Abstract AITranslate
High-entropy ceramics has become a major focus in the research of new ceramics in recent years,with promising prospects of development and application in the aerospace industry.High-entropy oxide ceramic coatings,designed based on the high-entropy strategy,can better solve the deficiencies of key performance of thermal/environmental barrier coatings,including service life,oxidation resistance,and CMAS(Ca/Mg/Al/Si oxides) corrosion resistance at high temperatures.The article reviews the research progress of quintuple-element high-entropy rare earth salt materials in different systems as alternate candidates in the field of thermal/environmental barrier coatings in recent years,and summarizes the characteristics of the materials in terms of structure,performance and main application fields.Finally,the future development direction of high-entropy rare earth salt ceramic coatings is discussed to provide insights for further research and development as well as optimization of key performance of the new material systems.
KeyWords AITranslate
1李庆科,王超会,王春圻,李广书,李晓生,林蔚,王铀.环境障涂层材料及结构的研究进展[J].化学世界,2020,61(4):229-236. 被引量:4
2郑伟,张佳平,杨翠波.陶瓷基复合材料环境障涂层研究进展[J].纤维复合材料,2021,38(2):65-72. 被引量:5
3马壮,张学勤,刘玲.环境障涂层的发展瓶颈及应对措施[J].中国表面工程,2020(5):99-114. 被引量:5
4刘涛,马北越,昝文宇.稀土盐类热障/环境障涂层研究现状[J].耐火材料,2023,57(2):175-179. 被引量:1
5李新慧,马文,尹轶川,马伯乐,白玉,贾瑞灵,董红英.液相等离子喷涂SrZrO_3热障涂层工艺的研究[J].中国腐蚀与防护学报,2017,37(1):41-46. 被引量:1
6吕自豪,顾华志,杨爽.高熵陶瓷国内外研究进展[J].耐火与石灰,2022,47(1):5-10. 被引量:1
7Huimin XIANG,Yan XING,Fu-zhi DAI,Hongjie WANG,Lei SU,Lei MIAO,Guojun ZHANG,Yiguang WANG,Xiwei QI,Lei YAO,Hailong WANG,Biao ZHAO,Jianqiang LI,Yanchun ZHOU.High-entropy ceramics:Present status,challenges,and a look forward[J].先进陶瓷(英文),2021,10(3):385-441. 被引量:18
8张伟明,向会敏,戴付志,孙志梅,周延春.高熵陶瓷:吸波材料设计新策略[J].宇航材料工艺,2022,52(2):13-25. 被引量:1
9Zifan Zhao,Heng Chen,Huimin Xiang,Fu-Zhi Dai,Xiaohui Wang,Wei Xu,Kuang Sun,Zhijian Peng,Yanchun Zhou.High-entropy(Y0.2Nd0.2Sm0.2Eu0.2Er0.2)AlO3:A promising thermal/environmental barrier material for oxide/oxide composites[J].材料科学技术:英文版,2020,47(12):45-51. 被引量:8
10Zifan ZHAO,Huimin XIANG,Heng CHEN,Fu-Zhi DAI,Xiaohui WANG,Zhijian PENG,Yanchun ZHOU.High-entropy(Nd_(0.2)Sm_(0.2)Eu_(0.2)Y_(0.2)Yb_(0.2))_(4)Al_(2)O_(9) with good high temperature stability,low thermal conductivity,and anisotropic thermal expansivity[J].先进陶瓷(英文),2020,9(5):595-605. 被引量:10
1崔铖,李双燕,崔李苹,杨俊琪,杨雪尧,李春雷,董国伟.铝合金硫酸阳极氧化添加剂和绿色封闭剂研究现状[J].电镀与涂饰,2023,42(14):11-20.
2陈年喜.流动理发人(外一篇)[J].天涯,2023(4):177-182.
3徐海阳.高压气淬热处理对高压辊磨机用硬质合金柱钉的性能影响[J].稀有金属与硬质合金,2023,51(4):88-91.
4惠俊杰,贾均红,白甘雨,岳瑞芳,张心怡,李金鑫.(MgCoNiCuZn)O高熵氧化物陶瓷涂层的制备及性能[J].机械工程材料,2023,47(5):41-46.
5徐初琪,董建业,彭儒,胡思堑,黄凯龙.海上光伏腐蚀防护系统性解决方案[J].上海涂料,2023,61(4):33-37.
6酒荣跃,刘嘉东.大型浮顶罐罐顶外表面的腐蚀与防护[J].石油化工腐蚀与防护,2023,40(4):31-34.
7师海峰,施子婧,孟刚刚.清洁能源轨道工程车网络控制及能量管理策略设计[J].智慧轨道交通,2023,60(5):20-24.
8赵强,李海,叶才铭,徐舟,罗俊卿,郭辉,盛波.燃油喷嘴精密微细零件加工工艺研究[J].航空精密制造技术,2023,59(3):1-3.
9桂庆霞,刘逸.“成长共同体”理念下自主课堂模式探析[J].北京教育:普教版,2023(8):84-85.
10陈传勇,瞿明敏,卢志辉,赵建江,宣海军,李洋,刘芳,王威.高转速下原位加热系统理论设计[J].铸造设备与工艺,2023(4):10-17.
Basic Information:
DOI:
Chinese Library Classification Number:V261.933[航空宇航科学与技术—航空宇航制造工程]
Citation Information:
High-entropy ceramics has become a major focus in the research of new ceramics in recent years,with promising prospects of development and application in the aerospace industry.High-entropy oxide ceramic coatings,designed based on the high-entropy strategy,can better solve the deficiencies of key performance of thermal/environmental barrier coatings,including service life,oxidation resistance,and CMAS(Ca/Mg/Al/Si oxides) corrosion resistance at high temperatures.The article reviews the research progress of quintuple-element high-entropy rare earth salt materials in different systems as alternate candidates in the field of thermal/environmental barrier coatings in recent years,and summarizes the characteristics of the materials in terms of structure,performance and main application fields.Finally,the future development direction of high-entropy rare earth salt ceramic coatings is discussed to provide insights for further research and development as well as optimization of key performance of the new material systems.
quote
| GB/T 7714-2015 | [1] ZAN Wen-yu, MA Bei-yue, LIU Tao. Research Progress of High-Entropy Rare Earth Salt Thermal/Environmental Barrier Ceramic Coating Systems[J]. Rare Metals and Cemented Carbides, 2023(4): 65-72. |
| MLA | [1] ZAN Wen-yu, et al., "Research Progress of High-Entropy Rare Earth Salt Thermal/Environmental Barrier Ceramic Coating Systems." Rare Metals and Cemented Carbides, no. 4, 2023, pp. 65-72. |
| APA | [1] ZAN Wen-yu, MA Bei-yue, & LIU Tao. (2023). Research Progress of High-Entropy Rare Earth Salt Thermal/Environmental Barrier Ceramic Coating Systems. Rare Metals and Cemented Carbides(4), 65-72. |
| IEEE | [1] ZAN Wen-yu, MA Bei-yue, and LIU Tao, "Research Progress of High-Entropy Rare Earth Salt Thermal/Environmental Barrier Ceramic Coating Systems," Rare Metals and Cemented Carbides, no. 4, pp. 65-72, 2023. keywords: {high-entropy ceramics;rare earth salt;thermal barrier coating;environmental barrier coating;re-search progress} |