Development of a variable tensioning system to reduce separation force in large scale stereolithography AITranslate

The University of Texas at Austin; The University of Texas at Austin; The University of Texas at Austin; The University of Texas at Austin; The University of Texas at Austin;Lawrence Livermore National Laboratory
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Projection micro stereolithography (PµSL) is an additive manufacturing tool that offers multiple advantages, including unparalleled resolution and throughput, but the ability to print high viscosity resin for large-scale parts is limited. One of the key challenges in PµSL is to separate a newly polymerized layer from the vat floor without damaging the part. Since the separation force scales with the printing area, the risk of damaging the part increases significantly with larger-scale systems and must be addressed. In this paper, a novel roll-to-roll, variable tensioning system is proposed to reduce the separation force during printing. A mathematical model is proposed to predict the separation force for different 2D geometries, and a set of experiments is conducted on an experimental prototype to validate the model. The effects of different separation parameters including peel rate and peel angle are discussed in detail. The results show that the proposed tensioning system reduces the separation force significantly.

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.addma.2020.101816

Chinese Library Classification Number:

Citation Information:

Projection micro stereolithography (PµSL) is an additive manufacturing tool that offers multiple advantages, including unparalleled resolution and throughput, but the ability to print high viscosity resin for large-scale parts is limited. One of the key challenges in PµSL is to separate a newly polymerized layer from the vat floor without damaging the part. Since the separation force scales with the printing area, the risk of damaging the part increases significantly with larger-scale systems and must be addressed. In this paper, a novel roll-to-roll, variable tensioning system is proposed to reduce the separation force during printing. A mathematical model is proposed to predict the separation force for different 2D geometries, and a set of experiments is conducted on an experimental prototype to validate the model. The effects of different separation parameters including peel rate and peel angle are discussed in detail. The results show that the proposed tensioning system reduces the separation force significantly.

quote

GB/T 7714-2015 [1] Hongtao Song, Nicholas A. Rodriguez, Carolyn Conner Seepersad, et al. Additive Manufacturing, 2021(38). DOI:10.1016/j.addma.2020.101816.
MLA [1] Hongtao Song, et al., Additive Manufacturing, no. 38, 2021, https://doi.org/10.1016/j.addma.2020.101816.
APA [1] Hongtao Song, Nicholas A. Rodriguez, Carolyn Conner Seepersad, Richard H. Crawford, Morgan Chen, & Eric B. Duoss. (2021). Additive Manufacturing(38). https://doi.org/10.1016/j.addma.2020.101816
IEEE [1] Hongtao Song, Nicholas A. Rodriguez, Carolyn Conner Seepersad, Richard H. Crawford, Morgan Chen, and Eric B. Duoss, Additive Manufacturing, no. 38, 2021, doi: 10.1016/j.addma.2020.101816.