daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Direct Synthesis of A-Type Molecular Sieve from Rare Earth Tailings by Hydrothermal Method AITranslate

Key Laboratory of Efficient and Clean Combustion in Inner Mongolia Autonomous Region,School of Energy and Environment,Inner Mongolia University of Science&Technology;Key Laboratory of Efficient and Clean Combustion in Inner Mongolia Autonomous Region,School of Energy and Environment,Inner Mongolia University of Science&Technology;Key Laboratory of Efficient and Clean Combustion in Inner Mongolia Autonomous Region,School of Energy and Environment,Inner Mongolia University of Science&Technology;Key Laboratory of Efficient and Clean Combustion in Inner Mongolia Autonomous Region,School of Energy and Environment,Inner Mongolia University of Science&Technology;Key Laboratory of Efficient and Clean Combustion in Inner Mongolia Autonomous Region,School of Energy and Environment,Inner Mongolia University of Science&Technology
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites Download PDF

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Taking the Bayan Obo rare earth tailings as raw materials,alkali melt-activated rare earth tailings as silicon source and sodium metaaluminate as aluminum source,A-type molecular sieve was direct synthetized by hydrothermal method to realize the secondary utilization of rare earth tailings.The effects of the amount of alkali addition on the silicon activation of rare earth tailings and the amount of sodium metaaluminate addition on the synthesis of the molecular sieve were studied,and the phase composition,micro-morphology,and pore structure of the synthesized molecular sieve were analyzed by XRF,XRD,SEM-EDS,and BET.The results show that when the alkali-ore mass ratio is 3,the tailings are fully activated and the crystalline silicon species are transformed into soluble active Si element,of which the dissolution rate is 84%.Under the template-free condition,the A-type molecular sieve can be synthesized from alkali melt-activated rare earth tailings with different SiO2/Al_2O3 molar ratios,presenting a regular spherical structure with large specific surface area and pore volume,with the pore structure in microporous form.When SiO2/Al2O3 molar ratios is 1.5,the synthesized A-type molecular sieve has the maximum specific surface area of 215.5 m2/g.Fe,Mg and Si in the tailings react with Al to form ferric aluminum anthophyllite impurities,which reduce the crystallinity of the A-type molecular sieve.

KeyWords AITranslate

rare earth tailings alkali melting activation hydrothermal method molecular sieve resource

1张晨,杨诚,李明阳,高翔鹏,于先坤,童雄,龙红明.尾废基地质聚合物制备分子筛的合成方法及在工业废水处理中的应用研究进展[J].过程工程学报,2022,22(6):720-733. 被引量:1

2高宁宁,刘相李,拓鹏飞,高俊魁,钟进,王辉国,郁灼.低硅X分子筛的合成研究[J].石油炼制与化工,2022,53(2):69-76. 被引量:1

3曹吉林,王颖,谭朝阳,刘秀伍.高岭土碱熔活化法制备4A型沸石研究[J].非金属矿,2007,30(1):23-25. 被引量:22

4孔德顺,李志,范佳鑫,吴红,连明磊.膨润土碱熔活化水热合成NaP沸石分子筛[J].无机盐工业,2013,45(3):22-24. 被引量:6

5李贵贤,袁琦罡,贠宏飞,张峰博.凹凸棒NaY分子筛模板炭材料的制备及其电化学性能研究[J].当代化工,2014,43(11):2211-2214. 被引量:1

6郑淑琴,程远坤,钱东,姚华.硅藻土的改性处理及合成NaY分子筛的初步研究[J].石油学报(石油加工),2012,28(4):550-554. 被引量:3

7刘海燕,孙鑫艳,郑涛,刘植昌.不同活化方法对天然硅铝矿物活化及分子筛合成效果的影响[J].燃料化学学报,2020,48(3):328-337. 被引量:3

8刘文卓,刘洋,李雲,郭宏飞,曹吉林.NaOH-NaCl亚熔盐法活化含钾岩石制备SOD沸石[J].过程工程学报,2023,23(2):263-271. 被引量:1

9李娜,陈泽东,李华,武文斐,侯丽敏,王晶晶,张凯.氟碳铈精矿矿物学分析及负载锰的NH_(3)-SCR脱硝性能的研究[J].中国稀土学报,2021,39(6):890-902. 被引量:3

1张银河.河南盐碱资源概论[J].中国盐业,2023(6):41-46.

