Research Progress of Biomedical Titanium Alloy AITranslate
Abstract AITranslate
Taking the third-generation titanium alloy as the research object,the preparation processes such as vacuum melting,powder metallurgy,additive manufacturing and gel-casting are introduced,as well as the treatment processes including cold rolling,aging,laser peening and so on.The biocompatibility of biomedical titanium alloy is reviewed,as well as the effects of microelement addition and such treatment processes as cold rolling and aging on the mechanical properties of various as-cast titanium alloys.The application of biomedical titanium alloy is also prospected.
KeyWords AITranslate
1魏芬绒,王海,金旭丹,杨晓康,崔文俊.生物医用钛合金材料及其应用[J].世界有色金属,2018,43(2):260-262. 被引量:17
2李佐臣,周廉,李军,王立新,王克光,蔡玉荣.外科植入物用第三代新型医用钛合金研究[J].钛工业进展,2003,20(4):46-48. 被引量:13
3王永善,李培友,马昕迪,蒲娇.热处理温度对生物医用Ti87Nb8Sn5合金微观组织和力学性能影响[J].材料热处理学报,2020,41(7):49-56. 被引量:3
4李元元,邹黎明,杨超.粉末冶金法合成高强低模超细晶医用钛合金[J].华南理工大学学报:自然科学版,2012,40(10):43-50. 被引量:8
5徐伟,路新,夏青,韩刚,王涛,曲选辉.粉末冶金超细晶医用Ti-Mo-Fe合金的制备与表征[J].稀有金属材料与工程,2017,46(5):1393-1398. 被引量:3
6李伯琼,谢瑞珍,李春林.烧结工艺对医用Ti-Nb-Ta-Zr合金微观结构及性能的影响[J].粉末冶金工业,2020,30(3):58-63. 被引量:4
7何杰,肖志瑜,杨硕,关航健,张文.Ti-29Nb-13Ta-4.6Zr高速压制行为及其烧结性能的研究[J].粉末冶金工业,2017,27(5):12-17. 被引量:8
8陈刚,路新,章林,秦明礼,郭志猛,曲选辉.钛及钛合金粉末制备与近净成形研究进展[J].材料科学与工艺,2020,28(3):98-108. 被引量:17
9韩立影,王存山,羌建兵.激光快速成形Ti_(64.52)Fe_(29.32)Zr_(5.86)Y_(0.30)医用合金组织与性能[J].中国有色金属学报,2018,28(3):474-482. 被引量:2
10许莹,王欢欢,王变.医用多孔β钛合金的制备方法研究进展[J].钛工业进展,2018,35(3):1-5. 被引量:5
1谢凤宽,章浩,刘谦.钛合金微弧氧化膜层摩擦学性能的研究进展[J].材料保护,2022,55(5):167-178. 被引量:4
2纪阿祥,王鸿云,毕成,徐爱群.医用接骨螺钉超声-磁流变抛光励磁装置设计[J].光学精密工程,2022,30(18):2219-2231.
3王彦龙,马昕宇,王庆相.Ti-Ta-Mo合金的制备及其力学性能[J].西安工程大学学报,2022,36(6):31-37.
4麦萍.硬脂酸添加量对多孔Ti-5Cu合金微观结构及性能的影响[J].热加工工艺,2022,51(24):25-29.
5王楚凡,蔡奇,刘金旭,严细锋.Mo含量对粉末冶金Ti-Mo合金组织与力学性能的影响[J].中国有色金属学报,2023,33(2):328-342.
1李宁.超声波辅助铁基体电沉积Zn-Ni-P/纳米ZrO_(2)复合镀层及性能研究[J].电镀与精饰,2023,45(7):8-16.
2邹永纯,王树棋,王亚明,陈国梁,张凯伟,欧阳家虎,贾德昌,周玉.钛合金微弧氧化涂层等离子体电解去除工艺与作用机制[J].材料保护,2023,56(7):25-30.
3赵昕睿,王树棋,付博达,陆寅松,邹永纯,陈国梁,王亚明.TC4合金微弧氧化涂层的组织结构与高温氧化行为研究[J].材料保护,2023,56(7):31-37.
4程赵辉,杨巍,张勇,石小倩,饶模松.纳米Nd_(2)O_(3)对TC11钛合金微弧氧化层耐磨性及高温抗氧化性能的影响[J].材料保护,2023,56(7):38-46.
1付静波,杨秦莉,赵虎,王娜,卜春阳,庄飞.系列Mo-Ti-Zr材料组织性能研究[J].中国钼业,2021,45(5):53-57.
2李海洋,丁玲玲,李家琪,方盈盈,李钢,施越,张志强,李良.碳化硅颗粒铜复合材料制备的研究进展[J].山东化工,2021,50(19):65-67.
Basic Information:
DOI:
Chinese Library Classification Number:TG146.23[金属学及工艺—金属材料]
Citation Information:
Taking the third-generation titanium alloy as the research object,the preparation processes such as vacuum melting,powder metallurgy,additive manufacturing and gel-casting are introduced,as well as the treatment processes including cold rolling,aging,laser peening and so on.The biocompatibility of biomedical titanium alloy is reviewed,as well as the effects of microelement addition and such treatment processes as cold rolling and aging on the mechanical properties of various as-cast titanium alloys.The application of biomedical titanium alloy is also prospected.
quote
| GB/T 7714-2015 | [1] YANG Jia-hui, ZHANG Yi-fan, WU Jun-xia, et al. Research Progress of Biomedical Titanium Alloy[J]. Rare Metals and Cemented Carbides, 2021(5): 29-34. |
| MLA | [1] YANG Jia-hui, et al., "Research Progress of Biomedical Titanium Alloy." Rare Metals and Cemented Carbides, no. 5, 2021, pp. 29-34. |
| APA | [1] YANG Jia-hui, ZHANG Yi-fan, WU Jun-xia, LIU Ya-ling, & LI Pei-you. (2021). Research Progress of Biomedical Titanium Alloy. Rare Metals and Cemented Carbides(5), 29-34. |
| IEEE | [1] YANG Jia-hui, ZHANG Yi-fan, WU Jun-xia, LIU Ya-ling, and LI Pei-you, "Research Progress of Biomedical Titanium Alloy," Rare Metals and Cemented Carbides, no. 5, pp. 29-34, 2021. keywords: {biomedical titanium alloy;preparation process;treatment process;biocompatibility;mechanical property;application prospect} |