,46(11):207-214. 被引量:3
1赵峻,周玉,王晓玉,童宣宝.异步热轧高锰无磁钢剪切应变场有限元分析[J].巢湖学院学报,2019,21(6):110-115.
2白辉东,刘华堂,侯沛云.立式九辊轧机的孔型标定与调整[J].锻压技术,2022,47(5):181-187. 被引量:2
3李亮,帅美荣,田恒光,王建梅,王辉绵.基于孔型形状系数的双相不锈钢棒材宽展模型研究[J].精密成形工程,2023,15(2):78-85.
4陈晨,双远华,陈建勋,苟毓俊,李潮.钛合金无缝管斜连轧新工艺研究[J].稀有金属材料与工程,2023,52(3):959-967.
5张金飞,李子正,尹宝良,邝霜,陈彤,白振华.热连轧机组宽展量预报模型及其影响因素[J].塑性工程学报,2023,30(7):205-211.
1张新旺,王勇,吴晓炜.钛合金棒材三辊螺旋轧制成形数值模拟[J].锻压技术,2011,36(1):61-64. 被引量:3
2张宏轩,王瑞雪,谢君贤,程明.纯铜棒材三辊螺旋轧制过程数值模拟[J].铜业工程,2016(6):15-18.
Basic Information:
DOI:
Chinese Library Classification Number:TG335.62[金属学及工艺—金属压力加工]
Citation Information:
The three-roll spiral rolling model of TC17 titanium alloy rod was established by using the finite element analysis software DEFORM-3D.The whole rolling process was numerically simulated and the change laws were analyzed of equivalent stress and strain of the rod with 30 mm or 50 mm reduction.And then the experimental study was carried out.The results show that it is feasible to simulate three-roll spiral rolling process of the titanium alloy rod.Controlling reduction can improve the forming quality of the rod,and the metal flow in the rod mainly occurs on the surface during rolling.
quote
| GB/T 7714-2015 | [1] WANG Rui, JIANG Li-li. Simulation of Three-roll Spiral Rolling Process of TC17 Titanium Alloy Rod Based on DEFORM-3D and its Application[J]. Rare Metals and Cemented Carbides, 2016(5): 70-73. |
| MLA | [1] WANG Rui, and JIANG Li-li. "Simulation of Three-roll Spiral Rolling Process of TC17 Titanium Alloy Rod Based on DEFORM-3D and its Application." Rare Metals and Cemented Carbides, no. 5, 2016, pp. 70-73. |
| APA | [1] WANG Rui, & JIANG Li-li. (2016). Simulation of Three-roll Spiral Rolling Process of TC17 Titanium Alloy Rod Based on DEFORM-3D and its Application. Rare Metals and Cemented Carbides(5), 70-73. |
| IEEE | [1] WANG Rui and JIANG Li-li, "Simulation of Three-roll Spiral Rolling Process of TC17 Titanium Alloy Rod Based on DEFORM-3D and its Application," Rare Metals and Cemented Carbides, no. 5, pp. 70-73, 2016. keywords: {TC17 titanium alloy rod;three-roll spiral rolling;DEFORM-3D;numerical simulation;reduction} |