daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Graft Copolymers of N-Isopropylacrylamide with Poly(d,l-lactide) or Poly(ε-caprolactone) Macromonomers: A Promising Class of Thermoresponsive Polymers with a Tunable LCST AITranslate

Belarus|Research Institute for Physical Chemical Problems of the Belarusian State University; Belarus|Research Institute for Physical Chemical Problems of the Belarusian State University; Sechenov First Moscow State Medical University; Sechenov First Moscow State Medical University; Lomonosov Moscow State University; Russia|National University of Ireland; Sechenov First Moscow State Medical University; Sechenov First Moscow State Medical University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

A series of well-defined poly(d,l-lactide) and poly(ε-caprolactone) macromonomers (Mn of ∼ 600 and ∼1200 Da) bearing a (meth)acrylate group at one side of the chain and either a hydrophobic nonpolar butyl group or a hydrophilic polar hydroxyl group at the other side of the chain were synthesized via 1,8-diazabicyclo[5.4.0]undec-7-ene-catalyzed ring-opening polymerization (ROP) of d,l-lactide and methanesulfonic acid-catalyzed ROP of ε-caprolactone, respectively. Then, a series of well-defined random copolymers (Mn of ∼ 30 000 Da, Đ < 1.25) were prepared via reversible addition–fragmentation chain transfer (RAFT)-mediated copolymerization of N-isopropylacrylamide with these macromonomers. It was found that the cloud point temperature of the graft copolymers almost linearly decreased from 32.1 to ∼14 °C, with increasing the content of the polyester macromonomer with a hydrophobic butyl end group in a copolymer chain from 0 to 17 wt %. A much smaller shift in the transition temperature (from 32.1 to ∼ 23 °C) was observed for the graft copolymers of N-isopropylacrylamide with polyesters bearing a polar hydroxyl group at the chain end. The thermoresponsive behavior dependence on the copolymer composition of the synthesized graft copolymers or their binary mixtures with poly(N-isopropylacrylamide) (PNIPAM) was also demonstrated in this study. Finally, it was proved that the obtained graft copolymers showed no cytotoxicity, and films prepared from these copolymers displayed better cell adhesion as compared to those prepared from neat PNIPAM.

KeyWords AITranslate

RAFT polymerization poly(Nisopropylacrylamide) thermoresponsive polymers cell adhesion graft copolymers Show More
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01732

Chinese Library Classification Number:

Citation Information:

A series of well-defined poly(d,l-lactide) and poly(ε-caprolactone) macromonomers (Mn of ∼ 600 and ∼1200 Da) bearing a (meth)acrylate group at one side of the chain and either a hydrophobic nonpolar butyl group or a hydrophilic polar hydroxyl group at the other side of the chain were synthesized via 1,8-diazabicyclo[5.4.0]undec-7-ene-catalyzed ring-opening polymerization (ROP) of d,l-lactide and methanesulfonic acid-catalyzed ROP of ε-caprolactone, respectively. Then, a series of well-defined random copolymers (Mn of ∼ 30 000 Da, Đ < 1.25) were prepared via reversible addition–fragmentation chain transfer (RAFT)-mediated copolymerization of N-isopropylacrylamide with these macromonomers. It was found that the cloud point temperature of the graft copolymers almost linearly decreased from 32.1 to ∼14 °C, with increasing the content of the polyester macromonomer with a hydrophobic butyl end group in a copolymer chain from 0 to 17 wt %. A much smaller shift in the transition temperature (from 32.1 to ∼ 23 °C) was observed for the graft copolymers of N-isopropylacrylamide with polyesters bearing a polar hydroxyl group at the chain end. The thermoresponsive behavior dependence on the copolymer composition of the synthesized graft copolymers or their binary mixtures with poly(N-isopropylacrylamide) (PNIPAM) was also demonstrated in this study. Finally, it was proved that the obtained graft copolymers showed no cytotoxicity, and films prepared from these copolymers displayed better cell adhesion as compared to those prepared from neat PNIPAM.

quote

GB/T 7714-2015 [1] Evgenii A. Ksendzov, Pavel A. Nikishau, Irina M. Zurina, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01732.
MLA [1] Evgenii A. Ksendzov, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01732.
APA [1] Evgenii A. Ksendzov, Pavel A. Nikishau, Irina M. Zurina, Viktoria S. Presniakova, Peter Timashev, Yuri A. Rochev, Svetlana Kotova, & Sergei V. Kostjuk. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01732
IEEE [1] Evgenii A. Ksendzov, Pavel A. Nikishau, Irina M. Zurina, Viktoria S. Presniakova, Peter Timashev, Yuri A. Rochev, Svetlana Kotova, and Sergei V. Kostjuk, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01732. keywords: {RAFT polymerization;poly(Nisopropylacrylamide);thermoresponsive polymers;cell adhesion;graft copolymers;Show More}