daohang fenxiangbox searchbox qikanlogonew daohangnew searchboxnew navrightzone footerzone paper

Superior Corrosion and UV-Resistant Highly Porous Poly(vinylidene fluoride-co-hexafluoropropylene)/alumina Superhydrophobic Coating AITranslate

Ain Shams University; and Development Institute; Ain Shams University; Ain Shams University; Qatar University
AITranslate
Publisher: ACS
Share Citation Information Add to Favorites
111111

    Scan to share on WeChat or Moments

Use WeChat scan.
Share with WeChat friends or Moments

Abstract AITranslate

The current research is devoted to fabricating a superhydrophobic coating on alumina surfaces via a facile one-step electrospinning technique. The wettability properties of the as-prepared coating were investigated. The polymeric coatings exhibited a water contact angle (WCA) of about 152° ± 3 and a sliding angle (SA) is 4 ± 2°. However, a WCA of 154 ± 2° and a SA of 3 ± 2° were recorded after the addition of Al2O3 nanoparticles. The wettability of the prepared coatings has also been inspected after exposure to intense UV irradiation of 0.89 W/(m2 nm) and high-temperature degree of 60 °C, for 500 h. It was found that the measured WCA and water contact hysteresis (WCAH) for the poly(vinylidene fluoride-co-hexafluoropropylene) PVDF-HFP/Al2O3 nanocomposite 150 ± 1° and 10 ± 1° compared with 122 ± 4° and 22 ± 4° of pure PVDF-HFP, respectively. The morphology of the superhydrophobic coating was explored, illustrating the construction of a beaded fiber structure. The surface roughness of the fabricated super water-repellent coatings was recorded using an atomic force microscope (AFM). The electrochemical behavior of superhydrophobic coating was evaluated by electrochemical impedance spectroscopy (EIS) in 3.5 wt % NaCl solution before and after exposure to UV radiation. The research outcomes promote a one-step fabrication technique to prepare polymeric superhydrophobic coatings with good resistance for corrosion and degradation under UV irradiation.

KeyWords AITranslate

superhydrophobic corrosion coatings UV irradiation PVDFHFP nanocomposite
No data

Basic Information:

DOI:https://doi.org/10.1021/acsapm.1c01710

Chinese Library Classification Number:

Citation Information:

The current research is devoted to fabricating a superhydrophobic coating on alumina surfaces via a facile one-step electrospinning technique. The wettability properties of the as-prepared coating were investigated. The polymeric coatings exhibited a water contact angle (WCA) of about 152° ± 3 and a sliding angle (SA) is 4 ± 2°. However, a WCA of 154 ± 2° and a SA of 3 ± 2° were recorded after the addition of Al2O3 nanoparticles. The wettability of the prepared coatings has also been inspected after exposure to intense UV irradiation of 0.89 W/(m2 nm) and high-temperature degree of 60 °C, for 500 h. It was found that the measured WCA and water contact hysteresis (WCAH) for the poly(vinylidene fluoride-co-hexafluoropropylene) PVDF-HFP/Al2O3 nanocomposite 150 ± 1° and 10 ± 1° compared with 122 ± 4° and 22 ± 4° of pure PVDF-HFP, respectively. The morphology of the superhydrophobic coating was explored, illustrating the construction of a beaded fiber structure. The surface roughness of the fabricated super water-repellent coatings was recorded using an atomic force microscope (AFM). The electrochemical behavior of superhydrophobic coating was evaluated by electrochemical impedance spectroscopy (EIS) in 3.5 wt % NaCl solution before and after exposure to UV radiation. The research outcomes promote a one-step fabrication technique to prepare polymeric superhydrophobic coatings with good resistance for corrosion and degradation under UV irradiation.

quote

GB/T 7714-2015 [1] A. Bahgat Radwan, Soliman I. ElHout, M. A. M. Ibrahim, et al. ACS Applied Polymer Materials, 2022(4). DOI:10.1021/acsapm.1c01710.
MLA [1] A. Bahgat Radwan, et al., ACS Applied Polymer Materials, no. 4, 2022, https://doi.org/10.1021/acsapm.1c01710.
APA [1] A. Bahgat Radwan, Soliman I. ElHout, M. A. M. Ibrahim, E. Hamed Ismail, & Aboubakr M. Abdullah. (2022). ACS Applied Polymer Materials(4). https://doi.org/10.1021/acsapm.1c01710
IEEE [1] A. Bahgat Radwan, Soliman I. ElHout, M. A. M. Ibrahim, E. Hamed Ismail, and Aboubakr M. Abdullah, ACS Applied Polymer Materials, no. 4, 2022, doi: 10.1021/acsapm.1c01710. keywords: {superhydrophobic;corrosion;coatings;UV irradiation;PVDFHFP;nanocomposite}