2李珍珍.富钛料制备中不同亚熔盐反应介质及工艺参数的影响研究[J].山西冶金,2023,46(3):21-23.

3张飞燕,纪开鑫,韩颖.我国关闭煤矿潜在资源分析及二次利用前景[J].中国煤炭,2023,49(1):64-68.

4沈茂森,赵永岗.白云鄂博矿床中究竟发现了多少种矿物[J].包钢科技,2023,49(1):6-9.

5王潇,李鑫,王天宇,刘宏涛.氟班色林片的制备工艺研究[J].西北药学杂志,2023,38(5):92-97.

6尹学杰,陈德胜,王丽娜,赵宏欣,甄玉兰,齐涛,王猛.Na_(2)O-TiO_(2)-SiO_(2)-CaO-Al_(2)O_(3)-V2O5-MnO-MgO-FeO渣系渣铁间硫分配比热力学模型[J].过程工程学报,2023,23(1):124-135.

7周彦阔,全学军,封承飞,蹇成宗.微波强化焙烧铬铁矿液相氧化浸出研究[J].重庆理工大学学报:自然科学,2023,37(4):315-320.

8张红智,张燕挺,宋金锐,刘景怡,高玉芳,李宁,李晓峰.晶种溶液辅助合成ZSM-5沸石及偏三甲苯异构化催化性能研究[J].硅酸盐通报,2023,42(7):2563-2578.

9彭雨涵,周舸,韩金科,张浩宇,林立,陈立佳.AlFeCoNiMo_(0.2)在不同pH值的3.5%NaCl酸性溶液中的腐蚀行为[J].中国冶金,2023,33(7):65-72.

10王诗桥,张西标,李涛,于利红,路文学.醋酸废水分离提纯及合成的研究进展[J].山东化工,2023,52(13):85-88.

Basic Information:

DOI:

Chinese Library Classification Number:TD983[矿业工程—选矿]

Citation Information:

Taking the Bayan Obo rare earth tailings as raw materials,alkali melt-activated rare earth tailings as silicon source and sodium metaaluminate as aluminum source,A-type molecular sieve was direct synthetized by hydrothermal method to realize the secondary utilization of rare earth tailings.The effects of the amount of alkali addition on the silicon activation of rare earth tailings and the amount of sodium metaaluminate addition on the synthesis of the molecular sieve were studied,and the phase composition,micro-morphology,and pore structure of the synthesized molecular sieve were analyzed by XRF,XRD,SEM-EDS,and BET.The results show that when the alkali-ore mass ratio is 3,the tailings are fully activated and the crystalline silicon species are transformed into soluble active Si element,of which the dissolution rate is 84%.Under the template-free condition,the A-type molecular sieve can be synthesized from alkali melt-activated rare earth tailings with different SiO2/Al_2O3 molar ratios,presenting a regular spherical structure with large specific surface area and pore volume,with the pore structure in microporous form.When SiO2/Al2O3 molar ratios is 1.5,the synthesized A-type molecular sieve has the maximum specific surface area of 215.5 m2/g.Fe,Mg and Si in the tailings react with Al to form ferric aluminum anthophyllite impurities,which reduce the crystallinity of the A-type molecular sieve.

quote

GB/T 7714-2015 [1] HOU Li-min, XU Jie, HE Yang, et al. Direct Synthesis of A-Type Molecular Sieve from Rare Earth Tailings by Hydrothermal Method[J]. Rare Metals and Cemented Carbides, 2023(4): 57-64.
MLA [1] HOU Li-min, et al., "Direct Synthesis of A-Type Molecular Sieve from Rare Earth Tailings by Hydrothermal Method." Rare Metals and Cemented Carbides, no. 4, 2023, pp. 57-64.
APA [1] HOU Li-min, XU Jie, HE Yang, LI Hao-bo, & WU Wen-fei. (2023). Direct Synthesis of A-Type Molecular Sieve from Rare Earth Tailings by Hydrothermal Method. Rare Metals and Cemented Carbides(4), 57-64.
IEEE [1] HOU Li-min, XU Jie, HE Yang, LI Hao-bo, and WU Wen-fei, "Direct Synthesis of A-Type Molecular Sieve from Rare Earth Tailings by Hydrothermal Method," Rare Metals and Cemented Carbides, no. 4, pp. 57-64, 2023. keywords: {rare earth tailings;alkali melting activation;hydrothermal method;molecular sieve;resource}