daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Fused filament fabrication of polypropylene: Influence of the bead temperature on adhesion and porosity AITranslate

IMT Lille Douai, Ecole nationale supérieure Mines-Télécom Lille Douai;IMT Lille Douai, Ecole nationale supérieure Mines-Télécom Lille Douai;IMT Lille Douai, Ecole nationale supérieure Mines-Télécom Lille Douai
AITranslate
Publisher: Elsevier
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The mechanical properties of the parts produced using fused filament fabrication (FFF) strongly depend on the adhesion strength between beads (FA), which substantially depends on the temperature of the polypropylene (PP) beads during their deposition. In this work, the temperature of the beads was controlled through the adjustment of the nozzle temperature (Tn) and the manufacturing chamber temperature (Tch) in order to control respectively the PP temperature at the nozzle end and the cooling of the PP beads after their deposition. SEM observations revealed an improvement of the coalescence between overlayed beads of different layers and between adjacent beads in the same layer with the increase in Tn. The increase of Tch promotes mainly the coalescence between adjacent beads within the layer. These observations were confronted with uniaxial tensile tests based on a Mode III fracture experiment allowed quantifying the influence of Tn and Tch on the adhesion strength between overlayed beads of different layers. Results reveals a weak increase in FA caused by the increase in the manufacturing chamber temperature from 80 °C to 100 °C, while an increase in the nozzle temperature from 170 °C to 180 °C causes a 145% FA increase. In the same time, this decrease in the manufacturing chamber temperature causes an important increase in porosity and a substantial decrease in the adhesion strength between layers. Graphical Download : Download high-res image (394KB) Download : Download full-size image

KeyWords AITranslate

No data

Basic Information:

DOI:https://doi.org/10.1016/j.addma.2021.101838

Chinese Library Classification Number:

Citation Information:

The mechanical properties of the parts produced using fused filament fabrication (FFF) strongly depend on the adhesion strength between beads (FA), which substantially depends on the temperature of the polypropylene (PP) beads during their deposition. In this work, the temperature of the beads was controlled through the adjustment of the nozzle temperature (Tn) and the manufacturing chamber temperature (Tch) in order to control respectively the PP temperature at the nozzle end and the cooling of the PP beads after their deposition. SEM observations revealed an improvement of the coalescence between overlayed beads of different layers and between adjacent beads in the same layer with the increase in Tn. The increase of Tch promotes mainly the coalescence between adjacent beads within the layer. These observations were confronted with uniaxial tensile tests based on a Mode III fracture experiment allowed quantifying the influence of Tn and Tch on the adhesion strength between overlayed beads of different layers. Results reveals a weak increase in FA caused by the increase in the manufacturing chamber temperature from 80 °C to 100 °C, while an increase in the nozzle temperature from 170 °C to 180 °C causes a 145% FA increase. In the same time, this decrease in the manufacturing chamber temperature causes an important increase in porosity and a substantial decrease in the adhesion strength between layers. Graphical Download : Download high-res image (394KB) Download : Download full-size image

quote

GB/T 7714-2015 [1] Sébastien Charlon, Julien Le Boterff, Jérémie Soulestin. Additive Manufacturing, 2021(38). DOI:10.1016/j.addma.2021.101838.
MLA [1] Sébastien Charlon, et al., Additive Manufacturing, no. 38, 2021, https://doi.org/10.1016/j.addma.2021.101838.
APA [1] Sébastien Charlon, Julien Le Boterff, & Jérémie Soulestin. (2021). Additive Manufacturing(38). https://doi.org/10.1016/j.addma.2021.101838
IEEE [1] Sébastien Charlon, Julien Le Boterff, and Jérémie Soulestin, Additive Manufacturing, no. 38, 2021, doi: 10.1016/j.addma.2021.101838.