Preparation and Characterization of La2Y2Al2O9 Fluorescent Matrix Material AITranslate

School of Petrochemical Engineering,Liaoning Petrochemical University;School of Petrochemical Engineering,Liaoning Petrochemical University;School of Petrochemical Engineering,Liaoning Petrochemical University;School of Petrochemical Engineering,Liaoning Petrochemical University;School of Petrochemical Engineering,Liaoning Petrochemical University;School of Petrochemical Engineering,Liaoning Petrochemical University;School of Petrochemical Engineering,Liaoning Petrochemical University
AITranslate
Publisher: Editorial Office of Rare Metals and Cemented Carbides
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

La2Y2Al2O9 fluorescent matrix material was synthesized by solution combustion method with lanthanum nitrate hexahydrate,yttrium oxide and aluminum nitrate nonahydrate having La:Y:Al molar ratio of 1:1:1 as raw materials,and glycine(C2H5NO2),mannitol(C6H14O6)and urea(CO(NH2)2)as combustion agents,respectively.The effects of calcination temperature,calcination time and combustion agents on the phase and appearance of the synthetic powder were analyzed by X-ray diffractometer(XRD)and scanning electron microscope(SEM).Under the optimized process conditions of glycine(C2H5NO2)as combustion agent,calcination temperature 800℃ and calcination time 4 h,a new compound La2Y2Al2O9 with high crystallinity and purity,good morphology and hammer net distribution can be obtained,and it belongs to the monoclinic crystal system.The luminescent properties of La2Y2Al2O9 powder were characte-rized by ultraviolet visible spectrometer and fluorescence spectrometer.The results show that the product has a wide and strong ultraviolet absorption band at 200~400 nm and a wide fluorescence excitation band at 350~440 nm.Therefore,La2Y2Al2O9 powder can be used as a matrix material in the preparation of luminescent powder.

KeyWords AITranslate

combustion method La2Y2Al2O9 fluorescent matrix glycine

1陈占恒.稀土新材料及其在高技术领域的应用[J].稀土,2000,21(1):53-57. 被引量:80

2袁曦明.Synthesis and Luminescence of Nano Fluorescent Powder of Y_4Al_2O_9:Eu^(3+)[J].武汉理工大学学报:材料科学英文版,2003,18(1):41-43. 被引量:2

3张希艳,姜薇薇,刘学,卢利平,王晓春,柏朝晖,刘全生,曹志峰.CaAl_2O_4:Eu^(2+),Nd^(3+)纳米粉体的合成与发光性质[J].光谱学与光谱分析,2005,25(10):1560-1563. 被引量:6

4ZUO Yinyan,CHEN Xia,LIU Xiaobin.Long Lasting Phosphorescence Properties and Multi-peak Fitting on Thermoluminescence of Red LaAlO3∶Eu3+ Phosphor[J].高等学校化学研究:英文版,2015,0(3):427-429. 被引量:1

5秦菲,王进贤,董相廷,于文生,刘桂霞.YAlO_3∶Eu^(3+)发光纳米纤维的制备与表征[J].中国激光,2012,39(6):143-149. 被引量:8

6方东,王亚娇,陈瑞瑞,李笑妍,张辉,郭琴,储刚.燃烧法制备纳米铝酸镧及其表征[J].粉末冶金工业,2013,23(2):1-5. 被引量:4

7石士考.稀土掺杂钇铝石榴石发光粉合成的新方法[J].稀土,2000,21(3):55-58. 被引量:12

8章少华,周明斌,胡江峰,谢冰.近紫外光激发的白光LED用单基质硅酸盐荧光粉的研究进展[J].材料导报,2009,23(9):25-29. 被引量:17

9袁曦明,许永胜,于江波,田熙科.溶胶-凝胶法制备纳米荧光粉Y_4Al_2O_9:Eu^(3+)的初步研究[J].地球科学:中国地质大学学报,2002,27(4):408-412. 被引量:7

1李楠,木肖玉,乔娟,齐莉.刺激-响应荧光聚合物的液滴微流控合成及其活体分析应用研究[J].光谱学与光谱分析,2020(S01):207-208.

