In Situ Construction of S-Scheme VIn-Zn2In2S5/O-Zn2In2S5 p–n Homojunctions for Enhanced Photocatalytic Hydrogen Evolution AITranslate

AITranslate
Publisher: Youke Publish Co., Ltd.
Share Citation Information Add to Favorites

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The construction of p–n homojunctions represents a promising strategy for effective solar-driven photocatalytic hydrogen evolution, owing to their inherent advantages of superior lattice matching and minimized charge transfer resistance. However, this approach remains largely unexplored. Herein, an interfacial p–n homojunction based on Zn2In2S5 was fabricated through the controlled assembly of p-type indium-defected Zn2In2S5 (VIn-ZIS) nanoflowers onto n-type oxygen-doped Zn2In2S5 (O-ZIS) nanosheets. Integrated theoretical simulations and comprehensive characterizations demonstrate that the VIn-ZIS/O-ZIS homojunctions adopt an S-scheme charge transfer route with a significantly strengthened interfacial electric field (IEF) effect, enabling spatial charge separation and a high driving force for both reduction and oxidation reactions. Consequently, VIn-ZIS/O-ZIS photocatalyst achieves a remarkable H2 evolution rate of 17.03 mmol g−1 h−1 without any cocatalysts, which is 7.6- and 3.8-fold higher than those of O-ZIS (2.23 mmol g−1 h−1) and VIn-ZIS (4.47 mmol g−1 h−1), respectively. Furthermore, an apparent quantum efficiency of 37.75% was attained at 370 nm. This work unravels the interplay among defect engineering, p–n homojunctions, and S-scheme charge transfer. The findings provide a blueprint for designing advanced photocatalysts.

KeyWords AITranslate

indium vacancy oxygen doping p-n homojunctions S-scheme system Zn2In2S5 photocatalysts
No data

Basic Information:

DOI:

Chinese Library Classification Number:

Citation Information:

The construction of p–n homojunctions represents a promising strategy for effective solar-driven photocatalytic hydrogen evolution, owing to their inherent advantages of superior lattice matching and minimized charge transfer resistance. However, this approach remains largely unexplored. Herein, an interfacial p–n homojunction based on Zn2In2S5 was fabricated through the controlled assembly of p-type indium-defected Zn2In2S5 (VIn-ZIS) nanoflowers onto n-type oxygen-doped Zn2In2S5 (O-ZIS) nanosheets. Integrated theoretical simulations and comprehensive characterizations demonstrate that the VIn-ZIS/O-ZIS homojunctions adopt an S-scheme charge transfer route with a significantly strengthened interfacial electric field (IEF) effect, enabling spatial charge separation and a high driving force for both reduction and oxidation reactions. Consequently, VIn-ZIS/O-ZIS photocatalyst achieves a remarkable H2 evolution rate of 17.03 mmol g−1 h−1 without any cocatalysts, which is 7.6- and 3.8-fold higher than those of O-ZIS (2.23 mmol g−1 h−1) and VIn-ZIS (4.47 mmol g−1 h−1), respectively. Furthermore, an apparent quantum efficiency of 37.75% was attained at 370 nm. This work unravels the interplay among defect engineering, p–n homojunctions, and S-scheme charge transfer. The findings provide a blueprint for designing advanced photocatalysts.

quote

GB/T 7714-2015 [1] In Situ Construction of S-Scheme VIn-Zn2In2S5/O-Zn2In2S5 p–n Homojunctions for Enhanced Photocatalytic Hydrogen Evolution[J]. Rare Metals, 2026(3).
MLA [1] "In Situ Construction of S-Scheme VIn-Zn2In2S5/O-Zn2In2S5 p–n Homojunctions for Enhanced Photocatalytic Hydrogen Evolution." Rare Metals, no. 3, 2026.
APA [1] (2026). In Situ Construction of S-Scheme VIn-Zn2In2S5/O-Zn2In2S5 p–n Homojunctions for Enhanced Photocatalytic Hydrogen Evolution. Rare Metals(3).
IEEE [1] "In Situ Construction of S-Scheme VIn-Zn2In2S5/O-Zn2In2S5 p–n Homojunctions for Enhanced Photocatalytic Hydrogen Evolution," Rare Metals, no. 3, 2026. keywords: {indium vacancy;oxygen doping;p-n homojunctions;S-scheme system;Zn2In2S5 photocatalysts}