Effect of Different Dielectrics on Preparation of TiAl Alloy Powder AITranslate

Naval Equipment Department;Naval Equipment Department;Naval Equipment Department;Naval Equipment Department
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Using Ti-46.2%Al-8%Ta as the experimental material,TiAl based alloy powder was prepared by spark plasma discharge method with different dielectrics.The results show that when the dielectric is anhydrous ethanol,the composition of the prepared powder is TiC and Al2O3,the sphericity of the powder is very low,and the oxygen content is very high.When the dielectric is liquid nitrogen,the powder is composed of TiN and AlN,and the nitrogen content in the powder is very high.When the dielectric is liquid argon,the composition of the prepared powder is TiAl,and the quality of the powder is relatively high,but the powder yield is very low.In subsequent research,liquid argon can be used as the dielectric and the process parameters need to be continuously optimized to further increase the output of the powder,while the quality of the powder is ensured.

KeyWords AITranslate

TiAl alloy Ti-Al-Ta spark plasma discharge method dielectric

1任保轶,王品,张学军.带有Al_2O_3涂层的γ-TiAl合金高温氧化动力学研究[J].稀有金属与硬质合金,2012,40(5):23-27. 被引量:1

2李亚非,张平则,许浩.等离子表面Cr-Si合金化改善TiAl基合金高温抗氧化性能的研究[J].稀有金属与硬质合金,2012,40(2):36-40. 被引量:3

3李宝辉,侯正全,邱立新,陈斌.TiAl合金精密成形技术研究进展[J].宇航材料工艺,2008,38(5):4-7. 被引量:8

4宋庆功,朱燕霞,王丽杰,顾威风,胡雪兰,康建海.Ce和V双掺杂对γ-TiAl基合金塑性和电子结构的影响[J].稀有金属,2019,43(9):942-951. 被引量:7

5王孟光,孙建科,陈志强.TiAl基合金的熔炼与铸造成形工艺研究现状[J].钛工业进展,2010,27(4):1-4. 被引量:13

6李宝辉,孔凡涛,陈玉勇,陈子勇,张军伟.TiAl金属间化合物的合金设计及研究现状[J].航空材料学报,2006,26(2):72-78. 被引量:31

7于军,葛昌纯,孟璐璐,沈卫平,燕青芝,孟月东.火花等离子体放电制备高温合金细粉新技术[J].金属学报,2008,44(7):892-896. 被引量:8

8黄传收,柳中强,吴苑标,温利平,陈进,肖志瑜.电极感应熔炼气雾化制备Ti-6Al-4V合金粉末的性能及其表征[J].稀有金属材料与工程,2019,48(10):3302-3308. 被引量:7

9刘军,许宁辉,于建宁.用等离子旋转电极雾化法制备TC4合金粉末的研究[J].宁夏工程技术,2016,15(4):340-342. 被引量:17

10王乃娟,吕振,刘丹,朱德贵.电火花放电法制备铂铑合金粉末[J].热加工工艺,2014,43(16):31-33. 被引量:3

1汪敏.电缆局部放电电信号的传播特性研究[J].电气开关,2021,59(5):42-44. 被引量:1

2胡海涛,左家斌,黄东,丁贤飞,南海.浇注系统对离心铸造TiAl合金叶片成形的影响[J].铸造,2021,70(9):1054-1059. 被引量:1

3黎淼,王虎虎,艾桃桃,刘洁,冯小明,赵堃.仿生TiAl基合金的制备及力学性能[J].陕西理工大学学报:自然科学版,2021,37(5):1-10.

4周振宇.大型空压机空气过滤室技术改造[J].安防科技,2021(19):103-103.

5宗师,刘保亮,冯晓花.TC25钛合金锻造工艺研究[J].锻造与冲压,2021(19):56-58. 被引量:1

6张晋,吕华江,曹瑞,周文敏,王婷婷.Ti-1300F钛合金熔炼工艺研究[J].世界有色金属,2021(12):12-14.

7梁直,么伟伟.基于计算机辅助技术的玻纤增强PA66止回阀阀体尺寸精度控制[J].塑料科技,2021,49(9):81-86. 被引量:5

8徐安林,周泽宇.玻纤增强PPA节温器插头注塑成型多目标优化分析[J].塑料科技,2021,49(9):61-65. 被引量:4

9Yang Bao,Lujun Huang,Shan Jiang,Rui Zhang,Qi An,Caiwei Zhang,Lin Geng,Xinxin Ma.A novel Ti cored wire developed for wire-feed arc deposition of TiB/Ti composite coating[J].材料科学技术:英文版,2021(24):145-160.

Basic Information:

DOI:

Chinese Library Classification Number:TG146.2[金属学及工艺—金属材料]

Citation Information:

Using Ti-46.2%Al-8%Ta as the experimental material,TiAl based alloy powder was prepared by spark plasma discharge method with different dielectrics.The results show that when the dielectric is anhydrous ethanol,the composition of the prepared powder is TiC and Al2O3,the sphericity of the powder is very low,and the oxygen content is very high.When the dielectric is liquid nitrogen,the powder is composed of TiN and AlN,and the nitrogen content in the powder is very high.When the dielectric is liquid argon,the composition of the prepared powder is TiAl,and the quality of the powder is relatively high,but the powder yield is very low.In subsequent research,liquid argon can be used as the dielectric and the process parameters need to be continuously optimized to further increase the output of the powder,while the quality of the powder is ensured.

quote

GB/T 7714-2015 [1] LAI Xu-ping, LI Tian-fang, LIU Rui, et al. Effect of Different Dielectrics on Preparation of TiAl Alloy Powder[J]. Rare Metals and Cemented Carbides, 2021(5): 35-40.
MLA [1] LAI Xu-ping, et al., "Effect of Different Dielectrics on Preparation of TiAl Alloy Powder." Rare Metals and Cemented Carbides, no. 5, 2021, pp. 35-40.
APA [1] LAI Xu-ping, LI Tian-fang, LIU Rui, & SUN Hong-liang. (2021). Effect of Different Dielectrics on Preparation of TiAl Alloy Powder. Rare Metals and Cemented Carbides(5), 35-40.
IEEE [1] LAI Xu-ping, LI Tian-fang, LIU Rui, and SUN Hong-liang, "Effect of Different Dielectrics on Preparation of TiAl Alloy Powder," Rare Metals and Cemented Carbides, no. 5, pp. 35-40, 2021. keywords: {TiAl alloy;Ti-Al-Ta;spark plasma discharge method;dielectric}