Study on Preparation Process of Yttrium-Stabilized Nano-Zirconia by Hydrothermal Hydrolysis AITranslate
Abstract AITranslate
Yttrium-stabilized zirconia(YSZ)was prepared by hydrothermal hydrolysis using zirconium oxychloride,yttrium chloride,and ammonia as raw materials and polyethylene glycol as a dispersant.The effects of zirconium ion concentration,reaction temperature,yttrium doping amount,dispersant addition,and calcination temperature on the morphology,dispersity,particle size,and crystal form of the zirconia products were systematically studied.The results show that under the conditions of zirconium ion concentration of 0.8 mol/L,reaction temperature of 180℃,yttrium doping amount of 3%(molar fraction),dispersant addition of 2%(mass fraction),and calcination temperature of 1000℃,yttrium-stabilized nano-zirconia powders with good dispersity,uniform particle size distribution and spherical-like shape could be obtained.
KeyWords AITranslate
1刘树信,王海滨.氧化锆及掺杂氧化锆的研究进展[J].耐火材料,2011,45(3):209-213. 被引量:11
2赵婷,王钢,齐嘉豪,武越,孙晓敏.纳米氧化锆的制备和表征[J].化工设计通讯,2018,44(12):88-90. 被引量:3
3刘志宏,赵立星,刘智勇,李玉虎,李启厚.钇稳定四方相氧化锆粉末的水热水解法制备[J].中国有色金属学报,2016,26(6):1339-1349. 被引量:5
4张帆,王鑫,张良,李芳,骈小璇,张锐.ZrO_2陶瓷的微波烧结制备及其性能[J].硅酸盐学报,2019,47(3):353-357. 被引量:12
5靳艺凯,陈鹏,郑华强,王双喜.纳米氧化锆粉体制备及其表面改性技术的研究进展[J].陶瓷,2020(12):12-20. 被引量:3
6于长清,余悠然,赵英民,巢雄宇,袁武华.稀土氧化物RE2O3(RE=La,Ce,Gd,Yb)掺杂氧化钇稳定氧化锆气凝胶相稳定性与晶粒生长分析[J].硅酸盐通报,2020,39(5):1620-1626. 被引量:2
1杨培周,陆书花,李丛旭,王泽民.柠檬酸水解法制备大豆多肽的研究[J].农产品加工,2023(10):1-5.
2朱绍伊,乔云河,刘英俊,杜爱华.基于锆离子(Ⅳ)-羧基金属配位键的高强高韧羧基丁腈橡胶[J].合成橡胶工业,2023,46(3):204-209.
3卫威,周亚芳.关于大学生思想政治教育协同育人机制研究[J].大学:思政教研,2023(5):41-44.
4周哲,夏大旺,李智,廖桓毅,金鑫.溶胶凝胶、碳热/硼热还原法制备ZrB_(2)-SiC-LaB_(6)超细复相粉体[J].粉末冶金材料科学与工程,2023,28(3):223-232.
5赵秀梅,马天洲,范三程.矿用大功率充电机防爆电控箱结构及散热设计研究[J].煤炭技术,2023,42(5):233-236.
6叶泽甫,孟献梁,吴国光.PSS分散剂亲油基团对不黏煤成浆特性及表面吸附行为影响[J].洁净煤技术,2023,29(6):180-188.
7白莹,毛旖旎,曾春梅.共同性内、外斜视患者术前眼表状况及术后视觉功能的比较[J].新疆医科大学学报,2023,46(6):772-776.
8刘文杰.数据产权的法律表达[J].法学研究,2023,45(3):36-53.
Basic Information:
DOI:
Chinese Library Classification Number:TQ134.12[化学工程—无机化工]
Citation Information:
Yttrium-stabilized zirconia(YSZ)was prepared by hydrothermal hydrolysis using zirconium oxychloride,yttrium chloride,and ammonia as raw materials and polyethylene glycol as a dispersant.The effects of zirconium ion concentration,reaction temperature,yttrium doping amount,dispersant addition,and calcination temperature on the morphology,dispersity,particle size,and crystal form of the zirconia products were systematically studied.The results show that under the conditions of zirconium ion concentration of 0.8 mol/L,reaction temperature of 180℃,yttrium doping amount of 3%(molar fraction),dispersant addition of 2%(mass fraction),and calcination temperature of 1000℃,yttrium-stabilized nano-zirconia powders with good dispersity,uniform particle size distribution and spherical-like shape could be obtained.
quote
| GB/T 7714-2015 | [1] TAN Hai-xiang, QIN Wen-zhong, WEI Shi-qiang, et al. Study on Preparation Process of Yttrium-Stabilized Nano-Zirconia by Hydrothermal Hydrolysis[J]. Rare Metals and Cemented Carbides, 2023(3): 77-81. |
| MLA | [1] TAN Hai-xiang, et al., "Study on Preparation Process of Yttrium-Stabilized Nano-Zirconia by Hydrothermal Hydrolysis." Rare Metals and Cemented Carbides, no. 3, 2023, pp. 77-81. |
| APA | [1] TAN Hai-xiang, QIN Wen-zhong, WEI Shi-qiang, GAN Pei-yuan, & HUANG Yu-feng. (2023). Study on Preparation Process of Yttrium-Stabilized Nano-Zirconia by Hydrothermal Hydrolysis. Rare Metals and Cemented Carbides(3), 77-81. |
| IEEE | [1] TAN Hai-xiang, QIN Wen-zhong, WEI Shi-qiang, GAN Pei-yuan, and HUANG Yu-feng, "Study on Preparation Process of Yttrium-Stabilized Nano-Zirconia by Hydrothermal Hydrolysis," Rare Metals and Cemented Carbides, no. 3, pp. 77-81, 2023. keywords: {yttrium-stabilized nano-zirconia;hydrothermal hydrolysis;zirconium oxychloride;ammonia;process condition} |