daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Large-Scale Manufacture of Recyclable Bioplastics from Renewable Cellulosic Biomass Derived from Softwood Kraft Pulp AITranslate

South China University of Technology; South China University of Technology; West Yunnan University of Applied Sciences; South China University of Technology; South China University of Technology; South China University of Technology; South China University of Technology
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

Petrochemical plastic accumulated on earth has caused a great threat to the ecological environment. Recently, the cellulose film has been one of the most attractive candidates to replace petroleum-based plastics owing to its favorable biodegradability, optical transparency, and resource abundance. However, the general strategies (including vacuum filtration, solution casting, etc.) to fabricate cellulose films are usually time-consuming and difficult to industrialize. Moreover, these films still suffer from inferior stability against water and poor mechanical strength in a humid environment, which is insufficient for practical applications. Herein, we report a facile and large-scale preparation strategy to manufacture high-performance cellulose bioplastic films composed of chemically and physically dual-crosslinked carboxymethylated cellulose fibers (CMFs). Moreover, the whole preparation time was within only 1 h, superior to the most reported method. In this process, bleached softwood kraft pulp was carboxymethylated to form a homogeneous negatively charged CMF slurry that can further crosslink with the polyamide epichlorohydrin resin or aluminum sulfate [Al2(SO4)3] via the strong electrostatic interaction. The resulting CMF-based bioplastic shows a high mechanical strength (158.2 MPa), excellent water stability, and improved wet strength (20.7 MPa). Furthermore, the CMF-based bioplastic also exhibits both high optical transparency (89.4%) and haze feature (77.9%), good thermal stability, and easy recyclability by mechanical disintegration. This fast, scalable, and low-cost strategy involving the simple papermaking process provides a promising industrialization route to produce a strong, recyclable, and sustainable cellulosic bioplastic that can potentially replace petrochemical plastics in engineering and packaging implications.

KeyWords AITranslate

bioplastic cellulosic biomass largescale fabrication papermaking process waterresistance
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01729

Chinese Library Classification Number:

Citation Information:

Petrochemical plastic accumulated on earth has caused a great threat to the ecological environment. Recently, the cellulose film has been one of the most attractive candidates to replace petroleum-based plastics owing to its favorable biodegradability, optical transparency, and resource abundance. However, the general strategies (including vacuum filtration, solution casting, etc.) to fabricate cellulose films are usually time-consuming and difficult to industrialize. Moreover, these films still suffer from inferior stability against water and poor mechanical strength in a humid environment, which is insufficient for practical applications. Herein, we report a facile and large-scale preparation strategy to manufacture high-performance cellulose bioplastic films composed of chemically and physically dual-crosslinked carboxymethylated cellulose fibers (CMFs). Moreover, the whole preparation time was within only 1 h, superior to the most reported method. In this process, bleached softwood kraft pulp was carboxymethylated to form a homogeneous negatively charged CMF slurry that can further crosslink with the polyamide epichlorohydrin resin or aluminum sulfate [Al2(SO4)3] via the strong electrostatic interaction. The resulting CMF-based bioplastic shows a high mechanical strength (158.2 MPa), excellent water stability, and improved wet strength (20.7 MPa). Furthermore, the CMF-based bioplastic also exhibits both high optical transparency (89.4%) and haze feature (77.9%), good thermal stability, and easy recyclability by mechanical disintegration. This fast, scalable, and low-cost strategy involving the simple papermaking process provides a promising industrialization route to produce a strong, recyclable, and sustainable cellulosic bioplastic that can potentially replace petrochemical plastics in engineering and packaging implications.

quote

GB/T 7714-2015 [1] Chunfa Lei, Yuan Wei, Yangyang Qian, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01729.
MLA [1] Chunfa Lei, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01729.
APA [1] Chunfa Lei, Yuan Wei, Yangyang Qian, Qinwen Wang, Penghui Zhu, Ge Qiu, & Gang Chen. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01729
IEEE [1] Chunfa Lei, Yuan Wei, Yangyang Qian, Qinwen Wang, Penghui Zhu, Ge Qiu, and Gang Chen, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01729. keywords: {bioplastic;cellulosic biomass;largescale fabrication;papermaking process;waterresistance}