Preparation of Nd3+ Doped LaBO3 Phosphors by Solution Combustion Method AITranslate
Abstract AITranslate
Using La(NO3)3·6H2O and H3BO3 as raw materials,C2H5NO2 as combustion agent,and Nd(NO3)3·6H2O as modifier,Nd3+ doped LaBO3 phosphors were synthesized by solution combustion method.The products were characterized by X-ray diffraction(XRD),scanning electron microscope(SEM),ultraviolet-visible diffuse reflection spectrum(UV-Vis DRS),and fluorescence spectrum(PL).The results show that the prepared powders are all orthorhombic lanthanum borate and the phosphors prepared under the optimized conditions of calcination temperature of 875 ℃ and Nd3+ doping amount of 3% have the best luminescent performance,showing good light absorption performance in both ultraviolet and visible light regions and emitting blue-green light,which can be widely used in the fields of laser illumination and LED lighting.
KeyWords AITranslate
1闫伟鹏,符荣,周宇,王亚楠,凌凤香,储刚.溶液燃烧法制备B改性的γ-Al_2O_3及其机理探讨[J].精细石油化工,2018,35(2):29-32. 被引量:2
2潘金根,王景,殷洁,潘尚可,潘建国.Nd^(3+)掺杂Gd_2O_3的合成及近红外发光性能[J].人工晶体学报,2015,44(12):3488-3492. 被引量:1
3麦海翔,谢致薇,徐继承,胡典禄,杨元政,陈先朝,何玉定.Eu、Nd、Y稀土掺杂CuAlO_2纳米粉末制备及相组织研究[J].功能材料,2015,46(17):17076-17081. 被引量:1
4杨儒,陶振林,秦杰,李敏.Nd∶YAG陶瓷粉体的晶相组成与发光性能[J].北京化工大学学报:自然科学版,2009,36(4):54-59. 被引量:2
5储刚,吴静,付丽婷,贾雅薇,吴钳,张静,孟竺.微波诱导燃烧法制备Nd^(3+)掺杂LaBO_(3)粉体及表征[J].化学研究与应用,2021,33(8):1589-1594. 被引量:1
1贾洋刚,陈诗洁,邵霞,程婕,林娜,方道来,冒爱琴,李灿华.高性能无钴化钙钛矿型高熵氧化物负极材料的制备及储锂性能研究[J].化学学报,2023,81(5):486-495. 被引量:1
2王立明,贾雅薇,孟竺,付丽婷,吴静,宋丽娟,储刚.钐掺杂改性γ-Al_(2)O_(3)粉体的热稳定性研究[J].稀有金属与硬质合金,2023,51(3):47-51.
3刘一诺,魏树权,徐丹丹,李刚.Ag/Bi_(5)O_(7)I/g-C_(3)N_(4)复合材料的制备及光催化性能研究[J].哈尔滨师范大学自然科学学报,2023,39(2):57-63.
4胡文丽,陈卫,王洪涛.高致密性Yb^(3+)和Gd^(3+)双掺杂CeO_(2)中温电解质的合成及其电性能研究[J].安阳师范学院学报,2023(2):13-17.
5郑旭惠,何艺施,赵文荻,李佳蔓,黄慧茹,江烨琳,朱健,任学梁.甘氨酸-硝酸盐燃烧合成制备铜/铁基纳米催化剂及表征[J].云南化工,2023,50(6):30-32.
6江海波,任鑫,劳学斌,钟美莲,孔安廷,姚政,施利毅.镓离子掺杂量对ZnO压敏电阻性能的影响[J].电瓷避雷器,2023(4):46-50.
7苏新悦,孔存辉,庆达,赵英娜,王建省.Ti_(3)C_(2)/SrTiO_(3)复合材料的制备及其光电化学阴极保护性能[J].复合材料学报,2023,40(7):3964-3972.
8赵巧丽,李龙.回火温度对LiNi_(0.5)Mn_(1.5)O_(4)结构、形貌及电化学性能的影响[J].河南化工,2023,40(9):33-35.
9李燕,张俊杰,郭俊明.Ni-La双掺LiMn_(2)O_(4)截角八面体正极材料的制备及电化学性能[J].材料导报,2023,37(14):16-23.
10吕奕菊,梁勇清,谭家栩,张晨霞,刘峥,邹品田.改性水系钠离子电极材料Na_(3)V_(2)(PO_(4))_(3)的制备及性能[J].材料工程,2023,51(9):158-166.
Basic Information:
DOI:
Chinese Library Classification Number:O614[理学—无机化学]
Citation Information:
Using La(NO3)3·6H2O and H3BO3 as raw materials,C2H5NO2 as combustion agent,and Nd(NO3)3·6H2O as modifier,Nd3+ doped LaBO3 phosphors were synthesized by solution combustion method.The products were characterized by X-ray diffraction(XRD),scanning electron microscope(SEM),ultraviolet-visible diffuse reflection spectrum(UV-Vis DRS),and fluorescence spectrum(PL).The results show that the prepared powders are all orthorhombic lanthanum borate and the phosphors prepared under the optimized conditions of calcination temperature of 875 ℃ and Nd3+ doping amount of 3% have the best luminescent performance,showing good light absorption performance in both ultraviolet and visible light regions and emitting blue-green light,which can be widely used in the fields of laser illumination and LED lighting.
quote
| GB/T 7714-2015 | [1] TAI Yue, FU Li-ting, MENG Zhu, et al. Preparation of Nd3+ Doped LaBO3 Phosphors by Solution Combustion Method[J]. Rare Metals and Cemented Carbides, 2023(4): 52-56. |
| MLA | [1] TAI Yue, et al., "Preparation of Nd3+ Doped LaBO3 Phosphors by Solution Combustion Method." Rare Metals and Cemented Carbides, no. 4, 2023, pp. 52-56. |
| APA | [1] TAI Yue, FU Li-ting, MENG Zhu, XU Ling-zi, WU Jing, JIA Ya-wei, & CHU Gang. (2023). Preparation of Nd3+ Doped LaBO3 Phosphors by Solution Combustion Method. Rare Metals and Cemented Carbides(4), 52-56. |
| IEEE | [1] TAI Yue, FU Li-ting, MENG Zhu, XU Ling-zi, WU Jing, JIA Ya-wei, and CHU Gang, "Preparation of Nd3+ Doped LaBO3 Phosphors by Solution Combustion Method," Rare Metals and Cemented Carbides, no. 4, pp. 52-56, 2023. keywords: {lanthanum borate;solution combustion method;Nd doping;fluorescence} |