2周仪君,倪梦娜,鲍晶,华馨柠.绿色荧光的粉紫色系尖晶石致色成因及发光机理探讨[J].中国宝石,2021(4):102-105. 被引量:1

3刘勤,张万明.Eu2+、Dy3+、La3++掺杂铝酸盐制备长余辉发光材料研究[J].材料科学,2021,11(10):1067-1075.

4张正工,张泉珍,朱盛华.六水合硝酸镧在乙醇中积分溶解热之测定[J].高等学校化学学报,1985,6(4):343-346.

5袁博,祁超超,张相挺,栾国颜.颜色可调Ca_(2)LaTaO_(6)∶Dy^(3+),Tb^(3+)荧光粉的制备、发光性能及能量传递[J].人工晶体学报,2021,50(9):1715-1722.

6汪正良,李童,袁俊恒.白光LED用K_(2)TaF_(7)∶Mn^(4+)红色发光晶体发光性能研究[J].云南民族大学学报:自然科学版,2021,30(5):488-492.

7张程璐,陈乃宏,苑玉和.帕金森病治疗药物研究进展[J].中国药理学与毒理学杂志,2021,35(10):803-803. 被引量:7

8关坤禹,牛晓巍,杨其磊,余仕选,魏政.Co掺杂对LaFeO_(3)钙钛矿和酸处理对LaFe_(0.2)Co_(0.8)O_(3)催化剂催化效果的影响[J].环境保护与循环经济,2021,41(9):19-23. 被引量:1

9李艳梅,贺龙强,胡鹏,徐燕.木质素磺酸盐基高吸水性树脂的制备及农用研究[J].塑料科技,2021,49(9):39-42.

10胡文杰,殷帅文,戴彩华,周升团.油樟中倍半萜化合物及其衍生物的合成与生物活性研究[J].浙江化工,2021,52(10):12-16. 被引量:1

Basic Information:

DOI:

Chinese Library Classification Number:TQ132.2[化学工程—无机化工]

Citation Information:

La2Y2Al2O9 fluorescent matrix material was synthesized by solution combustion method with lanthanum nitrate hexahydrate,yttrium oxide and aluminum nitrate nonahydrate having La:Y:Al molar ratio of 1:1:1 as raw materials,and glycine(C2H5NO2),mannitol(C6H14O6)and urea(CO(NH2)2)as combustion agents,respectively.The effects of calcination temperature,calcination time and combustion agents on the phase and appearance of the synthetic powder were analyzed by X-ray diffractometer(XRD)and scanning electron microscope(SEM).Under the optimized process conditions of glycine(C2H5NO2)as combustion agent,calcination temperature 800℃ and calcination time 4 h,a new compound La2Y2Al2O9 with high crystallinity and purity,good morphology and hammer net distribution can be obtained,and it belongs to the monoclinic crystal system.The luminescent properties of La2Y2Al2O9 powder were characte-rized by ultraviolet visible spectrometer and fluorescence spectrometer.The results show that the product has a wide and strong ultraviolet absorption band at 200~400 nm and a wide fluorescence excitation band at 350~440 nm.Therefore,La2Y2Al2O9 powder can be used as a matrix material in the preparation of luminescent powder.

quote

GB/T 7714-2015 [1] CHU Gang, WU Jing, JIA Ya-wei, et al. Preparation and Characterization of La2Y2Al2O9 Fluorescent Matrix Material[J]. Rare Metals and Cemented Carbides, 2021(5): 24-28.
MLA [1] CHU Gang, et al., "Preparation and Characterization of La2Y2Al2O9 Fluorescent Matrix Material." Rare Metals and Cemented Carbides, no. 5, 2021, pp. 24-28.
APA [1] CHU Gang, WU Jing, JIA Ya-wei, FU Li-ting, ZHANG Jing, MENG Zhu, & WU Qian. (2021). Preparation and Characterization of La2Y2Al2O9 Fluorescent Matrix Material. Rare Metals and Cemented Carbides(5), 24-28.
IEEE [1] CHU Gang, WU Jing, JIA Ya-wei, FU Li-ting, ZHANG Jing, MENG Zhu, and WU Qian, "Preparation and Characterization of La2Y2Al2O9 Fluorescent Matrix Material," Rare Metals and Cemented Carbides, no. 5, pp. 24-28, 2021. keywords: {combustion method;LaYAlO;fluorescent matrix;glycine}